DE492339C - Verfahren zur Herstellung von Heizwiderstaenden - Google Patents
Verfahren zur Herstellung von HeizwiderstaendenInfo
- Publication number
- DE492339C DE492339C DEE37220D DEE0037220D DE492339C DE 492339 C DE492339 C DE 492339C DE E37220 D DEE37220 D DE E37220D DE E0037220 D DEE0037220 D DE E0037220D DE 492339 C DE492339 C DE 492339C
- Authority
- DE
- Germany
- Prior art keywords
- heating resistors
- production
- container
- heating
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Herstellung von Heizwiderständen Zusatz zum Patent 481796 -Das Hauptpatent betrifft ein Verfahren zur-Herstellung von elektrischen Heizwiderständen für hauswirtschaftliche und industrielle Zwecke aller Art, bei dem ein Gemisch von Kohle und Metalloxyden in Formkörper gepreßt und dann durch Einschalten in einen Stromkreis oder durch Erhitzen in einem Ofen gebrannt wird, bis sich auf dem Formkörper eine isolierende Schicht aus Metallcarbonaten bildet, die dann durch Umschließen mit einer Metallschicht vor Zersetzung geschützt wird.
- Es hat sich nun gezeigt, daß die Bildung der Carbonatschicht dadurch wesentlich gefördert werden kann, daß man den mit einer Carbonatschicht versehenen Heizkörper in einen luftdicht abgeschlossenen Metallbehälter derart einbaut, daß ein freier Raum zwischen dem Widerstandskörper und dem ihn umschließenden Behälter bestehen bleibt.
- Setzt man einen derart in einen Metallbehälter eingebauten Heizwiderstand unter Strom, so bildet sich nach Inbetriebsetzung in dem Behälterraum Metalldampf, der jeweilig dem Material, aus dem der Behälter besteht, entspricht und der sich gemäß dem bekannten Sherardisierungsvorgang auf der Carbonatschicht des Widerstandskörpers niederschlägt und Veranlassung zur Bildung von Metallcarbonaten gibt, die die bereits bestehende isolierende Schicht des Heizwiderstandes verfestigen und deren mechanische Eigenschaften wesentlich verbessern.
- Die so behandelten Heizwiderstände mit verfestigter Carbonatschicht werden in einen Schutzbehälter luftdicht eingeschlossen. Es kann aber auch der so behandelte Heizwiderstand gleich in der ihn umschließenden Metallhülle verbleiben, die ihrerseits die Metallcarbonate vor Zerstörung schützt. Heizkörper der zuletzt erwähnten Art eignen sich besonders zur Erwärmung- von Gas oder flüssigen Stoffen.
Claims (1)
- PATENTANSPRÜCHE: i. Abänderung des Verfahrens zur Herstellung von elektrischen Heizwiderständen nach Patent 481 796, dadurch gekennzeichnet, daß die Carbonatschicht des Formkörpers durch Erhitzen desselben in einem Metallbehälter, in den der Formkörper unter Freilassung eines Luftzwischenraumes in zentraler Lage luftdicht eingebaut wird, verfestigt wird, wonach der so behandelte Körper in einen Schutzbehälter luftdicht eingeschlossen wird. z. Nach dem Verfahren gemäß Anspruch i hergestellter Heizkörper, dadurch gekennzeichnet, daß der bei der Behandlung benutzte Metallbehälter selbst als dauernde Schutzhülle dient.