SU386568A1 - Способ пассивации магни - Google Patents
Способ пассивации магниInfo
- Publication number
- SU386568A1 SU386568A1 SU7101723960A SU1723960A SU386568A1 SU 386568 A1 SU386568 A1 SU 386568A1 SU 7101723960 A SU7101723960 A SU 7101723960A SU 1723960 A SU1723960 A SU 1723960A SU 386568 A1 SU386568 A1 SU 386568A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- magnesium
- filler
- increase
- poured
- passivation
- Prior art date
Description
1
Изобретение относитс к рафинированию чугуна, в частности к его десульфурации.
Известен способ пассивации магни , заключающийс в его разубоживании наполнителем, например, доломитизированным известн ком. Однако известные способы не обеспечивают низкой скорости испарени магни в чугуне и высокой степени его усвоени .
С целью увеличени степени использовани магни , снижени пироэффекта при десульфурации и увеличени степени десульфурацин по предложенному способу расплав магни заливают на кусковой наполнитель, предварительно нагретый до 600-650° С. Причем, магний заливают в количестве 40-60% от веса исходных материалов, а в качестве наполнител используют легирующие элементы.
Кусковой наполнитель, нагретый до 600- 650° С и помещенный в изложницу, заливают расплавом магни , охлаждают и подают дл обработки чугуна.
Магний в процессе заливки заполн ет неплотности и пустоты между кусками наполнител .
В качестве пассиватора может использоватьс щлак металлургического производства, кокс и другие элементы, а также легирующие элементы.
Claims (3)
1.Способ пассивации магни разубоживанием его наполнителем, отличающийс тем, что, с целью увеличени степени использовани магни , снижени пироэффекта при десульфурации и увеличени степени десульфурацин, расплав магни заливают на кусковой наполнитель, предварительно нагретый до 6вО-650° С.
2.Способ по п. 1, отличающийс тем, что магний заливают в количестве 40-60% от веса исходных материалов.
3.Способ по МП. 1 и 2, отличающиЛс тем, что и качестве наполнител используют ле1ирующие элементы.