US20160088739A1 - Peripheral circuit of touch panel and manufacturing method thereof - Google Patents
Peripheral circuit of touch panel and manufacturing method thereof Download PDFInfo
- Publication number
- US20160088739A1 US20160088739A1 US14/955,050 US201514955050A US2016088739A1 US 20160088739 A1 US20160088739 A1 US 20160088739A1 US 201514955050 A US201514955050 A US 201514955050A US 2016088739 A1 US2016088739 A1 US 2016088739A1
- Authority
- US
- United States
- Prior art keywords
- conductive material
- peripheral circuit
- radiation curable
- substrate
- touch panel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A method for manufacturing a peripheral circuit of a touch panel includes: printing a radiation curable conductive material on a substrate having a transparent conductive pattern; irradiating the radiation curable conductive material with a radiated ray, in order to cure parts of the radiation curable conductive material; and removing uncured parts of the radiation curable conductive material, in order to form the peripheral circuit.
Description
- This application is a divisional of application Ser. No. 13/858,913, filed on Apr. 8, 2013 and entitled “PERIPHERAL CIRCUIT OF TOUCH PANEL AND MANUFACTURING METHOD THEREOF”, the contents of which are incorporated herein in their entirety.
- 1. Field of the Invention
- The present invention relates to a peripheral circuit of a touch panel and a manufacturing method thereof.
- 2. Description of the Prior Art
- Various types of touch technology are widely applied in electronic products. For example, in mobile phones and tablets, touch panels are often utilized as an input interface. The user can use their hand to directly contact the surface of the touch panel for performing operations, or slide their hand on the surface of the touch panel to control a mouse or perform a hand-written input. A display together with the touch panel may also show a virtual keyboard for the user, and the user can input characters via corresponding keys on the virtual keyboard.
- The touch panel may be divided into various types such as a resistive touch panel, capacitive touch panel, ultrasonic touch panel and infrared ray touch panel. Among these touch panels, the resistive touch panel is the most commonly utilized. The resistive touch panel may mainly be divided into a four-wire touch panel, five-wire touch panel, six-wire touch panel and eight-wire touch panel. Since the four-wire touch panel is more mature in consideration of cost and technology, it is currently the most widely manufactured. The capacitive touch panel, however, can sense a light-touch, and thus is more convenient for utilization. In addition, the capacitive touch panel rarely wears down due to finger contact. It is also more stable and has a longer life than the resistive touch panel. For these reasons, the capacitive touch panel is gradually replacing the resistive touch panel as the most commonly utilized touch panel applied in electronic products.
- The touch panel includes a substrate, a transparent conductive layer formed on the substrate, a peripheral circuit and an insulating layer. The touch panel may further include a connected flexible printed circuit board (FPC). The peripheral circuit is connected with the transparent conductive layer and the FPC. The peripheral circuit can be formed by a photolithography process. The conventional photolithography process includes the following steps: first, a metal layer is formed on the substrate by deposition or electrode planting; then a photoresist layer is applied on the metal layer, and selective exposure is performed on the photoresist layer; then developing is performed on the photoresist layer after exposure with a developer, to obtain a patterned photoresist layer; finally, the patterned photoresist layer is utilized as a mask to etch the metal layer, in order to form a conductive circuit on the substrate.
- When the conventional photolithography process is implemented, the steps are complex and need to utilize a large number of chemicals, such that the cost is high and the process may not comply with the requirements and trends of environmental protection emphasized in modern science and technology.
- In order to solve the problems of manufacturing the peripheral circuit with the conventional photolithography process, the industry provides a manufacturing method for forming the peripheral circuit with a printing process. This method prints a thermal setting conductive adhesive on the substrate, and then cures and bakes the thermal setting conductive adhesive with a high temperature, in order to form the peripheral circuit. This manufacturing method benefits from a simplified process in comparison to the photolithography process, but the peripheral circuit formed by utilizing the printing process may come off since the adherence degree of the printing ink connected with the substrate is low, which causes the conductive circuit to be cut off. In addition, this method may only be applied in a conductive pattern and circuit with a thicker wire width and a greater wire distance, and cannot effectively enhance the density of circuit disposition.
- Therefore, how to provide a peripheral circuit of a touch panel and a manufacturing method thereof which are capable of reducing wire width or wire distance in order to achieve higher integration while complying with environmental protection requirements becomes an important issue.
- It is an objective of the present invention to provide a peripheral circuit of a touch panel that can be manufactured using a simplified process while maintaining the adherence degree and electronic characteristics, and a manufacturing method thereof, which can reduce wire width or wire distance in order to achieve higher integration while complying with environmental protection requirements.
- In order to achieve the above objectives, a method of manufacturing a peripheral circuit of a touch panel according to the present invention comprises the following steps: printing a radiation curable conductive material on a substrate having a transparent conductive pattern; irradiating the radiation curable conductive material with a radiated ray, in order to cure parts of the radiation curable conductive material; and removing uncured parts of the radiation curable conductive material, in order to form the peripheral circuit.
- According to an embodiment of the present invention, a wavelength of the radiated ray is approximately within a range from 230 nanometers to 600 nanometers.
- According to an embodiment of the present invention, the transparent conductive pattern is connected with the peripheral circuit.
- According to an embodiment of the present invention, a wire width of the peripheral circuit is less than or equal to about 70 micrometers.
- According to an embodiment of the present invention, the radiation curable conductive material comprises radiation curable silver glue, radiation curable silver paste or radiation curable ink.
- According to an embodiment of the present invention, the step of curing parts of the radiation curable conductive material comprises selectively curing the radiation curable conductive material by disposing a photomask on the radiation curable conductive material, wherein a material of the photomask comprises glass, quartz or polyethylene terephthalate (PET).
- According to an embodiment of the present invention, the radiated ray irradiates the radiation curable conductive material with at least two different wavelength ranges.
- According to an embodiment of the present invention, the radiation curable conductive material is printed on the substrate by screen printing.
- According to an embodiment of the present invention, the substrate is a transparent plastic substrate, a transparent glass substrate or a PET thin film substrate.
- In order to achieve the above objectives, a touch panel according to the present invention comprises a substrate and a peripheral circuit. The substrate has a transparent conductive pattern. The peripheral circuit is connected with the transparent conductive pattern. A material of the peripheral circuit comprises a radiation curable conductive material.
- According to an embodiment of the present invention, a wire width of the peripheral circuit is less than or equal to about 70 micrometers.
- According to an embodiment of the present invention, the radiation curable conductive material comprises radiation curable silver glue, radiation curable silver paste or radiation curable ink.
- According to an embodiment of the present invention, the substrate is a transparent plastic substrate, a transparent glass substrate or a PET thin film substrate.
- In order to achieve the above objectives, a peripheral circuit of a touch panel according to the present invention is manufactured using the above methods.
- In order to achieve the above objectives, a method of manufacturing a peripheral circuit of another touch panel according to the present invention comprises the following steps: printing a photosensitive conductive material on a substrate by screen printing; disposing a photomask on the photosensitive conductive material; irradiating the photosensitive conductive material with a beam, in order to cure parts of the photosensitive conductive material; and etching uncured parts of the photosensitive conductive material, in order to form the peripheral circuit.
- According to an embodiment of the present invention, the substrate is a transparent substrate.
- According to an embodiment of the present invention, the photosensitive conductive material comprises a plurality of silver particles, and a diameter of the plurality of silver particles is within a range from 1 micrometer to 10 micrometers.
- According to an embodiment of the present invention, a wire width of the peripheral circuit is less than 100 micrometers.
- According to an embodiment of the present invention, a material of the photomask comprises glass, quartz or PET.
- According to an embodiment of the present invention, the step of etching is performed by wet etching.
- According to an embodiment of the present invention, the method further comprises connecting the peripheral circuit with a flexible printed circuit board (FPC) by using a conductive adhesive.
- According to an embodiment of the present invention, the conductive adhesive is an anisotropic conductive film (ACF) or anisotropic conductive paste (ACP).
- According to an embodiment of the present invention, the method further comprises disposing a protective film on the peripheral circuit.
- According to an embodiment of the present invention, the step of disposing the protective film on the peripheral circuit comprises disposing the protective film utilizing a pasting method or a printing method.
- According to an embodiment of the present invention, the beam comprises a visible light with a wavelength within a range from 350 micrometers to 780 micrometers.
- As mentioned above, the peripheral circuit of the touch panel and the manufacturing method thereof according to one exemplary embodiment of the present invention utilizes radiation curable conductive material as a printing material to be printed on the substrate, cures parts of the radiation curable conductive material, and then removes uncured parts of the radiation curable conductive material in order to form the peripheral circuit. These steps can realize the reduction of wire width or wire distance in order to achieve higher integration while complying with environmental protection requirements. The peripheral circuit of the touch panel and the manufacturing method thereof according to another exemplary embodiment of the present invention utilizes photosensitive conductive material as a printing material to be printed on the substrate, cures parts of the photosensitive conductive material, and then etches uncured parts of the photosensitive conductive material in order to form the peripheral circuit. These steps can realize the simplification of the manufacturing process while retaining the adherence degree and electronic characteristics. For the implementation of the present invention, the manufacturing method enjoys the benefits of screen printing and exposure/development; hence power consumption problems can be avoided, as opposed to the conventional thermal curing process where the power consumption is generated by using an oven for a long time. Therefore, the environmental protection requirements can also be met.
- In summary, the peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention enjoy the benefits of screen printing and exposure/development, which not only can manufacture the touch panel at a low cost and high speed, but can also provide the touch panel with the advantages of small wire width and wire distance. This method is therefore suitable for smaller electronic devices. The peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention can enlarge the visible area, which provides greater convenience for the user.
- These and other objectives of the present invention will no doubt become obvious to those of ordinary skill in the art after reading the following detailed description of the preferred embodiment that is illustrated in the various figures and drawings.
-
FIG. 1A andFIG. 1B are schematic diagrams of a touch panel according to a preferable embodiment of the present invention. -
FIG. 2A andFIG. 2B are schematic diagrams of another touch panel according to a preferable embodiment of the present invention. -
FIG. 3 is a block diagram of a method of manufacturing the peripheral circuit of the touch panel according to a preferable embodiment of the present invention. -
FIG. 4A toFIG. 4D are schematic diagrams of another touch panel according to a preferable embodiment of the present invention. -
FIG. 5 is a block diagram of a method of manufacturing the peripheral circuit of the touch panel according to a preferable embodiment of the present invention. -
FIG. 6A andFIG. 6B are schematic diagrams of another touch panel according to a preferable embodiment of the present invention. - In the following, the description refers to illustrations related to a peripheral circuit of a touch panel and a manufacturing method thereof according to preferable embodiments of the present invention, where the same elements are denoted by the same reference symbols.
- Please refer to
FIG. 1A andFIG. 1B , which are schematic diagrams of atouch panel 1 according to a preferable embodiment of the present invention. Thetouch panel 1 includes asubstrate 11 and aperipheral circuit 12. Thesubstrate 11 can be, for example, a transparent plastic substrate or a transparent glass substrate. In addition, thesubstrate 11 can also be a polyethylene terephthalate (PET) thin film substrate or other thin film-shaped substrates. Thesubstrate 11 has an outer surface S1 and an inner surface S2. The user usually views thetouch panel 1 from the outer surface S1 side, and performs various kinds of operations on the outer surface S1. Other structures and elements of thetouch panel 1 are disposed on the inner surface S2 side of thesubstrate 11. - The inner surface S2 of the
substrate 11 includes a transparentconductive pattern 111, a maskingdecoration layer 112 and aconductive layer 113. The transparentconductive pattern 111, disposed on the inner surface S2 of thesubstrate 11, is utilized for defining a touch sensing circuit. The material of the transparentconductive pattern 111 can be, for example, indium tin oxide (ITO). The maskingdecoration layer 112 is disposed next to a terminal of the transparentconductive pattern 111, and the material of the maskingdecoration layer 112 can be, for example, an insulating material or insulating ink with various colors. Theconductive layer 113 is disposed on the maskingdecoration layer 112 and the transparentconductive pattern 111, and extends from a terminal of the transparentconductive pattern 111 to the maskingdecoration layer 112. The material of theconductive layer 113 includes a transparent high molecular conductive material or ITO, and theconductive layer 113 maybe formed on the maskingdecoration layer 112 and the transparentconductive pattern 111 by printing. - The
peripheral circuit 12 is disposed on theconductive layer 113 and the maskingdecoration layer 112, and extends to theconductive layer 113 without exceeding an edge of the maskingdecoration layer 112. In other words, projection of theperipheral circuit 12 is located on the maskingdecoration layer 112, or is flush with the edge of the maskingdecoration layer 112. The material of theperipheral circuit 12 is a radiation curable conductive material, which can be, for example, radiation curable silver glue, radiation curable silver paste or radiation curable ink. Fine circuits of theperipheral circuit 12 are defined by using screen printing equipment together with a screen with fine wires, and are formed on the transparentconductive pattern 111 and the maskingdecoration layer 112 by printing. Please note that, in the above process, the radiation curable conductive material may preferably be disposed as block-shaped circuits on the substrate printed directly by the printing equipment. In this process, no fine wire mesh needs to be utilized, and the printed block-shaped circuits may further be utilized for forming finer circuits in cooperation with lithography technique. Such implementation allows the wire width of theperipheral circuit 12 to be less than or equal to 70 micrometers, and reduces the requirements for high precision screens, which favors cost reduction and quality enhancement. The following paragraphs will detail how to cooperate with the lithography technique, and the photolithography technique in particular. - The above radiation curable conductive material is not limited to be composed of some special elements. The radiation curable conductive can be a material which has a certain conductivity and will be dried or cured after being irradiated by a short wavelength radiated ray. Specifically, the radiation curable conductive material can be an ultraviolet radiation cured conductive material or an ultraviolet radiation dried conductive material, which is liquid or adherent when printed, where parts of the material which are irradiated by the ultraviolet radiation will be dried or cured immediately and adhered to the substrate. The non-irradiated parts will still be liquid or adherent, and can be removed easily. In addition, conductive materials which are dried or cured when irradiated by radiated rays with other wavelengths may also be utilized. The above is therefore not limited to ultraviolet radiation.
- As shown in
FIG. 1B , thetouch panel 1 may further include an insulatinglayer 13 and aconductive adhesive 14. The insulatinglayer 13 covers parts of theperipheral circuit 12 by screen printing, in order to prevent theperipheral circuit 12 from being oxidized due to exposure to the air. Theconductive adhesive 14 is adhered to theperipheral circuit 12 and a pin P of a flexible printed circuit board (FPC), such that the touch sensing signals generated by the transparentconductive pattern 111 can be transmitted to the pin P of the FPC via theconductive layer 113, theperipheral circuit 12 and theconductive adhesive 14. In other embodiments, theconductive adhesive 14 may be an anisotropic conductive film (ACF) or anisotropic conductive paste (ACP). When the touch panel is applied, the insulating layer may also be ignored, which is not limited herein. - Please note that the transparent
conductive pattern 111 in this embodiment is formed on thesubstrate 11 directly, and thesubstrate 11 belongs to a type having touch sensing functions and a cover plate simultaneously. The application is not limited to this, and various types of touch panels can be applied according to the present invention. For example, a substrate with a two-layer structure composed of two substrates may also be applied in the present invention, where the top layer substrate and the bottom layer substrate both possess the transparent conductive pattern. - Please refer to
FIG. 2A andFIG. 2B , which are schematic diagrams of anothertouch panel 2 according to a preferable embodiment of the present invention. Thetouch panel 2 includes asubstrate 21 and aperipheral circuit 22. Thesubstrate 21 can be a transparent substrate, which can be, for example, a plastic substrate or a glass substrate. Thesubstrate 21 may also be other types such as a PET thin film substrate or other thin film-shaped substrates. The user usually views thetouch panel 2 from the outer surface S1 side of thesubstrate 21 and performs various kinds of operations on the outer surface S1. Other structures and elements of thetouch panel 2 are disposed on the inner surface S2 side of thesubstrate 21. - The inner surface S2 of the
substrate 21 includes a transparentconductive pattern 211, a maskingdecoration layer 212 and aconductive layer 213. The transparentconductive pattern 211 is utilized for defining a touch sensing circuit. The material of the transparentconductive pattern 211 can be, for example, ITO. Theconductive layer 213 is disposed on thesubstrate 21, and extends to a terminal of the transparentconductive pattern 211 to cover parts of the transparentconductive pattern 211. The maskingdecoration layer 212 is disposed on thesubstrate 21 and theconductive layer 213 and extends to theconductive layer 213. The maskingdecoration layer 212 possesses an opening H on theconductive layer 213, where the maskingdecoration layer 212 is disposed without exceeding an edge of theconductive layer 213. - The material of the
conductive layer 213 includes conductive carbon paste, and the material of the maskingdecoration layer 212 can be, for example, an insulating material or insulating ink with various colors. For color selection of the maskingdecoration layer 212, a color similar to that of theconductive layer 213 is preferably selected to be utilized, such that the user may not feel the difference of color between the maskingdecoration layer 212 and theconductive layer 213 when viewing the outer surface S1 of thetouch panel 2. In addition, theconductive layer 213 and the maskingdecoration layer 212 may be formed on thesubstrate 21 by printing. - The
peripheral circuit 22 is disposed on the maskingdecoration layer 212, and a part of theperipheral circuit 22 is filled in the opening H and coupled to theconductive layer 213. The material of theperipheral circuit 22 is a radiation curable conductive material, which can be, for example, radiation curable silver glue, radiation curable silver paste or radiation curable ink. Theperipheral circuit 12 is formed on the maskingdecoration layer 212 by printing and irradiating of a radiated ray. - As shown in
FIG. 2B , thetouch panel 2 further includes an insulatinglayer 23 and aconductive adhesive 24. The insulatinglayer 23 is disposed on theperipheral circuit 22, in order to prevent theperipheral circuit 22 from being oxidized due to exposure to the air. Theconductive adhesive 24 is adhered to theperipheral circuit 22 and a pin P of an FPC. The pin P is coupled to theconductive layer 213 via theconductive adhesive 24 and theperipheral circuit 22, in order to receive the touch sensing signals generated by the transparentconductive pattern 211, where the conductive adhesive 24 can be ACF or ACP. In other embodiments, the insulating layer may also be ignored, which is not limited herein. - Please refer to the block diagram shown in
FIG. 3 together withFIG. 1A , which illustrates a method of manufacturing the peripheral circuit of the touch panel according to a preferable embodiment of the present invention. This method can be applied for manufacturing the abovementionedperipheral circuit 12 of thetouch panel 1. The steps of the manufacturing method include Steps S31-S33. - Step S31 is printing a radiation curable conductive material on the
substrate 11 having the transparentconductive pattern 111. For the implementation of Step S31, at least two methods may be included. One of the methods is forming the radiation curable conductive material on the transparentconductive pattern 111 and the maskingdecoration layer 112 of thesubstrate 11 by printing (especially screen printing) by using screen printing equipment in cooperation with a fine wire mesh, wherein the fine wires printed on the radiation curable conductive material are processed by follow-up radiation, in order to form the finerperipheral circuit 12. The second preferable method is printing the radiation curable conductive material on thesubstrate 11 directly by blocks or areas where the fine wire mesh is not utilized, and the follow-up operations are then performed on the formed pattern, in order to form a plurality of wires of theperipheral circuit 12. - The abovementioned radiation curable conductive material can be radiation curable silver glue, radiation curable silver paste or radiation curable ink. The
substrate 11 is a transparent substrate, which can be, for example, a plastic substrate or a glass substrate. In other cases, thesubstrate 11 may also be PET thin film substrate or other thin film-shaped substrates. The material of the transparentconductive pattern 111 can be, for example, ITO, and the material of the maskingdecoration layer 112 can be, for example, an insulating material or insulating ink with various colors. The transparentconductive pattern 111 may first be formed on thesubstrate 11 by sputtering and etching, and the maskingdecoration layer 112 may be disposed on thesubstrate 11 by deposition or printing according to its material. - Step S32 is irradiating the radiation curable conductive material with a radiated ray, in order to cure parts of the radiation curable conductive material. For the implementation of Step S32, the radiation curable conductive material is irradiated by a radiated ray having a wavelength within a range from 230 nanometers to 600 nanometers. In order to regulate the position of the circuit layout, the method for curing parts of the radiation curable conductive material is performed by disposing a photomask on the radiation curable conductive material, which allows the radiated ray to cure the radiation curable conductive material selectively according to product requirements or circuit designs. The material of the above photomask includes glass, quartz or PET, and the form of photomask can be, but is not limited to, positive or negative, which is determined according to the nature of the material and the structural requirements of the
peripheral circuit 12. - In order to enhance the integration of the radiation curable conductive material connected with the transparent
conductive pattern 111 and the maskingdecoration layer 112, and accelerate the speed for curing the radiation curable conductive material, the radiated ray may irradiate the radiation curable conductive material in at least two phases. During these two phases of irradiation, the radiated ray may have two different wavelength ranges. For example, the radiation curable conductive material may first be irradiated by the radiated ray with a wavelength range from 300 nanometers to 400 nanometers, and then be irradiated by the radiated ray with a wavelength range from 230 nanometers to 600 nanometers. Please note that the above wavelength ranges are only an exemplary illustration, and are not utilized for limiting the present invention. - Step S33 is removing uncured parts of the radiation curable conductive material, in order to form the
peripheral circuit 12. For the implementation of Step S33, the uncured parts of the radiation curable conductive material maybe removed by, for example, pure water, such that theperipheral circuit 12 can be formed by the cured parts of the radiation curable conductive material. Theperipheral circuit 12 is connected with the transparentconductive pattern 111, and transmits the touch sensing signals generated by the transparentconductive pattern 111 to an FPC. Since printing and parts of the photolithography process are integrated according to the present invention, theperipheral circuit 12 can be manufactured in an easy and low cost way, and the formed wire width can be less than or equal to about 70 micrometers, which enhances the integration. The utilization of a large number of chemicals is excluded in the present invention, which not only simplifies the process significantly, but also complies with environmental protection and power saving. - The
peripheral circuit 22 of theother touch panel 2 provided by the present invention may also be manufactured by the above methods, and both the structure characteristics and the process can be known by referring to the above illustration. These will not be narrated herein. - The above peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention utilizes radiation curable conductive material as a printing material to be printed on the substrate, cures parts of the radiation curable conductive material, and then removes uncured parts of the radiation curable conductive material in order to form the peripheral circuit, which realizes the reduction of wire width or wire distance in order to achieve higher integration while complying with environmental protection requirements. In addition to utilizing the radiation cured material as the above conductive material, other types of conductive materials may also be realized. What follows is an embodiment utilizing a photosensitive material as the conductive material, which is cured by a visible light in order to form the peripheral circuit.
- Please refer to
FIG. 4A , which is a schematic diagram of afurther touch panel 4 according to a preferable embodiment of the present invention. Thetouch panel 4 includes asubstrate 41 and aperipheral circuit 42. Thesubstrate 41 is a transparent substrate, which can be, for example, a plastic substrate or a glass substrate. In other embodiments, thesubstrate 41 may also be a thin film-shaped substrate such as a PET thin film, etc. In order to take advantage of the exposure and development process in which a high temperature baking process is not required, thesubstrate 41 can preferably be a thin film substrate having flexibility, which is called a flexible substrate, but is not limited herein. - The
substrate 41 has an outer surface S1 and an inner surface S2. The user usually views thetouch panel 4 from the outer surface S1 side of thesubstrate 41, and performs various kinds of operations on the outer surface S1. Other structures and elements of thetouch panel 4 are disposed on the inner surface S2 side of thesubstrate 41. In this embodiment, the inner surface S2 of thesubstrate 41 includes a transparentconductive layer 411. The transparentconductive layer 411 is utilized for defining a touch sensing circuit, and the material of the transparentconductive layer 411 can be, for example, ITO. - The
peripheral circuit 42 is disposed on the inner surface S2 of thesubstrate 41, and is placed next to a terminal of the transparentconductive layer 411 by screen printing. The material of theperipheral circuit 42 is a photosensitive conductive material, which includes a photosensitive resin composition and a plurality of silver particles. For the implementation of theperipheral circuit 42, a diameter of the silver particles is within a range from 1 micrometer to 10 micrometers, and more preferably, within a smaller range from 1 micrometer to 5 micrometers; it may also be blended with several nanometer silver particles. In addition, the photosensitive resin composition is a material which may react after being irradiated by a light. - As shown in
FIG. 4B , thetouch panel 4 may further include an insulatinglayer 43, aconductive adhesive 44 and anFPC 45. The insulatinglayer 43 is formed on parts of theperipheral circuit 42 by pasting or printing, in order to prevent theperipheral circuit 42 from being oxidized due to exposure to the air. The color of the insulatinglayer 43 may also be selected according to product requirements, which allows the insulatinglayer 43 to be a decoration layer simultaneously. Theconductive adhesive 44 is adhered to theperipheral circuit 42 and apin 451 of theFPC 45, such that the touch sensing signals generated by the transparentconductive layer 411 can be transmitted to thepin 451 of theFPC 45 via theperipheral circuit 42 and theconductive adhesive 44. In some embodiments, the conductive adhesive 44 can be ACF or ACP. - Please note that, in this embodiment, the transparent
conductive layer 411 is formed on thesubstrate 41 directly and provides touch sensing functions independently; hence thesubstrate 41 in this embodiment belongs to a type having touch sensing functions and a cover plate simultaneously. According to the present invention, a two-layer touch panel 4c with a two-layer structure may also be utilized, where the two-layer touch panel 4c is composed of twosubstrates 41, as illustrated inFIG. 4C . The following paragraphs illustrate that theabove substrate 41 with one-layer structure includes multiple functions. - After the assembly process of the
substrate 41 is accomplished, only the outer surface S1 of thesubstrate 41 is exposed to the outside, and the transparentconductive layer 411, theperipheral circuit 42 and other structures are covered by thesubstrate 41. In such a condition, thesubstrate 41 not only can provide decoration functions and cover these elements such as theperipheral circuit 42, etc., but can also protect theperipheral circuit 42 and the transparentconductive layer 411 from damages. Moreover, the complete transparentconductive layer 411 is disposed on thesubstrate 41, which is enough to provide sensing functions. Therefore, the present invention realizes both the simplification of substrate process and the diversification of functions. This prospective creation of the distinguishing features is suitable for a modular process to benefit from cost reduction. - Please keep referring to
FIG. 4D . Atouch panel 4d is substantially the same as theabove touch panel 4 shown inFIG. 4B , and the only difference is that thetouch panel 4d further includes aprotective film 46. Theprotective film 46 may be formed on theperipheral circuit 42 and the transparentconductive layer 411 by pasting or printing, in order to cover these two elements and provide protection and decoration functions. Theprotective film 46 can be adhered to thesubstrate 41 stably by adding an optical clear adhesive (OCA) 47. - Please refer to the block diagram shown in
FIG. 5 together withFIG. 4A , which illustrates a method of manufacturing the peripheral circuit of the touch panel according to a preferable embodiment of the present invention. This method can be applied for manufacturing the abovementionedperipheral circuit 42 of thetouch panel 4. The steps of the manufacturing method include Steps S51-S54. - Step S51 is printing a photosensitive conductive material on the
substrate 41 by screen printing. As shown inFIG. 6A , for the implementation of Step S51, a photosensitiveconductive material 63 is formed on the transparentconductive layer 411 of thesubstrate 41 by printing via screen printing equipment composed of ascraper 61 and ascreen 62. In detail, the screen printing equipment prints the photosensitiveconductive material 63 on thesubstrate 41 by blocks or areas. - The above photosensitive
conductive material 63 includes a photosensitive resin composition and a plurality of silver particles. A diameter of the silver particles is within a range from 1 micrometer to 10 micrometers, and more preferably within a range from 1 micrometer to 5 micrometers. Thesubstrate 41 is a transparent substrate, which can be, for example, a plastic substrate or a glass substrate. The material of the transparentconductive layer 411 can be, for example, ITO. The transparentconductive layer 411 may first be formed on thesubstrate 41 by sputtering and etching. - Step S52 is disposing a
photomask 64 on the photosensitive conductive material. In order to regulate the position of the circuit layout, thephotomask 64 is disposed on the photosensitiveconductive material 63 for the implementation of Step S52, as illustrated inFIG. 6B . The material of the above photomask includes glass, quartz or PET, and the form of thephotomask 64 can be, but is not limited to, positive or negative, which is determined according to the nature of the material and the structural requirements of theperipheral circuit 42. - Step S53 is irradiating the photosensitive conductive material with a
beam 65, in order to cure parts of the photosensitive conductive material. For the implementation of Step S53, a light wave generation apparatus is utilized for generating thebeam 65, which selectively irradiates the photosensitiveconductive material 63 via thephotomask 64, as illustrated inFIG. 6B . Thebeam 65 can be, for example, a visible light, which has a wavelength within a range from 350 nanometers to 780 nanometers. - Step S54 is etching uncured parts of the photosensitive conductive material, in order to form the
peripheral circuit 42. For the implementation of Step S54, for example, developer may be utilized for etching the uncured parts of the photosensitive conductive material, in order to remove the uncured parts of the photosensitive conductive material and form theperipheral circuit 42 with the cured parts of the photosensitive conductive material. Theperipheral circuit 42 is connected with the transparentconductive layer 411, wherein a wire width of theperipheral circuit 42 may be less than 100 micrometers and a wire distance of theperipheral circuit 42 may be less than 120 micrometers. - Please refer to
FIG. 4D . In this structure, the method of manufacturing the peripheral circuit of thetouch panel 4d further includes: adhering theperipheral circuit 42 to theFPC 45 by using theconductive adhesive 44, and disposing theprotective film 46 on theperipheral circuit 42. For the implementation of these steps, theprotective film 46 maybe formed on parts of theperipheral circuit 42 and the transparentconductive layer 411 by pasting or printing, in order to prevent theperipheral circuit 42 from being touched or oxidized due to exposure to the air directly. The color of theprotective film 46 may also be selected according to product requirements, which allows theprotective film 46 to be a decoration layer simultaneously, in order to prevent the user from viewing the inside circuits. - The
conductive adhesive 44 is adhered to theperipheral circuit 42 and thepin 451 of theFPC 45, such that the touch sensing signals generated by the transparentconductive layer 411 can be transmitted to thepin 451 of theFPC 45 via theperipheral circuit 42 and theconductive adhesive 44. In some embodiments, the conductive adhesive 44 can be ACF or ACP. - The above peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention utilizes photosensitive conductive material as a printing material to be printed on the substrate, cures parts of the photosensitive conductive material, and then etches uncured parts of the photosensitive conductive material in order to form the peripheral circuit, which realizes the simplification of the manufacturing process while retaining the adherence degree and electronic characteristic.
- In summary, the peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention enjoy the benefits of screen printing and exposure/development, ensuring that not only can the touch panel be manufactured at a low cost and high speed, but that the touch panel is also provided with the advantages of small wire width and wire distance. Therefore, this method is suitable for smaller electronic devices, while overcoming the barriers of the conventional processes. The method of manufacturing the peripheral circuit of the touch panel utilizing a printing technique according to the present invention can minimize the wire width and the wire distance of the peripheral circuit, in order to achieve a fine wire width process to enhance the resolution. The peripheral circuit of the touch panel and the manufacturing method thereof according to the present invention can also enlarge the visible area, which provides greater convenience to the user. For the implementation of the present invention, the manufacturing method enjoys the benefits of screen printing and exposure/development; hence power consumption problems can be avoided, as opposed to the conventional thermal curing process where the power consumption is generated by using an oven for a long time. Therefore, the environmental protection requirements can also be met.
- Those skilled in the art will readily observe that numerous modifications and alterations of the device and method may be made while retaining the teachings of the invention. Accordingly, the above disclosure should be construed as limited only by the metes and bounds of the appended claims.
Claims (16)
1. A method for manufacturing a peripheral circuit of a touch panel comprising:
printing a radiation curable conductive material on a substrate having a transparent conductive pattern;
irradiating the radiation curable conductive material with a radiated ray, in order to cure parts of the radiation curable conductive material; and
removing uncured parts of the radiation curable conductive material, in order to form the peripheral circuit.
2. The method of claim 1 , wherein a wavelength of the radiated ray is approximately within a range from 230 nanometers to 600 nanometers.
3. The method of claim 1 , wherein the transparent conductive pattern is connected with the peripheral circuit.
4. The method of claim 1 , wherein a wire width of the peripheral circuit is less than or equal to about 70 micrometers.
5. The method of claim 1 , wherein the radiation curable conductive material comprises radiation curable silver glue, radiation curable silver paste or radiation curable ink.
6. The method of claim 1 , wherein the step of curing parts of the radiation curable conductive material comprises selectively curing the radiation curable conductive material by disposing a photomask on the radiation curable conductive material.
7. The method of claim 1 , wherein the radiated ray irradiates the radiation curable conductive material with at least two different wavelength ranges.
8. The method of claim 1 , wherein the radiation curable conductive material is printed on the substrate by screen printing.
9. A method for manufacturing a peripheral circuit of a touch panel comprising:
printing a photosensitive conductive material on a substrate by screen printing;
disposing a photomask on the photosensitive conductive material;
irradiating the photosensitive conductive material with a beam, in order to cure parts of the photosensitive conductive material; and
etching uncured parts of the photosensitive conductive material, in order to form the peripheral circuit.
10. The method of claim 9 , wherein the photosensitive conductive material comprises a plurality of silver particles.
11. The method of claim 10 , wherein a diameter of the plurality of silver particles is within a range from 1 micrometer to 10 micrometers.
12. The method of claim 9 , wherein a wire width of the peripheral circuit is less than 100 micrometers.
13. The method of claim 9 , further comprising:
adhering the peripheral circuit to a flexible printed circuit board (FPC) by using a conductive adhesive, and the conductive adhesive is an anisotropic conductive film (ACF) or anisotropic conductive past (ACP).
14. The method of claim 9 , further comprising:
disposing a protective film on the peripheral circuit.
15. The method of claim 14 , wherein the step of disposing the protective film on the peripheral circuit comprises disposing the protective film utilizing a pasting method or a printing method.
16. The method of claim 9 , wherein the beam comprises a visible light with a wavelength within a range from 350 micrometers to 780 micrometers.