[go: up one dir, main page]

CN110630248B - Cementing quality evaluation device and method for well cementation two-interface - Google Patents

Cementing quality evaluation device and method for well cementation two-interface Download PDF

Info

Publication number
CN110630248B
CN110630248B CN201911037911.0A CN201911037911A CN110630248B CN 110630248 B CN110630248 B CN 110630248B CN 201911037911 A CN201911037911 A CN 201911037911A CN 110630248 B CN110630248 B CN 110630248B
Authority
CN
China
Prior art keywords
kettle body
core
interface
filter cake
fluid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201911037911.0A
Other languages
Chinese (zh)
Other versions
CN110630248A (en
Inventor
郭小阳
贾禛
李永刚
胡开利
毛德森
罗亮
江洪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southwest Petroleum University
Original Assignee
Southwest Petroleum University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southwest Petroleum University filed Critical Southwest Petroleum University
Priority to CN201911037911.0A priority Critical patent/CN110630248B/en
Publication of CN110630248A publication Critical patent/CN110630248A/en
Application granted granted Critical
Publication of CN110630248B publication Critical patent/CN110630248B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及固井二界面胶结质量评价装置及方法。该装置由圆柱形釜体1、岩心4、流体加压泵11、压力传感器12等组成,釜体有可拆卸的上密封盖2、下密封盖3,上密封盖有进液进气口6、泄压阀9和压力传感器12,下密封盖有出液出气口7;釜体内有岩心4,岩心表面有滤饼,岩心与釜体之间的环形空间内有水泥环。该方法包括:将带有滤饼的岩心抽真空,使岩心饱和树脂;将岩心放入釜体中,加入固井水泥浆,养护一定时间,岩心与釜体内壁之间形成水泥环;向釜体内注入流体;记录二界面滤饼发生破坏形成流体窜通通道时的破裂压力,得到二界面胶结系数。本发明能有效避免流体从岩心渗流,真实反映固井二界面的胶结质量,具有广阔的市场前景。

Figure 201911037911

The invention relates to a device and a method for evaluating the quality of cementing at the second interface of cementing. The device is composed of a cylindrical kettle body 1, a core 4, a fluid pressurizing pump 11, a pressure sensor 12, etc. The kettle body has a removable upper sealing cover 2, a lower sealing cover 3, and the upper sealing cover has a liquid inlet 6 , pressure relief valve 9 and pressure sensor 12, the lower sealing cover has a liquid outlet 7; there is a core 4 in the kettle body, a filter cake on the surface of the core, and a cement ring in the annular space between the core and the kettle body. The method includes: evacuating the core with filter cake to make the core saturated with resin; putting the core into the kettle body, adding cement slurry, curing for a certain period of time, and forming a cement ring between the core and the inner wall of the kettle; The fluid was injected into the body; the rupture pressure when the two-interface filter cake was destroyed to form a fluid channeling channel was recorded, and the two-interface cementation coefficient was obtained. The invention can effectively avoid the seepage of fluid from the core, truly reflect the cementation quality of the second interface of cementing, and has broad market prospects.

Figure 201911037911

Description

Cementing quality evaluation device and method for well cementation two-interface
Technical Field
The invention relates to a cementing quality evaluation device and method for a cementing two-interface in the field of oil and gas well exploration and development in the cementing process.
Background
For oil and gas well cementing and completion engineering, the cementing surface between a casing and a cement sheath is generally called a cementing interface, and the cementing surface between the cement sheath and a stratum is generally called a cementing interface. The cement sheath body and the first and second well cementation interfaces form a well cementation cement sheath sealing system. The quality of the well cementation and sealing system is directly related to the productivity and the service life of the oil and gas well and the development benefit of the oil field. If the interlayer packing capacity of the cement ring is reduced or even the interlayer packing effect is lost, formation fluid channeling and wellhead annulus pressure are induced, and normal oil and gas production is influenced. The main reason for causing the channeling is that the drilling fluid is lost to form a filter cake on the well wall in the drilling process, and the existence of the filter cake causes the well cementation cement paste to be not tightly cemented into a whole during well cementation, thereby providing a channel for the channeling of formation fluid and causing a series of well cementation problems.
The conventional method for evaluating the cementing quality of the two interfaces for indoor research has certain defects and shortcomings. Some scholars use a press machine to test the shear pressure (tregoring, warrior, CuiMaorong, and the like) required for the complete slippage of the rock core and the cement sheath in the presence of a filter cake, and a new method for evaluating the influence of the filter cake of the drilling fluid on the cementing quality of a well cementation second interface [ J ]. the natural gas industry, 2006,26(12):92-93), but the actual situation is that the slippage of the rock stratum and the cement sheath hardly occurs underground and the packing capacity of the second interface on formation fluid cannot be evaluated; some researchers consider the filter cake as a permeable substance, and use liquid to test seepage flow rate through a sample at one end of the core, so as to evaluate the cementing quality of the two interfaces (consider army, yankee, qin weng zhen, et al. research on the method for evaluating the cementing capacity of the two interfaces of well cementation, [ J ]. petroleum bulletin, 2008,29(3)), but the method does not consider that liquid can seep from the core, and also cannot reflect the cementing quality of the real two interfaces of well cementation.
Disclosure of Invention
The invention aims to provide a cementing quality evaluation device for a well cementation two-interface, which has reliable principle and simple and convenient operation, can effectively avoid the seepage of fluid from a rock core, truly reflects the cementing quality of the well cementation two-interface and has wide market prospect.
The invention also aims to provide a method for evaluating the cementing quality of the two well cementation interfaces by utilizing the device, which forms a fluid channeling channel on the two interfaces by pressurizing the fluid to penetrate the two interfaces with filter cakes, and obtains the cementing coefficient of the two interfaces according to the fluid channeling pressure of the two interfaces so as to evaluate the cementing quality of the two interfaces.
In order to achieve the technical purpose, the invention adopts the following technical scheme.
The cementing quality evaluation device for the well cementation two-interface consists of a cylindrical kettle body, a rock core, a heating sleeve, a heat insulation sleeve, a fluid pressure pump, a pressure sensor and the like. The inner diameter of the kettle body from the top to the bottom is gradually reduced, the inner wall of the kettle body forms an inverted circular truncated cone shape, a rock core is arranged in the kettle body, the rock core is plastically packaged after a filter cake is formed on the surface of the rock core, and a cement sheath is arranged between the rock core and the inner wall of the kettle body. The top of the kettle body is provided with a detachable upper sealing cover, the upper sealing cover is provided with a liquid inlet, a pressure release valve and a pressure sensor which are communicated with the inside of the kettle body respectively, the liquid inlet is connected with a fluid pressure pump through a pipeline, and the pipeline is provided with a one-way valve communicated to the inside of the kettle body through the fluid pressure pump. The bottom of the kettle body is provided with a detachable lower sealing cover, the rock core is placed on the inner surface of the lower sealing cover, the lower sealing cover is provided with a liquid outlet communicated with the inside of the kettle body, the liquid outlet is arranged between the rock core and the inner wall of the kettle body, and the outer wall of the kettle body is provided with a heating sleeve.
Preferably, the upper sealing cover is of an inverted U shape, a first sealing ring is arranged between the inner side wall of the upper sealing cover and the outer wall of the top of the kettle body, and the inner side wall of the upper sealing cover is in threaded connection with the outer wall of the kettle body.
Preferably, the lower sealing cover is U-shaped, a second sealing ring is arranged between the inner side wall of the lower sealing cover and the outer wall of the bottom of the kettle body, and the inner side wall of the lower sealing cover is in threaded connection with the outer wall of the kettle body.
Preferably, the liquid outlet air outlets are at least two and are uniformly distributed between the rock core and the inner wall of the bottom of the kettle body.
Preferably, the included angle formed by the inner wall of the top of the kettle body and the outer wall of the top of the kettle body is 7-8 degrees.
The method for evaluating the cementing quality of the well cementation second interface by using the device sequentially comprises the following steps:
(1) placing the rock core in a filter cake pressing device to form a compact drilling fluid filter cake on the surface of the rock core;
(2) placing the rock core with the filter cake in a vacuum tank, and dripping resin into the rock core while vacuumizing to saturate the rock core with resin, wherein the resin can be coagulated together with cement slurry without affecting the structure of the filter cake;
(3) placing the core into a kettle body, adding well cementation cement slurry into an annular space between the core and the kettle body, and maintaining for a certain time under the experimental requirement condition to form a cement sheath between the core and the inner wall of the kettle body;
(4) a fluid pressurizing pump injects fluid into the kettle body through a one-way valve and a liquid inlet, when the pressure is raised to a certain value, the fluid penetrates through two interfaces where filter cakes exist, a fluid channeling channel is formed on the two interfaces, and the fluid is discharged through a liquid outlet and a gas outlet;
(5) recording the fracture pressure when the filter cake of the second interface is damaged to form a fluid channeling channel to obtain a cementation coefficient of the second interface, thereby evaluating the cementation quality of the second interface, wherein the calculation formula of the cementation coefficient of the second interface is as follows:
Figure BDA0002252049460000021
in the formula, gamma is a two-interface cementation coefficient and is dimensionless;
r1is the outer diameter of the core containing the filter cake, cm;
r2the outer diameter of the core is cm without filter cake;
Pwrupture pressure, MPa;
μ1the friction coefficient between the interface and the set cement is dimensionless;
μ2the friction coefficient between the two interfaces and the rock core is dimensionless;
theta is the included angle between the two interfaces and the horizontal plane, and theta is more than 0 degree and less than 180 degrees.
The fracture pressure is the fluid channeling pressure in the filter cake state, the two-interface cementation quality is in direct proportion to the two-interface cementation coefficient, namely the larger the two-interface cementation coefficient is, the better the two-interface cementation quality is, and conversely, the smaller the two-interface cementation coefficient is, the worse the two-interface cementation quality is.
Compared with the prior art, the invention has the beneficial effects that:
(1) the invention truly simulates the bottom hole environment during well cementation under the heating and pressurizing environment, and forms a fluid channeling channel at two interfaces through the fracture of a filter cake.
(2) The filter cake is used as a weak layer of the two interfaces, and the pressure value is brought into a mathematical model to be calculated as a basis for visually expressing the cementation condition of the two interfaces, so that the actual condition of the two interfaces is closer to the actual condition in a well.
(3) The inner diameter of the kettle body is gradually reduced from the top to the bottom, and the inner wall of the kettle body forms an inverted circular truncated cone shape, so that the cement stone can be prevented from integrally slipping and is consistent with the actual underground condition; the included angle formed by the inner wall of the top of the kettle body and the outer wall of the top of the kettle body is 7-8 degrees, so that the anti-falling effect is better.
(4) By forming the core with the filter cake and plastic package, the core after plastic package can avoid fluid seepage from the core, so that the test result is more accurate.
Drawings
FIG. 1 is a schematic structural diagram of a cementing quality evaluation device of a cementing two-interface.
Fig. 2 is a schematic structural diagram of the sealing cover on the device.
FIG. 3 is a diagram of the stress state of the two-interface bond.
Reference numbers in the figures:
1-kettle body, 2-upper sealing cover, 3-lower sealing cover, 4-core, 5-heating jacket, 6-liquid inlet, 7-liquid outlet, 8-heat preservation jacket, 9-pressure release valve, 10-one-way valve, 11-fluid pressure pump, 12-pressure sensor, 13-pressure recorder, 14-sealing ring III and 15-bolt.
Detailed Description
The present invention is further described below with reference to the accompanying drawings so as to facilitate understanding of the present invention by those skilled in the art. It is to be understood that the invention is not limited in scope to the specific embodiments, but is intended to cover various modifications within the spirit and scope of the invention as defined and defined by the appended claims, as would be apparent to one of ordinary skill in the art.
As shown in fig. 1-2.
The cementing quality evaluation device for the well cementation two-interface consists of a cylindrical kettle body 1, a rock core 4, a heating sleeve 5, a heat insulation sleeve 8, a fluid pressure pump 11, a pressure sensor 12 and a pressure recorder 13.
The inner diameter of the kettle body 1 from the top to the bottom is gradually reduced, the inner wall of the kettle body forms an inverted circular truncated cone shape, and the kettle body is provided with an upper sealing cover 2 and a lower sealing cover 3 which are detachable; the upper sealing cover 2 is provided with a liquid inlet 6, a pressure release valve 9 and a pressure sensor 12, the liquid inlet is connected with a fluid pressure pump 11 through a one-way valve 10 and a pipeline, and the pressure sensor is connected with a pressure recorder 13; the lower sealing cover 3 is provided with a liquid outlet 7; a rock core 4 is arranged in the kettle body, the rock core is placed on the inner surface of the lower sealing cover, a filter cake is arranged on the surface of the rock core, and a cement sheath is arranged in an annular space between the rock core and the kettle body; the kettle body is externally provided with a heating jacket 5 and a heat preservation jacket 8.
The inner wall of the top of the kettle body and the outer wall of the top of the kettle body form an included angle of 7-8 degrees.
And at least two liquid outlet air outlets 7 are arranged and are uniformly distributed between the rock core and the inner wall of the kettle body.
The heating device is characterized in that an electric heating wire is arranged in the heating sleeve 5 and connected with a heating control device, a heat preservation sleeve 8 is arranged on the outer surface of the heating sleeve 5, and the heat preservation sleeve 8 is made of glass wool or rock wool.
The upper sealing cover 2 is of an inverted U shape, a first sealing ring is arranged between the inner side wall of the upper sealing cover and the outer wall of the top of the kettle body 1, and the inner side wall of the upper sealing cover is in threaded connection with the outer wall of the kettle body; the lower sealing cover 3 is U-shaped, a sealing ring II is arranged between the inner side wall of the lower sealing cover and the outer wall of the bottom of the kettle body 1, and the inner side wall of the lower sealing cover is in threaded connection with the outer wall of the kettle body.
As shown in fig. 2, the upper sealing cover 2 is provided with a downward positioning protrusion, the top of the kettle body 1 is provided with a positioning groove matched with the positioning protrusion, a third sealing ring 14 is arranged in the positioning groove, and the upper sealing cover is sealed with the top end of the kettle body through a bolt 15.
The invention evaluates the cementation quality of the two interfaces through the cementation coefficient of the two interfaces, and the calculation formula of the cementation coefficient of the two interfaces is as follows:
Figure BDA0002252049460000041
in the formula, gamma is a two-interface cementation coefficient and is dimensionless;
r1is the outer diameter of the core containing the filter cake, cm;
r2the outer diameter of the core is cm without filter cake;
Pwrupture pressure, MPa;
μ1the friction coefficient between the interface and the set cement is dimensionless;
μ2the friction coefficient between the two interfaces and the rock core is dimensionless;
theta is the included angle between the two interfaces and the horizontal plane, and theta is more than 0 degree and less than 180 degrees.
The derivation of this equation is as follows:
taking the cement sheath as a research object, and taking the two-interface cementing interface for stress analysis, thereby listing a balance equation of the two-interface cementing stress interface (see figure 3).
As can be seen from FIG. 3, the two interfaces have two stress directions, wherein the downward stress interface, i.e. the stress interface equation in the pressurizing direction, is as follows:
Fw=Pw×Ac (2)
the upward force, i.e. the resistance in the pressurizing direction, is divided into the following parts:
the vertical filter cake reaction force interface equation is:
F=(Pw-Pwsinθ)×Ac (3)
the internal stress interface equation of the cementing action is as follows:
Fγ=γC1 (4)
the interfacial equation of the cementing friction force with the cement sheath is as follows:
F1=(Pw-Pwsinθ)×C1μ1 (5)
the equation of the cementing friction force section of the rock core is as follows:
F2=PwC2μ2 (6)
at the instant of filter cake rupture, the forces on both sides are balanced, and the equations (2), (3), (4), (5) and (6) can be derived:
(Pw-Pwsinθ)Ac-γC1+(Pw-Pwsinθ)C1μ1+PwC2μ2=PwAc (7)
expanding the formula (7) to obtain:
Figure BDA0002252049460000051
in the formula: a. thecIs cement sheath and filter cakeCemented stressed cross-section, m2;C1The length of the lateral arc of the cement ring is m; c2The arc length of the side surface of the rock core is m; n is central angle degree; r is1The position contains the outer diameter of the filter cake, m; r is2Is the inner diameter of the filter cake free, m; gamma is a two-interface cementation coefficient and is dimensionless; p is a radical ofwRupture pressure, MPa; mu.s1The friction coefficient between the interface and the set cement is dimensionless; mu.s2The friction coefficient between the two interfaces and the rock core is dimensionless; theta is the included angle between the two interfaces and the horizontal plane, and theta is more than 0 degree and less than 180 degrees.
The formula (8) is simplified to obtain:
Figure BDA0002252049460000052
the relationship between the two interfacial bond coefficients and the fracture pressure is thus obtained:
Figure BDA0002252049460000053

Claims (1)

1. the device comprises a cylindrical kettle body (1), a rock core (4), a heating sleeve (5), a heat insulation sleeve (8), a fluid pressure pump (11), a pressure sensor (12) and a pressure recorder (13), wherein the inner diameter of the kettle body (1) from the top to the bottom is gradually reduced, the inner wall of the kettle body forms an inverted circular truncated cone shape, and the kettle body is provided with an upper sealing cover (2) and a lower sealing cover (3) which are detachable; the upper sealing cover is provided with a liquid inlet (6), a pressure release valve (9) and a pressure sensor (12), the liquid inlet is connected with a fluid pressure pump (11) through a one-way valve (10) and a pipeline, and the pressure sensor is connected with a pressure recorder (13); the lower sealing cover is provided with a liquid outlet (7); a rock core (4) is arranged in the kettle body, the rock core is placed on the inner surface of the lower sealing cover, a filter cake is arranged on the surface of the rock core, and a cement sheath is arranged in an annular space between the rock core and the kettle body; a heating sleeve (5) and a heat-insulating sleeve (8) are arranged outside the kettle body; the inner wall of the top of the kettle body and the outer wall of the top of the kettle body form an included angle of 7-8 degrees; the method comprises the following steps of:
(1) placing the rock core in a filter cake pressing device to form a compact drilling fluid filter cake on the surface of the rock core;
(2) placing the rock core with the filter cake in a vacuum tank, and dripping resin into the rock core while vacuumizing to saturate the rock core with resin, wherein the resin is coagulated together with cement slurry without affecting the structure of the filter cake;
(3) placing the core into a kettle body, adding well cementation cement slurry into an annular space between the core and the kettle body, and maintaining under the experimental requirement condition to form a cement sheath between the core and the inner wall of the kettle body;
(4) a fluid pressurizing pump injects fluid into the kettle body through a one-way valve and a liquid inlet, when the pressure is raised to a certain value, the fluid penetrates through two interfaces where filter cakes exist, a fluid channeling channel is formed on the two interfaces, and the fluid is discharged through a liquid outlet and a gas outlet;
(5) recording the fracture pressure when the filter cake of the second interface is damaged to form a fluid channeling channel to obtain a cementation coefficient of the second interface, thereby evaluating the cementation quality of the second interface, wherein the calculation formula of the cementation coefficient of the second interface is as follows:
Figure FDA0003352498020000011
in the formula, gamma is a two-interface cementation coefficient and is dimensionless;
r1is the outer diameter of the core containing the filter cake, cm;
r2the outer diameter of the core is cm without filter cake;
Pwrupture pressure, MPa;
μ1the friction coefficient between the interface and the set cement is dimensionless;
μ2the friction coefficient between the two interfaces and the rock core is dimensionless;
theta is the included angle between the two interfaces and the horizontal plane, and theta is more than 0 degree and less than 180 degrees.
CN201911037911.0A 2019-10-29 2019-10-29 Cementing quality evaluation device and method for well cementation two-interface Expired - Fee Related CN110630248B (en)