CN2747220Y - 柔性支撑的真空玻璃 - Google Patents
柔性支撑的真空玻璃 Download PDFInfo
- Publication number
- CN2747220Y CN2747220Y CN 200420109208 CN200420109208U CN2747220Y CN 2747220 Y CN2747220 Y CN 2747220Y CN 200420109208 CN200420109208 CN 200420109208 CN 200420109208 U CN200420109208 U CN 200420109208U CN 2747220 Y CN2747220 Y CN 2747220Y
- Authority
- CN
- China
- Prior art keywords
- glass
- flexible support
- flat glass
- flexible
- vacuum
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种柔性支撑的真空玻璃。至少含有两块形状相同的平面玻璃,相邻平面玻璃之间至少均匀分布三个相同材料制作的等高的柔性支撑,环绕平面玻璃边缘的缝隙中设有与柔性支撑相同材料制作的等高的柔性支撑条,沿柔性支撑条外侧通过胶粘剂将平面玻璃边缘连接,使相邻平面玻璃之间形成密封腔,相邻平面玻璃之间的柔性支撑条上设有一个抽真空接口,抽真空接口上覆有封口剂。本实用新型的优点在于:柔性支撑可以避免支撑在两块玻璃间滑动,保证玻璃受力均匀,半透明的柔性支撑透光性优于金属支撑;由于抽真空接口的设置隐蔽,生产的真空玻璃更加美观,并能生产三层以上平面玻璃形成的多个密封腔的平面玻璃。
Description
技术领域:
本实用新型涉及一种平面真空玻璃,尤其是一种柔性支撑的真空玻璃。
背景技术:
真空玻璃的概念最早出现在1913年国外一项专利文献,直到20世纪80年代,对它的研究才逐渐活跃,2001年7月,西安交大邓宏飞等人发表了研究实验成果,称采用0.8mm特种玻璃做成4×4mm2的支撑制作了500×500mm2的平面真空玻璃,并进行了太阳能集热实验,“集热性能比双层玻璃优越,集热温度比双层玻璃高15~30”;北京新立基真空玻璃公司称,在北京大学唐健正教授(曾在悉尼大学参与真空玻璃研究)的指导下,用金属做支撑,可生产不同规格的平面真空玻璃。上述两种平面真空玻璃,所用的都是钢性支撑,生产时对各支撑的高度要求绝对一致,否则会使平面真空玻璃受力不均,极易损坏;同时,对平面真空玻璃周边也没有采取保护措施,在搬运和安装的过程中,也容易使平面真空玻璃碰坏而丧失使用价值。针对上述问题,本人曾于2003年10月23日向国家知识产权局申请了名称为“柔性支撑弹力封口的真空玻璃”的实用新型专利,并授予专利权,专利号为ZL200320110369.5,在具体实施时我们发现,由于抽真空接口设在外侧的平面玻璃上,直接影响到真空玻璃的整体美感,同时,该专利主要生产由三层平面玻璃形成两个密封腔的平面玻璃,在生产三层以上平面玻璃形成的多个密封腔的平面玻璃中有一定的难度。
发明内容:
本实用新型的目的在于:针对本人申请的ZL200320110369.5号实用新型专利存在的问题,提供一种新的柔性支撑的真空玻璃。
本实用新型的目的是这样实现的:一种柔性支撑的真空玻璃,包括平面玻璃、支撑,其特征在于:至少含有两块形状相同的平面玻璃,相邻平面玻璃之间至少均匀分布三个相同材料制作的等高的柔性支撑,环绕平面玻璃边缘的缝隙中设有与柔性支撑相同材料制作的等高的柔性支撑条,沿柔性支撑条外侧通过胶粘剂将平面玻璃边缘连接,使相邻平面玻璃之间形成密封腔,相邻平面玻璃之间的柔性支撑条上设有一个抽真空接口,抽真空接口上覆有密封封口剂。
本实用新型的优点在于:保留了ZL200320110369.5号实用新型专利中采用半柔性支撑,避免安装过程中钢性支撑在两块玻璃间滑动,两块玻璃受力均匀,尤其是采用半透明的高分子材料制作柔性支撑,其加工工艺比采用特种玻璃或金属制作的支撑简单,其透光性优于金属支撑的优点,由于抽真空接口的设置隐蔽,生产的真空玻璃更加美观,并能生产三层以上平面玻璃形成的多个密封腔的平面玻璃。
附图说明:
图1是本实用新型一种实施例的截面示意图。
图中:1、平面玻璃,2、柔性支撑,3、柔性支撑条,4、胶粘剂,5、抽真空接口,6、封口剂。
具体实施方式:
附图非限制性地公开了本实用新型的一个具体实施例,下面结合实施例对本实用新型作进一步的分析。
由图1可见,本实用新型至少含有两块形状相同的平面玻璃1,相邻平面玻璃1之间至少均匀分布三个相同材料制作的等高的柔性支撑2,环绕平面玻璃1边缘的缝隙中设有与柔性支撑相同材料制作的等高的柔性支撑条3,沿柔性支撑条3外侧通过胶粘剂5将相邻平面玻璃1边缘连接,使相邻的平面玻璃1之间形成密封腔,相邻平面玻璃1之间的柔性支撑条3上设有一个抽真空接口4,抽完真空后,抽真空接口4上覆有封口剂6。具体实施时,所述的平面玻璃1可以采用浮法平面玻璃,其厚度≥3mm;柔性支撑2和柔性支撑条3均为半透明高分子弹性体,其高度为0.5~1.0mm,所述的胶粘剂5和封口剂6均选用密封胶,柔性支撑的支撑点呈正三角形或正四角形均匀分布,相邻的柔性支撑点之间的距离≤12cm。
在本实施例中,平面玻璃1采用厚度为4mm的三块浮法平面玻璃,相邻平面玻璃1之间柔性支撑2和柔性支撑条3的高度均为0.8mm,三块平面玻璃1形成了两个密封腔,每个密封腔的一根柔性支撑条3上设有一个抽真空接口4,柔性支撑的支撑点呈正三角形均匀分布,相邻的柔性支撑点之间的距离6cm,密封腔的真空度为1.33×10~10-3Pa,被抽真空后,抽真空接口4将通过封口剂6密封。本实施例的使用温度为-60~250℃,经检测,泄漏率为1.33×10-8Pa·L/S。
Claims (4)
1、一种柔性支撑的真空玻璃,包括平面玻璃、柔性支撑、密封胶粘剂,其特征在于:至少含有两块形状相同的平面玻璃,相邻平面玻璃之间至少均匀分布三个相同材料制作的等高的柔性支撑,环绕平面玻璃边缘的缝隙中设有与柔性支撑相同材料制作的等高的柔性支撑条,沿柔性支撑条外侧通过密封胶粘剂将平面玻璃边缘连接,使相邻平面玻璃之间形成密封腔,相邻平面玻璃之间的柔性支撑条上设有一个抽真空接口,抽真空接口上覆有密封封口剂。
2、根据权利要求1所述的柔性支撑的真空玻璃,其特征在于:所述的平面玻璃为浮法平面玻璃,其厚度≥3mm;柔性支撑和柔性支撑条均为半透明高分子弹性体,其高度为0.5~1.0mm。
3、根据权利要求1所述的柔性支撑的真空玻璃,其特征在于:所述的密封胶粘剂和密封封口剂均选用密封胶。
4、根据权利要求1或2或3所述的柔性支撑的真空玻璃,其特征在于:柔性支撑的支撑点呈正三角形或正四角形均匀分布,相邻的柔性支撑点之间的距离≤12cm。