[go: up one dir, main page]

DE602061C - Mold with slow heat dissipation - Google Patents

Mold with slow heat dissipation

Info

Publication number
DE602061C
DE602061C DEO19390D DEO0019390D DE602061C DE 602061 C DE602061 C DE 602061C DE O19390 D DEO19390 D DE O19390D DE O0019390 D DEO0019390 D DE O0019390D DE 602061 C DE602061 C DE 602061C
Authority
DE
Germany
Prior art keywords
mold
casting
walls
heat dissipation
inner walls
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DEO19390D
Other languages
German (de)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to DEO19390D priority Critical patent/DE602061C/en
Application granted granted Critical
Publication of DE602061C publication Critical patent/DE602061C/en
Expired legal-status Critical Current

Description

Kokille mit langsamer Wärmeableitung Die beim Kokillenguß auftretende rasche Ableitung der Wärme aus dem Gußstück, die für viele Zwecke unerwünscht ist, hat man bisher einerseits durch Auskleidung metallischer, gegebenenfalls wassergekühlter Kokillen mit Metallegierungen schlechter Wärmeleitfähigkeit, andererseits durch Heranziehung von Steingut, Porzellan, Schamotte oder ähnlichen keramischen Massen zur Herstellung der Gußformen zu bekämpfen versucht. Rasche Ableitung der Wärme begründet nämlich häufig schwammige, porige Zonen im Gußkörper, Auftreten von Spannungen, Lunkerbildungen, verschiedene Dichte des Gußkörpers usw. Trotz Anwendung der oben angeführten Maßnahmen war es bisher nicht möglich, mittels Kokillenguß Gußkörper völliger Homogenität herzustellen. Erfindungsgemäß wird die Kokille, deren sämtliche Innenwände zwecks langsamer Wärmeableitung mit einem schlecht leitenden Wärmeleiter ausgekleidet sind, so ausgebildet, daß die Kokilleninnenwände mit einem nicht metallischen Stoff mit im Verhältnis zu Metall äußerst geringem \Värmeleitungsvermögen, vorzugsweise einem feuerfesten keramischen Stoff, in solcher Stärke belegt sind, daß das Gußmaterial -während seiner Abkühlung an allen Stellen des Gußraumes jeweils die gleiche Temperatur hat. Die mit dem isolierten Stoff belegten .Hauptwandungen können als Wasserkästen ausgebildet werden. Die Wahl solcher Kokillen mit oder ohne Wasserkästen wird jeweils von dem Gußstück abhängen. Der Belag der Innenwandungen kann erfindungsgemäß in solcher Weise eingebracht werden, daß die Wandungen mit Führungen versehen sind, die dazu dienen, die isolierenden Beläge in Form von Plattenoder Leisten einschieben zu lassen.Chill mold with slow heat dissipation The one that occurs during chill casting rapid dissipation of heat from the casting, which is undesirable for many purposes, So far you have on the one hand by lining metallic, possibly water-cooled Molds with metal alloys with poor thermal conductivity, on the other hand through Use of earthenware, porcelain, chamotte or similar ceramic masses tried to fight for the production of the molds. Rapid dissipation of heat namely often causes spongy, porous zones in the cast body, occurrence of tensions, Formation of cavities, different densities of the cast body, etc. Despite the application of the above cited measures, it was not possible to use castings by means of permanent mold casting complete homogeneity. According to the invention, the mold, all of which Inner walls for slow heat dissipation with a poorly conductive heat conductor are lined, designed so that the mold inner walls with a non-metallic Material with extremely low thermal conductivity in relation to metal, preferably a refractory ceramic material, are occupied to such a degree that the casting material -during its cooling, the same temperature at all points in the casting space Has. The main walls covered with the insulated material can be used as water boxes be formed. The choice of such molds with or without water tanks is made in each case depend on the casting. The lining of the inner walls can according to the invention in be introduced in such a way that the walls are provided with guides, which are used to insert the insulating coverings in the form of panels or strips allow.

In der Zeichnung ist der Erfindungsgegenstand in beispielsweiser Ausführungsform dargestellt. Abb. i zeigt eine Hälfte der Kokille in Ansicht, Abb. a einen Vertikal-, Abb.3 einen Horizontalschnitt.In the drawing, the subject matter of the invention is shown in an exemplary embodiment shown. Fig. I shows a half of the mold in view, Fig. A a vertical, Fig.3 a horizontal section.

Der Kokillenkörper besteht aus zwei je in einem Stück gegossenen Kästen i, i', deren verhältnismäßig dünne Wände durch in dem Wasser führenden Mantelhohlraum angeordnete Stege z gegeneinander abgestützt sind. An den Innenwandungen 3 ansetzende Flanschen dienen zur Befestigung von Abschlußstücken 4 zur Bildung des Gußraumes. Diese Flanschen sind an drei Seiten gegen die Innenwände 3 zu unterschnitten, so daß deren dem Gußraum zugekehrte Flächen mit Platten 5 aus keramischem Stoff, wie z. B. Siliciumca.rbid oder Aluminiumoxyd, belegt werden können, die sich hinter den Flanschen verankern. Die Abschlußstücke sind an der Innenseite gleichfalls mit diesem Stoff verkleidet, wozu schmale Isolierplatten an ihnen mittels Feder und Nut verankert sind. Bei dem gezeichneten Ausführungsbeispiel ist der von den Platten 5 gebildete schlechte Wärmeleiter auswechselbar. Die beiden Kästen i, i' sind in üblicher Weise durch Scharniere miteinander verbunden und werden durch Schrauben 6 in der aneinandergeklappten Stellung gesichert.The mold body consists of two boxes each cast in one piece i, i ', the relatively thin walls of which through the jacket cavity leading into the water arranged webs z are supported against each other. On the inner walls 3 attaching Flanges are used to attach terminators 4 to form the casting space. These flanges are to be undercut on three sides against the inner walls 3, see above that their surfaces facing the casting space with plates 5 made of ceramic material, such as z. B. Siliciumca.rbid or aluminum oxide, which can be occupied behind anchor the flanges. The end pieces are also on the inside this material disguised, including narrow insulating plates on them by means of springs and Groove are anchored. In the illustrated embodiment, that of the plates 5 bad heat conductors formed replaceable. The two boxes i, i ' are connected to each other in the usual way by hinges and by screws 6 secured in the folded position.

Die Platten und Einsatzstücke bilden eine Umgrenzung des Gußraumes mit ebenen Flächen, bei denen die Gefahr des Ausbauchens vollständig vermieden ist. Wie Versuche ergeben haben, bedingen diese Auskleidungen des Gußraumes eine so langsame und an allen Stellen der Oberfläche des Gußstückes gleichmäßige Ableitung der Wärme, daß der Gußkörper ein vollkommen gleichmäßiges dichtes Gefüge erhält.The plates and inserts form a boundary for the casting space with flat surfaces where the risk of bulging is completely avoided. As tests have shown, these linings of the casting space are so slow and uniform dissipation of heat at all points on the surface of the casting, that the cast body has a completely uniform, dense structure.

Da die gegebenenfalls angeordneten Wasserkästen in sich geschlossen, also von 'den Formwänden völlig unabhängig sind, kann kein Wasser in den eigentlichen Gießraum gelangen.Since the possibly arranged water tanks are self-contained, So from 'the mold walls are completely independent, no water can in the actual Reach the casting room.

Der schlechte Wärmeleiter kann auch in die Innenwandungen der Kokille eingegossen oder eingestampft werden. Die Art der Anbringung hängt naturgemäß mit der Wahl des Isoliermaterials zusammen.The poor heat conductor can also get into the inner walls of the mold poured in or pulped. The type of attachment naturally depends the choice of insulation material.

Claims (3)

PATENTANSPRÜCHE: i. Kokille mit langsamer Wärmeableitung, deren sämtliche Innenwände mit einem schlecht leitenden Wärmeleiter ausgekleidet sind, zum Gießen von Metallen, dadurch gekennzeichnet, daß die Kokilleninnenwände mit einem nicht metallischen Stoff mit im Verhältnis zu Metall äußerst geringem Wärmeleitvermögen, vorzugsweise einem feuerfesten keramischen Stoff. in solcher Stärke belegt sind, daß das Gußmaterial während seiner Abkühlung an allen Stellen des Gußraumes jeweils die gleiche Temperatur hat. PATENT CLAIMS: i. Mold with slow heat dissipation, all inner walls of which are lined with a poorly conductive heat conductor, for casting metals, characterized in that the mold inner walls are made of a non-metallic material with extremely low thermal conductivity in relation to metal, preferably a refractory ceramic material. are proven to such an extent that the casting material has the same temperature at all points in the casting space during its cooling. 2. Kokille nach Anspruch i, dadurch gekennzeichnet, daß die mit dem isolieren-den Stoff belegten Hauptwandungen als Wasserkästen ausgebildet sind. 2. The mold according to claim i, characterized in that formed with the isolieren- the fabric occupied main walls as water tanks. 3. Kokille nach Anspruch i und 2, dadurch gekennzeichnet, daß die Wandungen 'mit Führungen versehen sind, in welche die isolierenden Beläge in Form von Platten oder Leisten einschiebbar sind.3. Mold according to claim i and 2, characterized in that the walls' are provided with guides in which the insulating coverings in Form of plates or strips can be inserted.
DEO19390D 1931-09-27 1931-09-27 Mold with slow heat dissipation Expired DE602061C (en)