JP4240312B2 - 電池 - Google Patents
電池 Download PDFInfo
- Publication number
- JP4240312B2 JP4240312B2 JP2004341181A JP2004341181A JP4240312B2 JP 4240312 B2 JP4240312 B2 JP 4240312B2 JP 2004341181 A JP2004341181 A JP 2004341181A JP 2004341181 A JP2004341181 A JP 2004341181A JP 4240312 B2 JP4240312 B2 JP 4240312B2
- Authority
- JP
- Japan
- Prior art keywords
- negative electrode
- active material
- material layer
- discharge
- electrode active
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
図1は、本発明の第1の実施の形態に係る二次電池の構成を表すものである。この二次電池は、いわゆるコイン型といわれるものであり、外装カップ11に収容された負極12と、外装缶13に収容された正極14とが、セパレータ15を介して積層されている。外装カップ11および外装缶13の周縁部は絶縁性のガスケット16を介してかしめることにより密閉されている。外装カップ11および外装缶13は、例えば、ステンレスあるいはアルミニウム(Al)などの金属によりそれぞれ構成されている。
図8は、本発明の第2の実施の形態に係る二次電池の構成を表すものである。この二次電池は、リード21,22が取り付けられた電極巻回体20をフィルム状の外装部材30の内部に収容したものであり、小型化,軽量化および薄型化が可能となっている。
図8,9に示した構造の二次電池を作製した。
負極活物質層23Bに予めリチウムを吸蔵させたことを除き、他は実施例1−2と同様にして二次電池を組み立てた。その際、リチウムは、負極活物質層23Bを成膜し、熱処理したのち、負極活物質層23Bの表面にリチウム金属を蒸着することにより吸蔵させた。吸蔵させるリチウムの量は、負極23の容量の5%とした。この場合、予め行った他の実験により、初期の充放電サイクルにおいては放電後にも負極23に電気化学的に活性なリチウムが残存することが確認された。
実施例3では、真空蒸着法に代えて、CVD法により負極活物質層23Bを成膜したのち、リチウムを吸蔵させ、更に熱処理を行ったことを除き、他は実施例1−1〜1−7と同様にして二次電池を組み立てた。実施例4では、真空蒸着法に代えて、スパッタリング法により負極活物質層23Bを成膜したのち、リチウムを吸蔵させ、更に熱処理を行ったことを除き、他は実施例1−1〜1−7と同様にして二次電池を組み立てた。
Claims (8)
- 正極および負極と共に電解質を備えた電池であって、
前記負極は、負極集電体に構成元素としてケイ素(Si)を含む負極活物質層が設けられており、
この負極活物質層は、放電後に電気化学的に活性なリチウム(Li)が残存している共に、複数の1次粒子が集合して形成された複数の2次粒子を有し、
この各2次粒子は、負極活物質層の厚み方向に深さを有する溝により、負極活物質層の面内方向において分離され、
前記1次粒子の一部は、前記溝により断裂された断裂粒子であり、
この断裂粒子は、前記負極活物質層が放電状態のとき、前記負極活物質層の少なくとも一部において、隣接する5つ以上の前記2次粒子における1つ当たりの平均で10個以上存在する電池。 - 前記2次粒子は、厚み方向の断面の少なくとも一部において、連続する10個のうち、厚み方向の長さよりもそれに対して垂直な方向の長さの方が長いものが、個数比で50%以上存在する請求項1記載の電池。
- 前記負極活物質層は、40サイクルを基準充放電とすると、基準充放電を繰り返した後の放電時における厚みが、基準充放電を行う前の放電時における厚みの1.7倍以下である請求項1記載の電池。
- 前記負極活物質層は、初回充放電前に予めリチウム(Li)を吸蔵している請求項1記載の電池。
- 正極および負極と共に電解質を備えた電池であって、
前記負極は、負極集電体に構成元素としてケイ素(Si)を含む負極活物質層が設けられており、
この負極活物質層は、放電後に電気化学的に活性なリチウム(Li)が残存していると共に、複数の1次粒子が集合して形成された複数の2次粒子を有し、
前記2次粒子は、前記負極活物質層が放電状態のとき、前記負極活物質層の少なくとも一部において、100μm×70μmの範囲内で100μmの長さの線を10μm間隔で8本引いた場合に、その1本当たりの直線上に存在する平均個数が、5個以上11個以下であり、
前記直線上に存在する前記2次粒子に含まれる1次粒子の数は、1つ当たりの平均で20個以上である電池。 - 前記2次粒子は、厚み方向の断面の少なくとも一部において、連続する10個のうち、厚み方向の長さよりもそれに対して垂直な方向の長さの方が長いものが、個数比で50%以上存在する請求項5記載の電池。
- 前記負極活物質層は、40サイクルを基準充放電とすると、基準充放電を数繰り返した後の放電時における厚みが、基準充放電を行う前の放電時における厚みの1.7倍以下である請求項5記載の電池。
- 前記負極活物質層は、初回充放電前に予めリチウム(Li)を吸蔵している請求項5記載の電池。