SU1675251A1 - В жущее - Google Patents
В жущее Download PDFInfo
- Publication number
- SU1675251A1 SU1675251A1 SU894734072A SU4734072A SU1675251A1 SU 1675251 A1 SU1675251 A1 SU 1675251A1 SU 894734072 A SU894734072 A SU 894734072A SU 4734072 A SU4734072 A SU 4734072A SU 1675251 A1 SU1675251 A1 SU 1675251A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- mpa
- gas cleaning
- production
- dust
- manganese
- Prior art date
Abstract
Изобретение относитс к промышленности строительных материалов и может быть использовано при изготовлении шлакощелочных в жущих и жаростойких растворов и бетонов на их основе Целью изобретени вл етс повышение остаточной прочности при 800°С В жущее содержит , мас.%: жидкое стекло 33-3-1, феррохромовый шлак 17-56 и пыль газопчист- ки производства силикомарганца 1050 ВР жущее обеспечивает прочность марочную 33-40 МПа; после сушки 54-63 МПа после нагрева до 800°С 68,6-80,96 МПа, после i.a- грева до 1100°С 104,7-108,5 МПа; угадку при нагревании до 800°С 0,67-0,88%. 2 табл
Description
Насто щее изобретение относитс к промышленности строительных материалов и может быть использовано при изготовлении шлакощелочных в жущих и жаростойких растворов и бетонов на их основе, эксплуатируемых при температурах до 1100°С.
Целью изобретени вл етс повышение остаточной прочности при 800°С.
Пример осуществлени изобретени .
Используют следующие материалы: жидкое стекло с силикатным модулем (Мс) 2,6-3, плотностью 1,33 г/см3; феррохромо- вый шлак (самораспадающийс ), химический состав указан в табл. 1; пыль газоочистки производства силикомарганца, химический состав указан в табл. 1.
Составы и свойства в жущего приведены в табл. 2.
Свойства компонентов приведены ниже .
Жидкое стекло Модуль 2,6-3,0
Феррохромовый распадающийс шлак Удельна поверхность 300-400 м2/кг
Пыль газоочистки производства силикомарганца Удельна поверхность 1200-1800 м /кг.
Образцы дл испытани приготовл ют по следующей методике.
Исходные компоненты дозируют по массе (отклонени не должны превышать ±1%) и перемешивают вручную не менее 1 мин, после чего в смесь добавл ют жидкое стекло и перемешивают не менее 3 мин Из приготовленной смеси формуют образцы- балочки размером 40 40 160 мм. Уплотнение смеси производ т на лабораторном вибростоле . Твердение образцов происходит в воздушно-сухих услови х при температуре 20±3°С. Марочную прочность определ ют испытанием при изгибе и сжатии образцов после трех суток твердени , Дл определени контрольной прочности образцы после трехсуточного твердени подвергают сушке
Ё
о Ki
ел
ю
101
до посто нной массы при температуре 105± 5°С. Остаточную прочность определ ют после сушки и последующего обжига образцов до температуры 800 и 1100°С.
Жаростойкие в жущие обладают следующими свойствами: прочность марочна (после твердени в течение трех суток в воздушно-сухих услови х) Рсж 33-40 МПа; огнеупорность 1100°С; прочность контрольна (после сушки при температуре 105±5°С) Рсж 54-63 МПа; усадка при нагревании до 800°С 0,67-0,88%.
0
Claims (1)
- Формула изобретени В жущее, включающее жидкое стекло, феррохромовый шлак и пыль газоочистки производства силицида металла, отличающеес тем, что, с целью повышени остаточной прочности при 800°С, она содержит в качестве последней пыль газоочистки производства силикомарганца при следующем соотношении компонентов, мас.%: Жидкое стекло33-34Феррохромовый шлак17-56Пыль газоочистки производства силикомарганца10-50.Таблица IМатериалСолервкаюм оксидов мае.2тГ111111Г11SiOzI ,A lO,CaOMgO TiO, SO,ttnO I На,,0 SIC ВгОп.п.п.Таблица 2