JP4899325B2 - 固体酸化物形燃料電池の製造方法 - Google Patents
固体酸化物形燃料電池の製造方法 Download PDFInfo
- Publication number
- JP4899325B2 JP4899325B2 JP2005062821A JP2005062821A JP4899325B2 JP 4899325 B2 JP4899325 B2 JP 4899325B2 JP 2005062821 A JP2005062821 A JP 2005062821A JP 2005062821 A JP2005062821 A JP 2005062821A JP 4899325 B2 JP4899325 B2 JP 4899325B2
- Authority
- JP
- Japan
- Prior art keywords
- metal oxide
- electrode layer
- oxide film
- fuel cell
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
金属源と、酸化剤又は還元剤とを含む金属酸化物膜形成用溶液に多孔質電極層を浸漬することにより、第1金属酸化物膜と、第2金属酸化物膜とを含む電解質層を形成しており、前記第1金属酸化物膜は前記多孔質電極層上に形成され、前記第2金属酸化物膜は、前記多孔質電極層内の全ての気孔において気孔を形成する壁面の少なくとも一部に沿って形成されることを特徴とする。
(化1) ClO4 - + H2O + 2e- ⇔ ClO3 - + 2OH-
(化2) ClO3 - + H2O + 2e- ⇔ ClO2 - + 2OH-
(化3) ClO2 - + H2O + 2e- ⇔ ClO- + 2OH-
(化4) 2ClO- + 2H2O + 2e- ⇔ Cl2 + 4OH-
(化5) BrO3 - + 2H2O + 4e- ⇔ BrO- + 4OH-
(化6) 2BrO- + 2H2O + 2e- ⇔ Br2 + 4OH-
(化7) NO3 - + H2O + 2e- ⇔ NO2 - + 2OH-
(化8) NO2 - + 3H2O + 3e- ⇔ NH3 + 3OH-
11 電解質層
11a 第1金属酸化物膜
11b 第2金属酸化物膜
12 燃料極層
12a,31a 壁面
13 空気極層
30 電解質層の一部
31 多孔質燃料極基板(燃料極層)
Claims (9)
- 電解質層と、前記電解質層の一部を挟持する一対の多孔質電極層とを有し、前記電解質層は、前記一対の多孔質電極層で挟持された第1金属酸化物膜と、一方の前記多孔質電極層内の気孔を形成する壁面の少なくとも一部に沿って形成された第2金属酸化物膜とを含み、前記第1金属酸化物膜及び前記第2金属酸化物膜は電解質材料で構成されており、前記一方の多孔質電極層内の全ての気孔内に前記第2金属酸化物膜の一部が存在している固体酸化物形燃料電池の製造方法であって、
金属源と、酸化剤又は還元剤とを含む金属酸化物膜形成用溶液に多孔質電極層を浸漬することにより、第1金属酸化物膜と、第2金属酸化物膜とを含む電解質層を形成しており、前記第1金属酸化物膜は前記多孔質電極層上に形成され、前記第2金属酸化物膜は、前記多孔質電極層内の全ての気孔において気孔を形成する壁面の少なくとも一部に沿って形成されることを特徴とする固体酸化物形燃料電池の製造方法。 - 前記第1金属酸化物膜は、厚みが10nm以上10μm以下である請求項1に記載の固体酸化物形燃料電池の製造方法。
- 前記第1金属酸化物膜は、厚みが100nm以上1μm以下である請求項2に記載の固体酸化物形燃料電池の製造方法。
- 前記第2金属酸化物膜は、厚みが10nm以上1μm以下である請求項1に記載の固体酸化物形燃料電池の製造方法。
- 前記気孔は、平均径が1μm以上100μm以下である請求項1に記載の固体酸化物形燃料電池の製造方法。
- 前記第1及び第2金属酸化物膜のうち少なくとも一方は、酸化ジルコニウム、酸化セリウム及び酸化ランタンから選ばれる少なくとも一つを含む複合金属酸化物からなる請求項1に記載の固体酸化物形燃料電池の製造方法。
- 前記複合金属酸化物は、蛍石型又はペロブスカイト型の結晶構造を有する請求項6に記載の固体酸化物形燃料電池の製造方法。
- 前記一対の多孔質電極層は、燃料極層及び空気極層であり、
前記燃料極層は、蛍石型又はペロブスカイト型の結晶構造を有する酸化物イオン伝導体と金属触媒とを含む請求項1に記載の固体酸化物形燃料電池の製造方法。 - 前記一対の多孔質電極層は、燃料極層及び空気極層であり、
前記空気極層は、ペロブスカイト型の結晶構造を有する金属酸化物及び貴金属から選ばれる少なくとも一つを含む請求項1又は請求項8に記載の固体酸化物形燃料電池の製造方法。