[go: up one dir, main page]

CN2597147Y - Sleeve barrel - Google Patents

Sleeve barrel Download PDF

Info

Publication number
CN2597147Y
CN2597147Y CNU032038658U CN03203865U CN2597147Y CN 2597147 Y CN2597147 Y CN 2597147Y CN U032038658 U CNU032038658 U CN U032038658U CN 03203865 U CN03203865 U CN 03203865U CN 2597147 Y CN2597147 Y CN 2597147Y
Authority
CN
China
Prior art keywords
sleeve
peripheral edge
black
layer
outer peripheral
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNU032038658U
Other languages
Chinese (zh)
Inventor
彭盈豪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changchen International Co ltd
Original Assignee
Changchen International Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changchen International Co ltd filed Critical Changchen International Co ltd
Priority to CNU032038658U priority Critical patent/CN2597147Y/en
Application granted granted Critical
Publication of CN2597147Y publication Critical patent/CN2597147Y/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model relates to a sleeve has a through hole, and its outer peripheral edge has one and dyes black layer, and the outer peripheral edge sets for the position and has a mark depressed grain, the outer peripheral edge of mark depressed grain and the internal periphery of through hole have an electroplating layer respectively, make mark depressed grain and dye black layer between form silver, black alternate form, by this, not only have splendid antirust effect, and mark depressed grain and dye black layer between, form silver, black alternate form, with the telescopic specification of highlighting, size, and can make the user show clearly and see and reach.

Description

一种套筒a sleeve

技术领域technical field

本实用新型涉及一种套筒,特别是一种套筒的规格、尺寸标记得以凸显的套筒。The utility model relates to a sleeve, in particular to a sleeve whose specifications and size marks are highlighted.

背景技术Background technique

请配合参阅图7及附件四所示,传统套筒成型方式是,先以车制加工,成型出一套筒50,使该套筒50具有一大径部51及一小径部52,且该套筒50中央具有一贯通该大径部51及该小径部52的贯孔53,之后,于该套筒50的大径部51位置,以辊压方式辊印出规格、尺寸的标记凹纹54(请配合参阅附件四所示);Please refer to FIG. 7 and Annex 4. The traditional sleeve molding method is to first process a sleeve 50 by turning, so that the sleeve 50 has a large diameter portion 51 and a small diameter portion 52. The center of the sleeve 50 has a through hole 53 passing through the large-diameter portion 51 and the small-diameter portion 52, and then, at the position of the large-diameter portion 51 of the sleeve 50, the marking grooves of specifications and sizes are rolled out by rolling 54 (please refer to Annex 4 for details);

于成型后的套筒50大、小径部51、52的外周缘及贯孔53的内周缘,进行表面电镀处理,使该套筒50的外周缘及内周缘形成一电镀层60,俾具有较佳的防锈功能(请配合参阅附件四右边的套筒实品照片所示);Surface electroplating treatment is carried out on the outer periphery of the large and small diameter parts 51, 52 of the formed sleeve 50 and the inner periphery of the through hole 53, so that an electroplating layer 60 is formed on the outer periphery and the inner periphery of the sleeve 50, so as to have a relatively Excellent anti-rust function (please refer to the photo of the actual sleeve on the right side of Annex 4);

此种传统的套筒表面电镀处理方式,虽然具有防锈的功能,但是,由于标记凹纹54上具有呈银色的电镀层60,与套筒50的大、小径51、52外表面的电镀层60是呈同一色是,使用时,极不易看出该套筒50上的标记凹纹54所显示的套筒50规格、尺寸,造成使用上的困扰。Although this kind of traditional sleeve surface electroplating treatment method has the function of antirust, because there is a silver electroplating layer 60 on the mark concave groove 54, it is different from the electroplating layer on the large and small diameters 51,52 outer surfaces of the sleeve 50. 60 is the same color, when in use, it is extremely difficult to see the specification and size of the sleeve 50 shown by the marked concave groove 54 on the sleeve 50, which causes troubles in use.

另外,有一种藉由磷酸锰渗入套筒50内部的套筒表面处理方法,虽然亦具有前述的防锈功能,但是经过磷酸锰表面处理后的套筒,整体是呈黑色状(请配合参阅附件四左边的套筒实品照片所示),更使得标记凹纹54上的字体变得模糊、不清晰,前述的使用缺失,亦无法有效解决。In addition, there is a sleeve surface treatment method in which manganese phosphate penetrates into the sleeve 50. Although it also has the aforementioned anti-rust function, the sleeve after the manganese phosphate surface treatment is black as a whole (please refer to the attachment 4 shown in the actual product photo of the sleeve on the left side), the font on the mark concave groove 54 becomes fuzzy and unclear, and the aforementioned lack of use cannot be effectively solved.

针对前述两种套筒的表面处理方法,更衍生出利用印刷方式,于套筒的外表面印刷出不同色是的字体,虽然,可解决前述的字体模糊、不清晰的问题,但是,此种套筒经过一段时间的使用之后,会使得印刷的字体产生剥落,乃至于完全被刮除,其所造成的问题更是严重。Regarding the surface treatment methods of the above two sleeves, a printing method is derived to print fonts of different colors on the outer surface of the sleeve. Although it can solve the aforementioned problems of blurred and unclear fonts, this method After the sleeve has been used for a period of time, the printed font will peel off, or even be completely scraped off, which causes even more serious problems.

发明内容Contents of the invention

本实用新型的主要目的是提供一种得以凸显套筒的规格、尺寸相关的标记,令使用者清楚看见及方便操作的套筒。The main purpose of the utility model is to provide a sleeve that can highlight the specifications and dimensions of the sleeve so that users can see it clearly and operate it conveniently.

为达前述的目的,本实用新型提供了一种套筒,该套筒具有一贯孔,且该套筒的外周缘具有一染黑层,而该套筒的外周缘设定位置具有一标记凹纹,该标记凹纹的外周缘及该贯孔的内周缘,分别具有一电镀层,使该标记凹纹与该染黑层之间形成银色、黑色相间的形态,以凸显该标记凹纹。In order to achieve the aforementioned purpose, the utility model provides a sleeve, the sleeve has a through hole, and the outer peripheral edge of the sleeve has a black layer, and the outer peripheral edge of the sleeve has a marking concave The outer peripheral edge of the marked concave grain and the inner peripheral edge of the through hole respectively have an electroplating layer, so that the marking concave grain and the black layer form a silver and black pattern to highlight the marking concave grain.

下面结合附图以具体实例对本实用新型进行详细说明。The utility model will be described in detail below with specific examples in conjunction with the accompanying drawings.

附图说明Description of drawings

图1是本实用新型的流程示意图;Fig. 1 is a schematic flow sheet of the utility model;

图2是本实用新型的套筒外观示意图;Fig. 2 is a schematic diagram of the appearance of the sleeve of the present utility model;

图3是本实用新型进行电镀处理后的剖面示意图;Fig. 3 is the schematic sectional view of the utility model after the electroplating treatment;

图4是本实用新型进行表面研磨处理后的剖面示意图;Fig. 4 is a schematic sectional view of the utility model after the surface grinding treatment;

图5是本实用新型进行表面染黑处理后的剖面示意图;Fig. 5 is a schematic sectional view of the utility model after the surface is blackened;

图6是本实用新型进行表面电着处理后的剖面示意图;Fig. 6 is a schematic cross-sectional view of the utility model after the surface electrodeposition treatment;

图7是现有套筒电镀处理后的剖面示意图;Fig. 7 is a schematic cross-sectional view of an existing sleeve after electroplating;

附件一是本实用新型进行表面处理后的套筒外观示意图;Attachment 1 is a schematic diagram of the appearance of the sleeve after the surface treatment of the utility model;

附件二是本实用新型与现有套筒表面处理后的外观比较示意图(小规格的套筒者);Annex 2 is a schematic diagram of the appearance comparison between the utility model and the existing sleeve after surface treatment (sleeve of small size);

附件三是本实用新型与现有套筒表面处理后的外观比较示意图(大规格的套筒者);Attachment 3 is a schematic diagram of the appearance comparison between the utility model and the existing sleeve after surface treatment (large size sleeve);

附件四是现有套筒表面处理后的外观示意图。Attachment 4 is a schematic diagram of the appearance of the existing sleeve after surface treatment.

具体实施方式Detailed ways

请配合参阅图1至图5所示,本实用新型为一种套筒,该套筒的成型方法包含:套筒外观成型、辊印标记、表面电镀处理、表面研磨处理、表面染黑处理及表面电着处理等步骤,以完成本实用新型的套筒成品(请配合参阅图1所示);其中:Please refer to Fig. 1 to Fig. 5. The utility model is a sleeve. The forming method of the sleeve includes: sleeve appearance forming, roll printing mark, surface electroplating treatment, surface grinding treatment, surface blackening treatment and Steps such as surface electric treatment, to complete the sleeve finished product of the present utility model (please cooperate and refer to shown in Fig. 1); Wherein:

在套筒外观成型步骤中:是以车制加工,成型出一套筒10,该套筒10具有一大径部11及一小径部12,且该套筒10中央具有一贯通该大径部11及该小径部12的贯孔13,而该大径部11的外周缘具有若干止滑沟14(请配合参阅图2所示);In the sleeve appearance forming step: a sleeve 10 is formed by turning, the sleeve 10 has a large diameter part 11 and a small diameter part 12, and the center of the sleeve 10 has a through the large diameter part 11 and the through hole 13 of the small-diameter portion 12, and the outer peripheral edge of the large-diameter portion 11 has some anti-slip grooves 14 (please refer to FIG. 2 for cooperation);

在辊印标记步骤中:将该套筒10的大径部11的设定位置处以辊压方式,辊印出设定的标记凹纹15,该标记凹纹15得以为该套筒10的规格、尺寸(请配合参阅图2所示);In the rolling marking step: the set position of the large-diameter portion 11 of the sleeve 10 is rolled to print the set marking grooves 15, and the marking grooves 15 can be the specifications of the sleeve 10. , size (please refer to Figure 2 for cooperation);

在表面电镀处理步骤中:将该套筒10的大、小径部11、12的外周缘及贯孔13的内周缘,进行表面电镀处理,使该套筒10的外周缘及内周缘形成一电镀层20,俾具有较佳的防锈功能及表面外观(请配合参阅图3所示);In the surface electroplating treatment step: the outer peripheral edges of the large and small diameter parts 11, 12 and the inner peripheral edges of the through holes 13 of the sleeve 10 are subjected to surface electroplating treatment, so that the outer peripheral edge and the inner peripheral edge of the sleeve 10 form a plated surface. Layer 20, in order to have better anti-rust function and surface appearance (please refer to shown in Figure 3);

在表面研磨处理步骤中:将该套筒10的标记凹纹15外周缘进行表面研磨,使该标记凹纹15的电镀层20被磨除(请配合参阅图4所示);In the surface grinding treatment step: surface grinding is carried out on the outer periphery of the marked concave groove 15 of the sleeve 10, so that the electroplating layer 20 of the marked concave groove 15 is ground away (please refer to FIG. 4 for cooperation);

在表面染黑处理步骤中:将该套筒10放置于磷酸锰溶液中,进行磷酸锰处理,令磷酸锰溶液得以渗入不具电镀层20的标记凹纹15的大径部11表面,使之形成一染黑层30(请续配合参阅图5及附件一所示);In the surface blackening treatment step: place the sleeve 10 in a manganese phosphate solution, and perform manganese phosphate treatment, so that the manganese phosphate solution can penetrate into the surface of the large-diameter portion 11 of the marking concave groove 15 without the electroplating layer 20, so that it forms A black layer 30 (please refer to Figure 5 and Annex 1 for further cooperation);

在表面电着处理步骤中:利用表面电着处理,使该套筒10的外周缘形成一保护膜40,使之具有较佳的防锈功能及美化表面外观的功效(请续配合参阅图6及附件一所示),如此,即得以完成套筒10表面处理。In the surface electrodeposition treatment step: use the surface electrodeposition treatment to form a protective film 40 on the outer periphery of the sleeve 10, so that it has better anti-rust function and beautifies the effect of the surface appearance (please continue to refer to Fig. 6 And shown in Annex 1), in this way, the surface treatment of the sleeve 10 can be completed.

藉由以上的表面处理程序,所成型出的套筒10具有一大径部11及一小径部12,该套筒10中央具有一贯通该大径部11及该小径部12的贯孔13,且该套筒10外周缘具有一由磷酸锰渗入表面的染黑层30,该染黑层30的外周缘披覆一保护膜40,而该大径部11的外周缘具有若干止滑沟14,且该大径部11的设定位置具有一可为该套筒10的规格、尺寸的标记凹纹15,该标记凹纹15、小径部12的外周缘及该贯孔13的内周缘分别具有一电镀层20,使该标记凹纹15与该染黑层30之间形成银色、黑色相间的形态,使得以凸显该标记凹纹15。Through the above surface treatment procedures, the molded sleeve 10 has a large diameter portion 11 and a small diameter portion 12, and the sleeve 10 has a through hole 13 in the center of the large diameter portion 11 and the small diameter portion 12, And the outer periphery of the sleeve 10 has a black dyed layer 30 infiltrated into the surface by manganese phosphate, the outer peripheral edge of the black dyed layer 30 is covered with a protective film 40, and the outer peripheral edge of the large diameter portion 11 has a number of non-slip grooves 14 , and the setting position of the large-diameter portion 11 has a marking groove 15 that can be the specification and size of the sleeve 10, the marking groove 15, the outer peripheral edge of the small-diameter portion 12 and the inner peripheral edge of the through hole 13 respectively There is an electroplating layer 20, so that the pattern of silver and black is formed between the marked concave groove 15 and the black dyed layer 30, so that the marked concave groove 15 is highlighted.

请配合参阅附件一及图1、图5所示,利用本实用新型的表面处理方法,所成形出的套筒10,不仅于套筒10的小径部12外周缘及贯孔13的内周缘形成一具有防锈功效的电镀层20,且套筒10的大径部11外周缘形成一磷酸锰的染黑层30,而染黑层30外周缘披覆一保护膜40,使得整个套筒10具有极佳的防锈功效。Please refer to Annex 1 and Fig. 1 and Fig. 5. Using the surface treatment method of the present invention, the formed sleeve 10 is not only formed on the outer peripheral edge of the small diameter portion 12 of the sleeve 10 and the inner peripheral edge of the through hole 13. An electroplating layer 20 with antirust effect, and the outer periphery of the large-diameter portion 11 of the sleeve 10 forms a blackened layer 30 of manganese phosphate, and the outer periphery of the blackened layer 30 is coated with a protective film 40, so that the entire sleeve 10 Has excellent anti-rust effect.

同时,更值得注意的是,经过本实用新型的表面处理方法所成型出的套筒10,于大径部11上具有银色电镀层20的标记凹纹15,及黑色的染黑层30,使标记凹纹15与染黑层30之间形成银色、黑色相间的形态,俾显示套筒10规格、尺寸的标记凹纹15,得以让使用者一眼视及,使用上极具实用性,且与传统的表面处理方法比较,本实用新型所成型出的套筒更具明显的对比(请配合参阅附件二、三所示)。At the same time, it is worth noting that the sleeve 10 formed by the surface treatment method of the present invention has a silver electroplating layer 20 marking concave pattern 15 on the large diameter portion 11, and a black dyed black layer 30, so that Between the marking grooves 15 and the black dyed layer 30, silver and black forms are formed, so that the marking grooves 15 showing the specifications and sizes of the sleeve 10 can be seen by the user at a glance. Compared with the traditional surface treatment method, the sleeve formed by the utility model has a more obvious contrast (please refer to the attachments 2 and 3).

Claims (4)

1、一种套筒,其特征在于该套筒具有一贯孔,且该套筒的外周缘具有一染黑层,而该套筒的外周缘设定位置具有一标记凹纹,该标记凹纹的外周缘及该贯孔的内周缘,分别具有一电镀层,使该标记凹纹与该染黑层之间形成银色、黑色相间的形态,以凸显该标记凹纹。1. A sleeve, characterized in that the sleeve has a through hole, and the outer periphery of the sleeve has a blackened layer, and the set position of the outer periphery of the sleeve has a marking groove, and the marking groove The outer peripheral edge of the through hole and the inner peripheral edge of the through hole respectively have an electroplating layer, so that the pattern of silver and black is formed between the marked concave pattern and the blackened layer, so as to highlight the marked concave pattern. 2、如权利要求1所述的套筒,其中,该套筒的大径部外周缘具有若干止滑沟。2. The sleeve according to claim 1, wherein the outer periphery of the large-diameter portion of the sleeve has several anti-slip grooves. 3、如权利要求1所述的套筒,其中,该染黑层是磷酸锰染黑层。3. The sleeve of claim 1, wherein the black coating is a manganese phosphate black coating. 4、如权利要求1所述的套筒,其中,该染黑层的外周缘披覆一保护膜。4. The sleeve as claimed in claim 1, wherein the outer periphery of the black dyed layer is coated with a protective film.
CNU032038658U 2003-02-14 2003-02-14 Sleeve barrel Expired - Lifetime CN2597147Y (en)