SU973642A1 - Method for heat treating of welded joints - Google Patents
Method for heat treating of welded joints Download PDFInfo
- Publication number
- SU973642A1 SU973642A1 SU813241534A SU3241534A SU973642A1 SU 973642 A1 SU973642 A1 SU 973642A1 SU 813241534 A SU813241534 A SU 813241534A SU 3241534 A SU3241534 A SU 3241534A SU 973642 A1 SU973642 A1 SU 973642A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- cooling
- heating
- temperature
- heat treatment
- formation
- Prior art date
Description
Изобретение относитс к термической обработке и может йыть использовано при локальной обработке сварных соединений высоколегированных сталей мартенситного и мартенситноферритного классов с мартенситом высокой устойчивости.The invention relates to heat treatment and may be used in the local processing of welded joints of high-alloy steels of martensitic and martensite-ferrite classes with high-resistance martensite.
Известен способ термической обработки сварных соединений, включающий нагрев до температуры (30 40С ) с последующим замедленным охлаждением до температуры А - (30 40«С )С1.The known method of heat treatment of welded joints, including heating to a temperature of (30 40C), followed by slow cooling to a temperature of A - (30 40 "C) C1.
Обнако подобна термическа обработка не приводит в стал х указанного класса к заметному распаду мартенсита и не устран ет хрупкости сварного соединени и склонности к образованию трещин при дешьнейшем охлаждении.However, such a thermal treatment does not lead to the steels of this class to a noticeable decomposition of martensite and does not eliminate the brittleness of the welded joint and the tendency to form cracks with the cheapest cooling.
Наиболее близким к предлагаемому по технической сущности вл етс способ термической обработки сварных соединений, заключающийс в охлаждении сварного шва до температуры Ау. и импульсном нагреве до температуры 5 Aj..3TOT способ позвол ет в значительной мере уменьшить возможность образовани холодных трещин 2.The closest to the proposed technical essence is the method of heat treatment of welded joints, which consists in cooling the weld to the temperature Ay. and pulsed heating to a temperature of 5 Aj. 3.TOT method significantly reduces the possibility of cold cracks 2.
Однако способ не обеспечивает эксплуатационной стойкости к ударным нагрузкам шва и околошовнрй зоны,However, the method does not provide operational resistance to shock loads of the seam and near-zone,
Целью изобретени вл етс устранение возможности образовани холодных трещин и обеспечени высокой ударной в зкости сварного шва и околошовной зоны.The aim of the invention is to eliminate the possibility of the formation of cold cracks and the provision of high impact toughness of the weld and heat-affected zone.
Поставленна цель достигаетс The goal is achieved
10 тем, что согласно способу, включающему охлаждение после сварки, ускоренный нагрев и охлаждение, охлаждение после сварки производ т до температуры образовани / 50% мартен15 сита, но не ниже 150С, нагревают в межкритическом интервале температур , охлаждают до 100-150°С и вновь нагревают до температуры Aj. (50 - 100°С ) с последующим охлгикде20 нием на воздухе.10 by the fact that, according to the method including cooling after welding, accelerated heating and cooling, cooling after welding is carried out to the formation temperature of / 50% marten15 sieve, but not lower than 150 ° C, heated in the intercritical temperature range, cooled to 100-150 ° C re-heated to temperature Aj. (50 - 100 ° С) with subsequent cooling in air.
Нагрев и охлаждение производ т многократно.Heating and cooling are performed multiple times.
Claims (2)