DE439088C - Rectifier made of iron - Google Patents
Rectifier made of ironInfo
- Publication number
- DE439088C DE439088C DEA46728D DEA0046728D DE439088C DE 439088 C DE439088 C DE 439088C DE A46728 D DEA46728 D DE A46728D DE A0046728 D DEA0046728 D DE A0046728D DE 439088 C DE439088 C DE 439088C
- Authority
- DE
- Germany
- Prior art keywords
- iron
- vessel
- rectifier
- welds
- rectifier made
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Gleichrichtergefäß aus Eisen. Die aus Eisen hergestellten Gefäße für Ouecksilberdampfgleichrichter erfüllen ihre Aufgabe nicht immer in vollkommen einwandfreier Weise, denn es kommt vor, daß poröse Stellen in den Gefäßwänden oder in den etwa vorhandenen Schweißnähten vorhanden sind, die Luft in das Gefäßinnere eindringen lassen. Um diese Porosität unschädlich zu machen, ist bereits vorgeschlagen «-orden, die chtveißnähte mit einem besonderen evakuierten Hohlraum zu umgeben oder das ganze Gefäß mit metallischen oder Emailleüberzügen zu versehen. Diese Abdichtungsverfahren sind verhältnismäßig umständlich und kostspielig.Rectifier vessel made of iron. The vessels made of iron for Mercury vapor rectifiers do not always do their job perfectly Way, because it happens that porous places in the vessel walls or in the approx existing welds are present, the air can penetrate into the interior of the vessel permit. In order to render this porosity harmless, it has already been proposed to surround the chtviss seams with a special evacuated cavity or the whole To provide the vessel with metallic or enamel coatings. This waterproofing method are relatively cumbersome and expensive.
Gemäß der Erfindung wird das eiserne Gleichrichtergefäß an den Schweißnähten oder auf dem ganzen Umfang mit einer aufvulkanisierten Gummischicht überzogen. Hierbei ist es vorteilhaft, diejenigen Teile, bei denen die Bildung von Poren wahrscheinlicher ist, also z. B. die Schweißnähte, mit einer starken, die übrigen Teile des Gefäßes aber mit einem schwächeren Gummiüberzug zu versehen. Die hiermit verbundenen. Vorteile bestehen darin, daß die Teile, die eines besseren Schutzes bedürfen, auch tatsächlich sicherer abgedichtet werden, während andererseits die Abkühlung infolge des schwachen- Gummiüberzuges auf der übrigen Gefäßoberfläche nicht nennenswert beeinträchtigt wird.According to the invention, the iron rectifier vessel is attached to the welds or covered over the entire circumference with a vulcanized rubber layer. Here it is beneficial to those parts where the formation of pores is more likely is, so z. B. the welds, with a strong, the remaining parts of the vessel but to be provided with a weaker rubber coating. The associated. advantages consist in the fact that the parts that require better protection actually do be sealed more securely, while on the other hand, the cooling due to the weak Rubber coating on the rest of the vessel surface is not significantly impaired will.
Claims (1)