JP5479729B2 - 金属精製方法及び装置、精製金属、鋳造品、金属製品及び電解コンデンサ - Google Patents
金属精製方法及び装置、精製金属、鋳造品、金属製品及び電解コンデンサ Download PDFInfo
- Publication number
- JP5479729B2 JP5479729B2 JP2008332050A JP2008332050A JP5479729B2 JP 5479729 B2 JP5479729 B2 JP 5479729B2 JP 2008332050 A JP2008332050 A JP 2008332050A JP 2008332050 A JP2008332050 A JP 2008332050A JP 5479729 B2 JP5479729 B2 JP 5479729B2
- Authority
- JP
- Japan
- Prior art keywords
- purification
- cooling body
- metal
- peripheral speed
- stage
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
(1)精製すべき溶融金属中に冷却体を浸漬し、この冷却体を回転させながら冷却体表面に高純度金属を晶出させる金属の精製方法において、精製初期前半の冷却体の最大周速を精製初期以降の平均周速よりも大きく設定し、かつ精製初期後半の冷却体の平均周速を精製初期以降の平均周速よりも小さく設定し、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように設定して精製を行うことを特徴とする金属精製方法。
(2)前記精製初期前半が精製開始から全精製時間×0.1まで、前記精製初期後半が精製初期前半の終了から全精製時間×0.1までである前項1に記載の金属精製方法。
(3)前記精製初期前半が精製開始から全精製時間×0.05まで、前記精製初期後半が精製初期前半の終了から全精製時間×0.05までである前項1に記載の金属精製方法。
(4)前記精製初期前半の冷却体の最大周速V1と、前記精製初期後半の冷却体の平均周速V2と、精製初期以降の平均周速V4の関係が、V1≧V4×1.1、V2≦V4×0.9に設定されている前項1〜3のいずれかに記載の金属精製方法。
(5)精製される金属がアルミニウムである前項1〜4のいずれかに記載の金属精製方法。
(6)不純物元素の組成分布が、その不純物平均濃度の70%以上、130%以下の範囲内である金属精製塊。
(7)精製すべき溶融金属を収容する炉体と、前記炉体に収容された溶融金属中に浸漬される冷却体と、前記冷却体を回転させる回転駆動装置と、精製初期前半の冷却体の最大周速が精製初期以降の平均周速よりも大きくなるように、かつ精製初期後半の冷却体の平均周速が精製初期以降の平均周速よりも小さくなるように、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように、前記回転駆動装置による冷却体の回転速度を制御する制御手段と、を備えたことを特徴とする金属精製装置。
(8)前記精製初期前半が精製開始から全精製時間×0.1まで、前記精製初期後半が精製初期前半の終了から全精製時間×0.1までである前項7に記載の金属精製装置。
(9)前記精製初期前半が精製開始から全精製時間×0.05まで、前記精製初期後半が精製初期前半の終了から全精製時間×0.05までである前項7に記載の金属精製装置。
(10)前記制御手段は、前記精製初期前半の冷却体の最大周速V1と、前記精製初期後半の冷却体の平均周速V2と、精製初期以降の平均周速V4の関係が、V1≧V4×1.1、V2≦V4×0.9となるように、回転駆動装置による冷却体の回転速度を制御する前項7〜9のいずれかに記載の金属精製装置。
(11)請求項1ないし5のいずれかに記載の方法で精製された精製金属。
(12)請求項11に記載の精製金属から製造された鋳造品。
(13)請求項12に記載の鋳造品が圧延されてなる金属製品。
(14)請求項13に記載の金属製品が電極材として用いられている電解コンデンサ。
不純物として主にFe:500ppm、Si:400ppmが含まれるアルミニウム溶湯を精製保持炉内に入れ、精製炉ヒーターの電力を調整し665℃の温度に保持する。その後、温度を調整した上端部の外径が150mmであるテーパー形状の回転冷却体を溶湯中に浸潰し、以下に示す速度で回転させながら、7分間回転冷却体周面に精製アルミニウムを晶出させた。なお回転冷却体内には圧縮エアーを直接当てて冷却させた。
(1)冷却体の回転数を、精製開始から全精製時間×0.025まで周速V1:3.5m/sec、その後全精製時間×0.05まで平均周速V2:2.7m/sec、最大周速V3:2.9m/sec、それ以降周速3.1m/sec(従って平均周速V4も3.1m/sec)に設定して、5回の精製実験を実施した結果、精製塊重量は平均で6.16kgであった。また、精製中に発生した剥離回数を精製開始後の時間経過とともに調査したところ、表1の通りであり、精製開始から全精製時間×0.05以内での剥離発生率は減少した。
不純物として主にFe:500ppm、Si:400ppmが含まれるアルミニウム溶湯を精製保持炉内に入れ、精製炉ヒーターの電力を調整し665℃の温度に保持する。その後、温度を調整した上端部の外径が150mmであるテーパー形状の回転冷却体を溶湯中に浸潰し、周速3.1m/secの一定速度で回転させながら、7分間回転冷却体周面に精製アルミニウムを晶出させた。なお回転冷却体内には圧縮エアーを直接当てて冷却させた。
2 溶融金属(溶湯)
3 冷却体
4 回転駆動装置
5 制御部
6 精製金属塊
Claims (8)
- 精製すべき溶融金属中に冷却体を浸漬し、この冷却体を回転させながら冷却体表面に高純度金属を晶出させる金属の精製方法において、
前記冷却体を前記溶融金属中へ浸漬したときを精製開始とし、この精製開始から前記冷却体を前記溶融金属から引き上げたときまでを全精製時間とし、精製開始から全精製時間×0.1までを精製初期前半とし、精製初期前半の終了から全精製時間×0.1までを精製初期後半とし、前記精製初期前半と精製初期後半を合わせて精製初期としたとき、精製初期前半の冷却体の最大周速を精製初期以降の平均周速よりも大きく設定し、かつ精製初期後半の冷却体の平均周速を精製初期以降の平均周速よりも小さく設定し、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように設定して精製を行うことを特徴とする金属精製方法。 - 精製すべき溶融金属中に冷却体を浸漬し、この冷却体を回転させながら冷却体表面に高純度金属を晶出させる金属の精製方法において、
前記冷却体を前記溶融金属中へ浸漬したときを精製開始とし、この精製開始から前記冷却体を前記溶融金属から引き上げたときまでを全精製時間とし、精製開始から全精製時間×0.05までを精製初期前半とし、精製初期前半の終了から全精製時間×0.05までを精製初期後半とし、前記精製初期前半と精製初期後半を合わせて精製初期としたとき、精製初期前半の冷却体の最大周速を精製初期以降の平均周速よりも大きく設定し、かつ精製初期後半の冷却体の平均周速を精製初期以降の平均周速よりも小さく設定し、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように設定して精製を行うことを特徴とする金属精製方法。 - 前記精製初期前半の冷却体の最大周速V1と、前記精製初期後半の冷却体の平均周速V2と、精製初期以降の平均周速V4の関係が、V1≧V4×1.1、V2≦V4×0.9に設定されている請求項1または2に記載の金属精製方法。
- 精製される金属がアルミニウムである請求項1〜3のいずれかに記載の金属精製方法。
- 不純物元素の組成分布が、その不純物平均濃度の70%以上、130%以下の範囲内であるアルミニウム精製塊。
- 精製すべき溶融金属を収容する炉体と、
前記炉体に収容された溶融金属中に浸漬される冷却体と、
前記冷却体を回転させる回転駆動装置と、
前記冷却体を前記溶融金属中へ浸漬したときを精製開始とし、この精製開始から前記冷却体を前記溶融金属から引き上げたときまでを全精製時間とし、精製開始から全精製時間×0.1までを精製初期前半とし、精製初期前半の終了から全精製時間×0.1までを精製初期後半とし、前記精製初期前半と精製初期後半を合わせて精製初期としたとき、精製初期前半の冷却体の最大周速が精製初期以降の平均周速よりも大きくなるように、かつ精製初期後半の冷却体の平均周速が精製初期以降の平均周速よりも小さくなるように、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように、 前記回転駆動装置による冷却体の回転速度を制御する制御手段と、
を備えたことを特徴とする金属精製装置。 - 精製すべき溶融金属を収容する炉体と、
前記炉体に収容された溶融金属中に浸漬される冷却体と、
前記冷却体を回転させる回転駆動装置と、
前記冷却体を前記溶融金属中へ浸漬したときを精製開始とし、この精製開始から前記冷却体を前記溶融金属から引き上げたときまでを全精製時間とし、精製開始から全精製時間×0.05までを精製初期前半とし、精製初期前半の終了から全精製時間×0.05までを精製初期後半とし、前記精製初期前半と精製初期後半を合わせて精製初期としたとき、精製初期前半の冷却体の最大周速が精製初期以降の平均周速よりも大きくなるように、かつ精製初期後半の冷却体の平均周速が精製初期以降の平均周速よりも小さくなるように、さらに精製初期後半の冷却体の最大周速が精製初期以降の平均周速を超えないように、 前記回転駆動装置による冷却体の回転速度を制御する制御手段と、
を備えたことを特徴とする金属精製装置。 - 前記制御手段は、前記精製初期前半の冷却体の最大周速V1と、前記精製初期後半の冷却体の平均周速V2と、精製初期以降の平均周速V4の関係が、V1≧V4×1.1、V2≦V4×0.9となるように、回転駆動装置による冷却体の回転速度を制御する請求項6または7に記載の金属精製装置。