Summary of the invention
The purpose of this invention is to provide a kind of look porcelain composite membrane and the technology of windowing thereof, can on the technology porcelain, adopt the Liu Baijia coloured silk of windowing, to adapt to the demand that the modern pursues elegant artistic level.
A kind of color porcelain windowing processing technique, its processing technology is following:
1, with after the fine finishining of micro-nano carbonic acid calcium composite powder, add clear water, brute force stirs; It is mixed; Be the suspension state, add the polyisoprene latex again and mix, promptly get complex liquid; The ratio of said micro-nano carbonic acid calcium composite powder and clear water is 1: 1~1.5, and the fluid behind the said micro-nano carbonic acid calcium composite powder adding clear water and the ratio of polyisoprene latex are 1: 1~1.5.
2, make the lines mould of windowing of various bodies in advance.
3, before the glazing,, select for use suitable mould to glue prepared Chinese ink, again through trimming according to the design demand of product decoration; After the drying, the lines boundary line of the scope of windowing of on the base substrate suitable position, drawing evenly is coated with micro-nano complex liquid then carefully and neatly in the boundary line, form soft diaphragm; The unlikely infiltration of color glaze is windowed in the boundary, and integral body is executed color glaze immediately, tear diaphragm off behind upward intact first kind of glaze; In the boundary line of windowing, execute another kind of glaze again, on the glaze of two kinds of different color and lusters intact after, can realize disposablely going into klining and becoming; Product after burning till, two kinds of glaze colors set each other off, and are exceptionally eye-catching.On the white glaze of windowing, can add color various scenery with hills and waters according to design; Pictures such as birds and flowers, personage, animal worker poem literal, abundant intension and the color decorated, the artistry of raising product; Reach the effect that has more artistry than pure color glaze product, thereby improve the grade and the economic worth of product.
Said micro-nano carbonic acid calcium composite powder comprises porcelain powder, calcium carbonate, lithium carbonate, zinc oxide, silica flour, wherein the porcelain powder be 30%~70%, calcium carbonate 5%~15%, lithium carbonate 5%~10%, zinc oxide 5%~10%, silica flour 15%~30%.
Said micro-nano carbonic acid calcium composite powder comprises that the porcelain powder is 52%, calcium carbonate 10%, lithium carbonate 8%, zinc oxide 5%, silica flour 25%.
Said micro-nano carbonic acid calcium composite powder comprises that the porcelain powder is 40%, calcium carbonate 10%, lithium carbonate 8%, zinc oxide 5%, silica flour 30%.
Said micro-nano carbonic acid calcium composite powder comprises that the porcelain powder is 60%, calcium carbonate 5%, lithium carbonate 5%, zinc oxide 5%, silica flour 25%.
This color porcelain windowing processing technique has many characteristics than traditional decoration technology of windowing: 1, simple and easy, the effect raising of operation; 2, compound liquid film property is soft, and high resilience once can integral body tear off, need not the part is remake cleaning, and is simple; 3, not adsorbed water and colorant of composite membrane avoids causing product defects; 4, base substrate can twice glazing, and once-firing is saved energy resource consumption; 5, the color glaze that is adhered on composite membrane after the use and the film can be recycled respectively, both cuts the waste, again escapable cost; 6, the scope of application is extensive, both can be applicable to various art display, also can use the practical porcelain of various top grades, increases the designs and varieties of product, upgrade class and economic actual effect.
The specific embodiment
Implement 1
A kind of color porcelain windowing processing technique, its processing technology is following: 1, by the porcelain powder be 30%~70%, calcium carbonate 5%~15%, lithium carbonate 5%~10%, zinc oxide 5%~10%, silica flour 15%~30% is mixed with micro-nano carbonic acid calcium composite powder, through fine finishining; Add clear water; Brute force stirs, and it is mixed, and is the suspension state; Adding the polyisoprene latex again mixes; Promptly get complex liquid, the ratio of said micro-nano carbonic acid calcium composite powder and clear water is 1: 1~1.5, and the fluid behind the said micro-nano carbonic acid calcium composite powder adding clear water and the ratio of polyisoprene latex are 1: 1~1.5.
2, make the lines mould of windowing of various bodies in advance.
3, before the glazing,, select for use suitable mould to glue prepared Chinese ink, again through trimming according to the design demand of product decoration; After the drying, the lines boundary line of the scope of windowing of on the base substrate suitable position, drawing evenly is coated with micro-nano complex liquid then carefully and neatly in the boundary line, form soft diaphragm; The unlikely infiltration of color glaze is windowed in the boundary, and integral body is executed color glaze immediately, tear off to protect behind upward intact first kind of glaze and expand film; In the boundary line of windowing, execute another kind of glaze again, on the glaze of two kinds of different color and lusters intact after, can realize disposablely going into klining and becoming; Product after burning till, two kinds of glaze colors set each other off, and are exceptionally eye-catching.On the white glaze of windowing, can add color various scenery with hills and waters according to design; Pictures such as birds and flowers, personage, animal worker poem literal, abundant intension and the color decorated, the artistry of raising product; Reach the effect that has more artistry than pure color glaze product, thereby improve the grade and the economic worth of product.
Implement 2
A kind of color porcelain windowing processing technique, its processing technology is following: 1, by the porcelain powder be 52%, calcium carbonate 10%, lithium carbonate 8%, zinc oxide 5%, silica flour 25% is mixed with micro-nano carbonic acid calcium composite powder, through fine finishining; Add clear water; Brute force stirs, and it is mixed, and is the suspension state; Adding the polyisoprene latex again mixes; Promptly get complex liquid, the ratio of said micro-nano carbonic acid calcium composite powder and clear water is 1: 1~1.5, and the fluid behind the said micro-nano carbonic acid calcium composite powder adding clear water and the ratio of polyisoprene latex are 1: 1~1.5.
2, make the lines mould of windowing of various bodies in advance.
3, before the glazing,, select for use suitable mould to glue prepared Chinese ink, again through trimming according to the design demand of product decoration; After the drying, the lines boundary line of the scope of windowing of on the base substrate suitable position, drawing evenly is coated with micro-nano complex liquid then carefully and neatly in the boundary line, form soft diaphragm; The unlikely infiltration of color glaze is windowed in the boundary, and integral body is executed color glaze immediately, tear diaphragm off behind upward intact first kind of glaze; In the boundary line of windowing, execute another kind of glaze again, on the glaze of two kinds of different color and lusters intact after, can realize disposablely going into klining and becoming; Product after burning till, two kinds of glaze colors set each other off, and are exceptionally eye-catching.On the white glaze of windowing, can add color various scenery with hills and waters according to design; Pictures such as birds and flowers, personage, animal worker poem literal, abundant intension and the color decorated, the artistry of raising product; Reach the effect that has more artistry than pure color glaze product, thereby improve the grade and the economic worth of product.
Implement 3
A kind of color porcelain windowing processing technique, its processing technology is following: 1, by the porcelain powder be 40%, calcium carbonate 10%, lithium carbonate 8%, zinc oxide 5%, silica flour 30% is mixed with micro-nano carbonic acid calcium composite powder, through fine finishining; Add clear water; Brute force stirs, and it is mixed, and is the suspension state; Adding the polyisoprene latex again mixes; Promptly get complex liquid, the ratio of said micro-nano carbonic acid calcium composite powder and clear water is 1: 1~1.5, and the fluid behind the said micro-nano carbonic acid calcium composite powder adding clear water and the ratio of polyisoprene latex are 1: 1~1.5.
2, make the lines mould of windowing of various bodies in advance.
3, before the glazing,, select for use suitable mould to glue prepared Chinese ink, again through trimming according to the design demand of product decoration; After the drying, the lines boundary line of the scope of windowing of on the base substrate suitable position, drawing evenly is coated with micro-nano complex liquid then carefully and neatly in the boundary line, form soft diaphragm; The unlikely infiltration of color glaze is windowed in the boundary, and integral body is executed color glaze immediately, tear diaphragm off behind upward intact first kind of glaze; In the boundary line of windowing, execute another kind of glaze again, on the glaze of two kinds of different color and lusters intact after, can realize disposablely going into klining and becoming; Product after burning till, two kinds of glaze colors set each other off, and are exceptionally eye-catching.On the white glaze of windowing, can add color various scenery with hills and waters according to design; Pictures such as birds and flowers, personage, animal worker poem literal, abundant intension and the color decorated, the artistry of raising product; Reach the effect that has more artistry than pure color glaze product, thereby improve the grade and the economic worth of product.
Implement 4
A kind of color porcelain windowing processing technique, its processing technology is following: 1, by the porcelain powder be 60%, calcium carbonate 5%, lithium carbonate 5%, zinc oxide 5%, silica flour 25% is mixed with micro-nano carbonic acid calcium composite powder, through fine finishining; Add clear water; Brute force stirs, and it is mixed, and is the suspension state; Adding the polyisoprene latex again mixes; Promptly get complex liquid, the ratio of said micro-nano carbonic acid calcium composite powder and clear water is 1: 1~1.5, and the fluid behind the said micro-nano carbonic acid calcium composite powder adding clear water and the ratio of polyisoprene latex are 1: 1~1.5.
2, make the lines mould of windowing of various bodies in advance.
3, before the glazing,, select for use suitable mould to glue prepared Chinese ink, again through trimming according to the design demand of product decoration; After the drying, the lines boundary line of the scope of windowing of on the base substrate suitable position, drawing evenly is coated with micro-nano complex liquid then carefully and neatly in the boundary line, form soft diaphragm; The unlikely infiltration of color glaze is windowed in the boundary, and integral body is executed color glaze immediately, tear diaphragm off behind upward intact first kind of glaze; In the boundary line of windowing, execute another kind of glaze again, on the glaze of two kinds of different color and lusters intact after, can realize disposablely going into klining and becoming; Product after burning till, two kinds of glaze colors set each other off, and are exceptionally eye-catching.On the white glaze of windowing, can add color various scenery with hills and waters according to design; Pictures such as birds and flowers, personage, animal worker poem literal, abundant intension and the color decorated, the artistry of raising product; Reach the effect that has more artistry than pure color glaze product, thereby improve the grade and the economic worth of product.