[go: up one dir, main page]

SU84711A1 - Way to pour non-ferrous metals and alloys - Google Patents

Way to pour non-ferrous metals and alloys

Info

Publication number
SU84711A1
SU84711A1 SU375720A SU375720A SU84711A1 SU 84711 A1 SU84711 A1 SU 84711A1 SU 375720 A SU375720 A SU 375720A SU 375720 A SU375720 A SU 375720A SU 84711 A1 SU84711 A1 SU 84711A1
Authority
SU
USSR - Soviet Union
Prior art keywords
alloys
way
ferrous metals
ingot
pour non
Prior art date
Application number
SU375720A
Other languages
Russian (ru)
Inventor
И.А. Алексеев
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU375720A priority Critical patent/SU84711A1/en
Application granted granted Critical
Publication of SU84711A1 publication Critical patent/SU84711A1/en

Description

Применение местных кокилей, охлаждающих отдельные участки отливки, дл  устранени  усадочной рыхлоты, известно.The use of local chill molds that cool individual casting areas to eliminate shrinkage loosening is well known.

Предлагаетс  примен ть местный кокиль в виде медного стержн  дл  лить  слитков цветных металлов, с целью быстрого охлаждени  усадочной части слитка и повышени  плотности его.It is proposed to use a local chill mold in the form of a copper rod for casting non-ferrous metal ingots in order to rapidly cool the shrink part of the ingot and increase its density.

Л1еталл заливают в изложницу, после чего в верхнюю жидкую часть слитка на глубину 2-3 лш погрул ;ают металлический стержень; после затвердевани  слитка стержень удал ют.L1 metal is poured into the mold, after which it is immersed in the upper liquid part of the ingot to a depth of 2-3 ps; after the ingot solidifies, the core is removed.

Дл  алюминиевых слитков стержень берут медный, а дл  медных - медный стержень должен иметь железный наконечник во избелсапие его сваривани  со слитком.For aluminum ingots, the core is taken from copper, and for copper ones, the copper core must have an iron tip to prevent its welding with the ingot.

При погружении кокил -стержн  в верхнюю часть слитка происходит рассредоточение тенла в усадочной его части и слиток в этом месте получаетс  более плотным.When the chill-rod is immersed in the upper part of the ingot, the tenl is dispersed in its shrinkage part and the ingot in this place becomes more dense.

Предмет изобретени Subject invention

Способ лить  цветных металлов и сплавов, отличающийс  тем, что, в цел х устранени  усадочной рыхлоты в верхней части слитка, в открытую изложницу, залитую металлом, сверху по центровой оси ее погружают металлический стержень на глубину 2-3 мм.The method of casting non-ferrous metals and alloys, characterized in that, in order to eliminate shrinkage loosening in the upper part of the ingot, a metal core is immersed to the depth of 2-3 mm in the open mold filled with metal from above along its central axis.

SU375720A 1948-02-16 1948-02-16 Way to pour non-ferrous metals and alloys SU84711A1 (en)