JP5063966B2 - 溶鋼の製造方法 - Google Patents
溶鋼の製造方法 Download PDFInfo
- Publication number
- JP5063966B2 JP5063966B2 JP2006241585A JP2006241585A JP5063966B2 JP 5063966 B2 JP5063966 B2 JP 5063966B2 JP 2006241585 A JP2006241585 A JP 2006241585A JP 2006241585 A JP2006241585 A JP 2006241585A JP 5063966 B2 JP5063966 B2 JP 5063966B2
- Authority
- JP
- Japan
- Prior art keywords
- treatment
- molten steel
- converter
- hot metal
- steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
[1]溶銑から連続鋳造に供する溶鋼を製造する方法であって、高炉から出銑された溶銑をそのまま転炉に装入し、冷鉄源を配合して溶銑比を83.1%以下とし、以降の精錬については、脱Si脱P処理を行った後、排滓を行い、その後同一転炉で、引き続き脱C処理を行い、吹き止め温度を1660℃以下とし、溶鋼を取鍋に出鋼してアーク加熱取鍋精錬装置で昇温を施し、脱Si脱Pは、前記転炉に装入した一連の工程の中でのみ行い、脱S処理は、前記アーク加熱取鍋精錬装置でのみ行うことを特徴とする溶鋼の製造方法。
[2]溶銑から連続鋳造に供する溶鋼を製造する方法であって、下記の(1)〜(5)の一連の工程を順に行うことを特徴とする上記[1]記載の溶鋼の製造方法。
(1)溶銑を転炉に装入し、該装入した溶銑に脱Si処理および脱P処理を施す工程
(2)上記(1)の工程で生成したスラグのみを排出し、溶銑を転炉内に残留させる工程
(3)転炉内に残留させた溶銑に脱C処理を施し、吹き止め温度を1660℃以下にして吹き止め溶鋼中P濃度を上記(1)の工程終了時の溶銑中P濃度以下に抑制し、取鍋に出鋼する工程
(4)出鋼中または出鋼後の溶鋼に、Alを添加して脱酸処理を施す工程
(5)Alを添加して脱酸処理を施した溶鋼に、アーク加熱取鍋精錬装置により、昇温を施すと共に、脱S処理を施す工程
[3]溶銑から連続鋳造に供する溶鋼を製造する方法であって、下記の(1)〜(6)の一連の工程を順に行うことを特徴とする上記[1]記載の溶鋼の製造方法。
(1)溶銑を転炉に装入し、該装入した溶銑に脱Si処理および脱P処理を施す工程
(2)上記(1)の工程で生成したスラグのみを排出し、溶銑を転炉内に残留させる工程
(3)転炉内に残留した溶銑に脱C処理を施し、吹き止め温度を1660℃以下にして吹き止め溶鋼中P濃度を上記(1)の工程終了時の溶銑中P濃度以下に抑制し、取鍋に出鋼する工程
(4)出鋼中または出鋼後の溶鋼に、Alを添加して脱酸処理を施す工程
(5)Alを添加して脱酸処理を施した溶鋼に、アーク加熱取鍋精錬装置により、昇温を施すと共に、脱S処理を施す工程
(6)昇温および脱S処理した溶鋼に真空脱ガス処理を施す工程
[4]脱C処理の吹き止め%Cを0.07%以上とすることを特徴とする上記[1]乃至[3]のいずれかに記載の溶鋼の製造方法。
[5]上記(4)の工程と(5)の工程の間に、溶鋼上のスラグを排出する工程を介在させることを特徴とする上記[2]乃至[4]のいずれかに記載の溶鋼の製造方法。
[6]真空脱ガス処理では、Al添加による昇熱を行わないことを特徴とする上記[2]記載の溶鋼の製造方法。
さらにLF処理後の温度を高めに制御することで次工程でRH処理を行う場合は、RHでのAl昇熱を行わないで処理が可能となり、アルミナ生成による介在物品質の悪化を回避できる。
Claims (6)
- 溶銑から連続鋳造に供する溶鋼を製造する方法であって、高炉から出銑された溶銑をそのまま転炉に装入し、冷鉄源を配合して溶銑比を83.1%以下とし、以降の精錬については、脱Si脱P処理を行った後、排滓を行い、その後同一転炉で、引き続き脱C処理を行い、吹き止め温度を1660℃以下とし、溶鋼を取鍋に出鋼してアーク加熱取鍋精錬装置で昇温を施し、脱Si脱Pは、前記転炉に装入した一連の工程の中でのみ行い、脱S処理は、前記アーク加熱取鍋精錬装置でのみ行うことを特徴とする溶鋼の製造方法。
- 溶銑から連続鋳造に供する溶鋼を製造する方法であって、下記の(1)〜(5)の一連の工程を順に行うことを特徴とする請求項1記載の溶鋼の製造方法。
(1)溶銑を転炉に装入し、該装入した溶銑に脱Si処理および脱P処理を施す工程
(2)上記(1)の工程で生成したスラグのみを排出し、溶銑を転炉内に残留させる工程
(3)転炉内に残留させた溶銑に脱C処理を施し、吹き止め温度を1660℃以下にして吹き止め溶鋼中P濃度を上記(1)の工程終了時の溶銑中P濃度以下に抑制し、取鍋に出鋼する工程
(4)出鋼中または出鋼後の溶鋼に、Alを添加して脱酸処理を施す工程
(5)Alを添加して脱酸処理を施した溶鋼に、アーク加熱取鍋精錬装置により、昇温を施すと共に、脱S処理を施す工程 - 溶銑から連続鋳造に供する溶鋼を製造する方法であって、下記の(1)〜(6)の一連の工程を順に行うことを特徴とする請求項1記載の溶鋼の製造方法。
(1)溶銑を転炉に装入し、該装入した溶銑に脱Si処理および脱P処理を施す工程
(2)上記(1)の工程で生成したスラグのみを排出し、溶銑を転炉内に残留させる工程
(3)転炉内に残留した溶銑に脱C処理を施し、吹き止め温度を1660℃以下にして吹き止め溶鋼中P濃度を上記(1)の工程終了時の溶銑中P濃度以下に抑制し、取鍋に出鋼する工程
(4)出鋼中または出鋼後の溶鋼に、Alを添加して脱酸処理を施す工程
(5)Alを添加して脱酸処理を施した溶鋼に、アーク加熱取鍋精錬装置により、昇温を施すと共に、脱S処理を施す工程
(6)昇温および脱S処理した溶鋼に真空脱ガス処理を施す工程 - 脱C処理の吹き止め%Cを0.07%以上とすることを特徴とする請求項1乃至3のいずれかに記載の溶鋼の製造方法。
- 上記(4)の工程と(5)の工程の間に、溶鋼上のスラグを排出する工程を介在させることを特徴とする請求項2乃至4のいずれかに記載の溶鋼の製造方法。
- 真空脱ガス処理では、Al添加による昇熱を行わないことを特徴とする請求項3記載の溶鋼の製造方法。