[go: up one dir, main page]

CN115122711A - A plastic honeycomb edge sealing molding process - Google Patents

A plastic honeycomb edge sealing molding process Download PDF

Info

Publication number
CN115122711A
CN115122711A CN202210900611.6A CN202210900611A CN115122711A CN 115122711 A CN115122711 A CN 115122711A CN 202210900611 A CN202210900611 A CN 202210900611A CN 115122711 A CN115122711 A CN 115122711A
Authority
CN
China
Prior art keywords
glue
plastic honeycomb
cross
section
plastic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202210900611.6A
Other languages
Chinese (zh)
Inventor
陈庆双
范文正
张增耀
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Huacheng Industrial Co ltd
Original Assignee
Shenzhen Huacheng Industrial Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Huacheng Industrial Co ltd filed Critical Shenzhen Huacheng Industrial Co ltd
Priority to CN202210900611.6A priority Critical patent/CN115122711A/en
Publication of CN115122711A publication Critical patent/CN115122711A/en
Pending legal-status Critical Current

Abstract

本发明公开了一种塑料蜂窝封边成型工艺,包括以下步骤:1)通过物理的方法,处理塑料蜂窝横截面的表层,增加其受力面积,增强附着力;2)通过化学的方法,处理塑料蜂窝横截面部分,提高塑料蜂窝横截面的极性,增加其附着力;3)使用特制的热融胶水及设备。步骤1中的物理方法是通过特种设备处理的。通过特种设备处理横截面,把横截面蜂窝芯直线结构处理成细孔或微孔状,增加胶水的吃胶面积及受力面积,更利于排气及吃胶的牢固性。步骤2中的化学方法是通过化学试剂氧化的,通过使用强极性特制的热融胶水,通过特殊的封边设备,保证成型过程中封边条与塑料蜂窝芯两面都有胶水相融,才能保证其牢固性,达到了塑料蜂窝封边成型的效果。The invention discloses a plastic honeycomb edge-sealing molding process, which comprises the following steps: 1) by a physical method, the surface layer of the cross section of the plastic honeycomb is treated to increase its stress area and enhance the adhesion; 2) by a chemical method, the surface layer is treated The plastic honeycomb cross-section part increases the polarity of the plastic honeycomb cross-section and increases its adhesion; 3) Use special hot-melt glue and equipment. The physical method in step 1 is handled by special equipment. The cross-section is processed by special equipment, and the straight-line structure of the cross-section honeycomb core is processed into fine pores or micro-pores, which increases the glue-eating area and the force-bearing area of the glue, which is more conducive to the firmness of exhaust and glue-eating. The chemical method in step 2 is oxidized by chemical reagents. By using special hot-melt glue with strong polarity and special edge-sealing equipment, it is ensured that the edge-sealing strip and the plastic honeycomb core are melted with glue on both sides during the molding process. Ensure its firmness and achieve the effect of plastic honeycomb edge sealing.

Description

一种塑料蜂窝封边成型工艺A plastic honeycomb edge sealing molding process

技术领域technical field

本发明涉及塑料蜂窝封边技术领域,具体为一种塑料蜂窝封边成型工艺。The invention relates to the technical field of plastic honeycomb edge sealing, in particular to a plastic honeycomb edge sealing molding process.

背景技术Background technique

塑料蜂窝是采用PVC、PET、PP等塑料片材叠合而成的蜂窝状材料,具有质量轻、强度大等特点。蜂窝孔形态:六角形圆孔半圆槽型。Plastic honeycomb is a honeycomb material made of PVC, PET, PP and other plastic sheets, which has the characteristics of light weight and high strength. Honeycomb hole shape: hexagonal round hole semi-circular groove type.

塑料蜂窝具有质量轻、绝缘性好、耐腐蚀性优越、易加工成型、成本低廉等特点,已广泛用于建筑、日用品、电子等行业。然而其表面能低、极性小、润湿性差及有一定的结晶度,不易与含有极性官能团或极性成分的油漆,胶水等材料直接粘附。塑料(主要是pp)分子无极性,在塑料里面与外物附着力属最差之一,而其通过横截面封边更是把这个难度提高了一个等级,横截面封边具有受力面积小,不好受力成型等特点,使得封边的难度进一步提高。Plastic honeycomb has the characteristics of light weight, good insulation, excellent corrosion resistance, easy processing and molding, and low cost. It has been widely used in construction, daily necessities, electronics and other industries. However, its surface energy is low, its polarity is small, its wettability is poor, and it has a certain degree of crystallinity, so it is not easy to directly adhere to materials such as paints and glues containing polar functional groups or polar components. Plastic (mainly pp) molecules are non-polar, and the adhesion to foreign objects in plastic is one of the worst, and its cross-section edge sealing increases the difficulty to a level, and the cross-section edge sealing has a small stress area. , it is not easy to be subjected to force forming and other characteristics, which further increases the difficulty of edge sealing.

发明内容SUMMARY OF THE INVENTION

(一)解决的技术问题(1) Technical problems solved

针对现有技术的不足,本发明提供了一种塑料蜂窝封边成型工艺,解决了上述背景所提出的问题。In view of the deficiencies of the prior art, the present invention provides a plastic honeycomb edge sealing molding process, which solves the problems raised by the above background.

(二)技术方案(2) Technical solutions

为实现上述目的,本发明提供如下技术方案:一种塑料蜂窝封边成型工艺,包括以下步骤:In order to achieve the above purpose, the present invention provides the following technical solutions: a plastic honeycomb edge sealing molding process, comprising the following steps:

1)通过物理的方法,处理塑料蜂窝横截面的表层,增加其受力面积,增强附着力;1) Through physical methods, the surface layer of the plastic honeycomb cross section is treated to increase its stress area and enhance adhesion;

2)通过化学的方法,处理塑料蜂窝横截面部分,提高塑料蜂窝横截面的极性,增加其附着力;2) Process the cross-section of the plastic honeycomb by chemical methods, improve the polarity of the cross-section of the plastic honeycomb, and increase its adhesion;

3)使用特制的热融胶水及设备。3) Use special hot melt glue and equipment.

优选的,步骤1中的物理方法是通过特种设备处理的。Preferably, the physical method in step 1 is processed by special equipment.

优选的,通过特种设备处理横截面,把横截面蜂窝芯直线结构处理成细孔或微孔状,增加胶水的吃胶面积及受力面积,更利于排气及吃胶的牢固性。Preferably, the cross-section is processed by special equipment, and the straight-line structure of the cross-section honeycomb core is processed into pores or micropores, so as to increase the glue-eating area and the force-bearing area of the glue, which is more conducive to the firmness of exhaust and glue-eating.

优选的,步骤2中的化学方法是通过化学试剂氧化的。Preferably, the chemical method in step 2 is oxidation by chemical reagents.

优选的,通过化学试剂氧化,增加塑料蜂窝表面的表面能,增加其吸附力,为进一步胶水的渗透融合,提高更大的可能性。Preferably, the surface energy of the plastic honeycomb surface is increased by chemical reagent oxidation, and its adsorption force is increased, so as to improve the possibility of further penetration and fusion of glue.

优选的,根据步骤3通过特殊的封边设备,保证成型过程中封边条与塑料蜂窝芯两面都有胶水相融,才能保证其牢固性。Preferably, according to step 3, special edge-sealing equipment is used to ensure that the edge-sealing strip and the plastic honeycomb core are melted with glue on both sides during the molding process, so as to ensure its firmness.

优选的,所述胶水为为一种强极性胶水,与塑料材质的材料特性相适应。Preferably, the glue is a strong polar glue, which is compatible with the material properties of the plastic material.

(三)有益效果(3) Beneficial effects

与现有技术相比,本发明提供了一种塑料蜂窝封边成型工艺,具备以下有益效果:Compared with the prior art, the present invention provides a plastic honeycomb edge sealing molding process, which has the following beneficial effects:

1、该一种塑料蜂窝封边成型工艺,通过使用特种设备进行物理处理的方法,处理塑料蜂窝横截面的表层,增加其受力面积,增强附着力,从而把横截面蜂窝芯直线结构处理成细孔或微孔状,增加胶水的吃胶面积及受力面积,更利于排气及吃胶的牢固性,达到了便于使用的效果。1. This plastic honeycomb edge sealing molding process uses special equipment for physical treatment to treat the surface layer of the plastic honeycomb cross section, increase its force area, and enhance the adhesion, so as to process the cross section honeycomb core linear structure into a Porous or micro-porous, increase the glue-eating area and force-bearing area of the glue, which is more conducive to the firmness of exhaust and glue-eating, and achieves the effect of being easy to use.

2、该一种塑料蜂窝封边成型工艺,通过使用化学试剂氧化,处理塑料蜂窝横截面部分,提高塑料蜂窝横截面的极性,增加其附着力,从而增加塑料蜂窝表面的表面能,增加其吸附力,为进一步胶水的渗透融合,提高更大的可能性,达到了便于使用的效果。2. This plastic honeycomb edge sealing molding process uses chemical reagents to oxidize, process the cross-sectional part of the plastic honeycomb, improve the polarity of the cross-section of the plastic honeycomb, and increase its adhesion, thereby increasing the surface energy of the plastic honeycomb surface and increasing its Adsorption force, in order to further the penetration and fusion of glue, improve the possibility of greater use, and achieve the effect of ease of use.

3、该一种塑料蜂窝封边成型工艺,通过使用强极性特制的热融胶水,通过特殊的封边设备,保证成型过程中封边条与塑料蜂窝芯两面都有胶水相融,才能保证其牢固性,达到了塑料蜂窝封边成型的效果。3. This plastic honeycomb edge-sealing molding process uses special hot-melt glue with strong polarity and special edge-sealing equipment to ensure that the edge-sealing strip and the plastic honeycomb core are melted with glue on both sides during the molding process. Its firmness achieves the effect of plastic honeycomb edge sealing.

具体实施方式Detailed ways

下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。The technical solutions in the embodiments of the present invention will be described clearly and completely below. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative efforts shall fall within the protection scope of the present invention.

在本发明的描述中,需要理解的是,术语“中心”、“纵向”、“横向”、“长度”、“宽度”、“厚度”、“上”、“下”、“前”、“后”、“左”、“右”、“竖直”、“水平”、“顶”、“底”“内”、“外”、“顺时针”、“逆时针”、“轴向”、“径向”、“周向”等指示的方位或位置关系,仅是为了便于描述本发明和简化描述,而不是指示或暗示所指的装置或元件必须具有特定的方位、以特定的方位构造和操作,因此不能理解为对本发明的限制。In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", " Rear, Left, Right, Vertical, Horizontal, Top, Bottom, Inner, Outer, Clockwise, Counterclockwise, Axial, The orientations or positional relationships indicated by "radial direction", "circumferential direction", etc. are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the referred device or element must have a specific orientation or be configured in a specific orientation and operation, and therefore should not be construed as limiting the present invention.

在本发明中,除非另有明确的规定和限定,术语“安装”、“相连”、“连接”、“固定”等术语应做广义理解,例如,可以是固定连接,也可以是可拆卸连接,或成一体;可以是机械连接,也可以是电连接;可以是直接相连,也可以通过中间媒介间接相连,可以是两个元件内部的连通或两个元件的相互作用关系。对于本领域的普通技术人员而言,可以根据具体情况理解上述术语在本发明中的具体含义。In the present invention, unless otherwise expressly specified and limited, the terms "installed", "connected", "connected", "fixed" and other terms should be understood in a broad sense, for example, it may be a fixed connection or a detachable connection , or integrated; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the internal connection of the two elements or the interaction relationship between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific situations.

本发明提供一种技术方案:一种塑料蜂窝封边成型工艺,包括以下步骤:The invention provides a technical solution: a plastic honeycomb edge sealing molding process, comprising the following steps:

1)通过物理的方法,处理塑料蜂窝横截面的表层,增加其受力面积,增强附着力;1) Through physical methods, the surface layer of the plastic honeycomb cross section is treated to increase its stress area and enhance adhesion;

2)通过化学的方法,处理塑料蜂窝横截面部分,提高塑料蜂窝横截面的极性,增加其附着力;2) Process the cross-section of the plastic honeycomb by chemical methods, improve the polarity of the cross-section of the plastic honeycomb, and increase its adhesion;

3)使用特制的热融胶水及设备。3) Use special hot melt glue and equipment.

步骤1中的物理方法是通过特种设备处理的。The physical method in step 1 is handled by special equipment.

通过特种设备处理横截面,把横截面蜂窝芯直线结构处理成细孔或微孔状,增加胶水的吃胶面积及受力面积,更利于排气及吃胶的牢固性。The cross-section is processed by special equipment, and the straight-line structure of the honeycomb core of the cross-section is processed into a fine hole or a microporous shape, which increases the glue-eating area and the force-bearing area of the glue, which is more conducive to the firmness of exhaust and glue-eating.

步骤2中的化学方法是通过化学试剂氧化的。The chemical method in step 2 is oxidation by chemical reagents.

通过化学试剂氧化,增加塑料蜂窝表面的表面能,增加其吸附力,为进一步胶水的渗透融合,提高更大的可能性。Through the oxidation of chemical reagents, the surface energy of the plastic honeycomb surface is increased, its adsorption force is increased, and the possibility of further penetration and fusion of glue is improved.

根据步骤3通过特殊的封边设备,保证成型过程中封边条与塑料蜂窝芯两面都有胶水相融,才能保证其牢固性。According to step 3, special edge sealing equipment is used to ensure that the edge sealing strip and the plastic honeycomb core are melted with glue on both sides during the molding process, so as to ensure its firmness.

胶水为为一种强极性胶水,与塑料材质的材料特性相适应。The glue is a kind of strong polar glue, which is suitable for the material properties of the plastic material.

本发明的有益效果是:The beneficial effects of the present invention are:

通过使用特种设备进行物理处理的方法,处理塑料蜂窝横截面的表层,增加其受力面积,增强附着力,从而把横截面蜂窝芯直线结构处理成细孔或微孔状,增加胶水的吃胶面积及受力面积,更利于排气及吃胶的牢固性,达到了便于使用的效果。By using special equipment for physical treatment, the surface layer of the plastic honeycomb cross-section is treated to increase its stress area and enhance the adhesion, so as to process the straight-line structure of the cross-section honeycomb core into pores or micropores, and increase the glue sticking. The area and the force-bearing area are more conducive to the firmness of the exhaust and the glue, which achieves the effect of being easy to use.

通过使用化学试剂氧化,处理塑料蜂窝横截面部分,提高塑料蜂窝横截面的极性,增加其附着力,从而增加塑料蜂窝表面的表面能,增加其吸附力,为进一步胶水的渗透融合,提高更大的可能性,达到了便于使用的效果。By using chemical reagents to oxidize and treat the cross-section of the plastic honeycomb, improve the polarity of the plastic honeycomb cross-section and increase its adhesion, thereby increasing the surface energy of the plastic honeycomb surface, increasing its adsorption force, and improving the penetration and fusion of glue. Great possibility to achieve the effect of ease of use.

通过使用强极性特制的热融胶水,通过特殊的封边设备,保证成型过程中封边条与塑料蜂窝芯两面都有胶水相融,才能保证其牢固性,达到了塑料蜂窝封边成型的效果。Through the use of special hot-melt glue with strong polarity and special edge-sealing equipment, it is ensured that the edge-sealing strip and the plastic honeycomb core are melted with glue on both sides during the molding process, so as to ensure its firmness and achieve the plastic honeycomb edge-sealing molding. Effect.

尽管已经示出和描述了本发明的实施例,对于本领域的普通技术人员而言,可以理解在不脱离本发明的原理和精神的情况下可以对这些实施例进行多种变化、修改、替换和变型,本发明的范围由所附权利要求及其等同物限定。Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, and substitutions can be made in these embodiments without departing from the principle and spirit of the invention and modifications, the scope of the present invention is defined by the appended claims and their equivalents.

Claims (7)

1. A plastic honeycomb edge sealing and forming process is characterized by comprising the following steps:
1) the surface layer of the cross section of the plastic honeycomb is processed by a physical method, so that the stress area of the surface layer is increased, and the adhesive force is enhanced;
2) the cross section part of the plastic honeycomb is treated by a chemical method, so that the polarity of the cross section of the plastic honeycomb is improved, and the adhesive force of the cross section is increased;
3) special hot melt glue and equipment are used.
2. The process of claim 1, wherein the physical method of step 1 is performed by special equipment.
3. The plastic honeycomb edge sealing and forming process according to claim 1, wherein the cross section is processed by special equipment, the linear structure of the honeycomb core of the cross section is processed into pores or micropores, the glue-eating area and the stress area of the glue are increased, and the firmness of air exhaust and glue eating is facilitated.
4. The process of claim 1, wherein the chemical method in step 2 is oxidation by a chemical agent.
5. The process of claim 4, wherein the oxidation by a chemical agent increases the surface energy of the surface of the plastic honeycomb, increases the adsorption capacity of the plastic honeycomb, and increases the possibility of further glue penetration and fusion.
6. The plastic honeycomb edge sealing and forming process of claim 1, wherein the firmness of the edge sealing strip and the plastic honeycomb core can be ensured only by ensuring that glue is melted on both surfaces of the edge sealing strip and the plastic honeycomb core in the forming process through special edge sealing equipment according to the step 3.
7. The process of claim 6, wherein the glue is a strong polar glue adapted to the material properties of the plastic material.
CN202210900611.6A 2022-07-28 2022-07-28 A plastic honeycomb edge sealing molding process Pending CN115122711A (en)