FR2426903A1 - Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defects - Google Patents
Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defectsInfo
- Publication number
- FR2426903A1 FR2426903A1 FR7815588A FR7815588A FR2426903A1 FR 2426903 A1 FR2426903 A1 FR 2426903A1 FR 7815588 A FR7815588 A FR 7815588A FR 7815588 A FR7815588 A FR 7815588A FR 2426903 A1 FR2426903 A1 FR 2426903A1
- Authority
- FR
- France
- Prior art keywords
- prods
- defects
- soln
- substance
- coated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The surface of the rolled prod. is coated with a substance (A) forming a background for a second substance (B) which changes colour when heated. High frequency heating is then used so that defects on or near the surface of the prod. cause a thermochemical change in substance (B) altering its colour so the defects are clearly visible. When substance (B) is used as a soln., drying is pref. used for coating (B) at a temp. below that causing its colour to change. Substances (A,B) may alternatively be combined in an aq. colloidal suspension, contg. 30-160 g/l KOH in soln. and 5-20 g/l soluble potato starch. Used for inspection of ingots and slabs which still have a scaled surface due to hot rolling, or for examining profiles, e.g. rails or girders. The invention can be used without prior surface treatment of the rolled prods.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7815588A FR2426903A1 (en) | 1978-05-25 | 1978-05-25 | Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defects |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7815588A FR2426903A1 (en) | 1978-05-25 | 1978-05-25 | Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defects |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2426903A1 true FR2426903A1 (en) | 1979-12-21 |
FR2426903B1 FR2426903B1 (en) | 1981-05-08 |
Family
ID=9208690
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7815588A Granted FR2426903A1 (en) | 1978-05-25 | 1978-05-25 | Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defects |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR2426903A1 (en) |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE907946C (en) * | 1950-08-25 | 1954-04-01 | Aral Ag B V | Method for testing tubular metal workpieces for defects, especially for longitudinal cracks |
US3871212A (en) * | 1973-05-04 | 1975-03-18 | Goodyear Tire & Rubber | System and method for monitoring quality characteristics of a moving web |
-
1978
- 1978-05-25 FR FR7815588A patent/FR2426903A1/en active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE907946C (en) * | 1950-08-25 | 1954-04-01 | Aral Ag B V | Method for testing tubular metal workpieces for defects, especially for longitudinal cracks |
US3871212A (en) * | 1973-05-04 | 1975-03-18 | Goodyear Tire & Rubber | System and method for monitoring quality characteristics of a moving web |
Also Published As
Publication number | Publication date |
---|---|
FR2426903B1 (en) | 1981-05-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA1013032A (en) | Method of testing for and preventing the possibility of cracking, spalling or like defects in a body surface subjected to mechanical forces | |
US2492682A (en) | Processes of producing glass coated silicon steel | |
FR2426903A1 (en) | Inspecting rolled prods. for surface defects - where prods. are coated with indicator soln. and subjected to high frequency induction heating which reveals the defects | |
US2878151A (en) | Method for producing single-fire enameling stock devoid of fish-scaling and product thereof | |
JPS5367488A (en) | Method and apparatus for inspection of sticks of smoking articles as for defects of coatings | |
JPS51135590A (en) | Surface defect detection method and its equipment | |
FR2015451A2 (en) | Descaling stainless steel | |
SE405129B (en) | PROCEDURE FOR FIXING TEXTILE ROLLS CONTAINING HEALTH FIBERS WITH BLACK FERRY ON THE BASIS OF THE DIAZO OR OXIDATION FERCING TECHNIQUE AND ACCORDING TO THE EXTRACTION METHOD | |
JPS51147378A (en) | Flaw detecting method of steel pieces | |
JPS51114981A (en) | Steel surface scar detecting method and equipment | |
ES362055A1 (en) | Potassium silicate coated silicon steel article | |
JPS5772718A (en) | Hot rolling method for steel | |
JPS53112244A (en) | Coiling method for titanium strip | |
Koterazawa et al. | Propagation of part-through cracks by alternating bending stresses | |
JPS5232387A (en) | Method of detecting defects of weld zones of steel pipes | |
Fedorov | Mechanisms of Crack Initiation and Role of Twins in Dynamic Loading of Fe+ 3. 25% Si Alloy in the 77-573 K Temperature Range | |
Wu | Influence of Residual Copper and Tin and Heating Process on Surface Hot-Shortness or Cracks of Rolled Products of Plain Carbon Steel | |
JPS53112248A (en) | Method and facilities for hot direct rolling of steel material | |
JPS51121416A (en) | Rolls for heat treatment | |
SU116288A1 (en) | The method of steel cementation in solid carburizer | |
JPS55128534A (en) | Preparation of cold rolled steel plate | |
JPS53110890A (en) | Method and apparatus for testing thermal fatigue | |
Pacl | Defects of Oriented Transformer Strips | |
SU668728A1 (en) | Method of manufacturing small-section steel and wire rod | |
JPS55147339A (en) | Method of measuring length of crack |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
ST | Notification of lapse |