Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by IndividualfiledCriticalIndividual
Priority to ES204116ApriorityCriticalpatent/ES204116A3/en
Publication of ES204116A3publicationCriticalpatent/ES204116A3/en
Improvements in the manufacture of copper-based alloys according to which the zinc and nickel copper alloy is formed and manganese itself is incorporated in such a way that the alloy comes to contain approximately 53% to 75% copper a minimum of 5% manganese and a minimum of 5% nickel with the sum of manganese and nickel in the order of 12% to 20% and the zinc balance. (Machine-translation by Google Translate, not legally binding)
ES204116A1952-06-131952-06-13Improvements in the manufacture of copper-based alloys (Machine-translation by Google Translate, not legally binding)
ExpiredES204116A3
(en)
Procedure to increase the temperature of recristalization and restrict the growth of grain in brasses (Machine-translation by Google Translate, not legally binding)