[go: up one dir, main page]

CN108912902A - A kind of reality color bottom paint and preparation method thereof - Google Patents

A kind of reality color bottom paint and preparation method thereof Download PDF

Info

Publication number
CN108912902A
CN108912902A CN201710281699.7A CN201710281699A CN108912902A CN 108912902 A CN108912902 A CN 108912902A CN 201710281699 A CN201710281699 A CN 201710281699A CN 108912902 A CN108912902 A CN 108912902A
Authority
CN
China
Prior art keywords
parts
agent
stirring
revs
color bottom
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710281699.7A
Other languages
Chinese (zh)
Inventor
孟奎
孟运
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hu Baoxin Materials Science And Technology (shanghai) Ltd By Share Ltd
Original Assignee
Hu Baoxin Materials Science And Technology (shanghai) Ltd By Share Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hu Baoxin Materials Science And Technology (shanghai) Ltd By Share Ltd filed Critical Hu Baoxin Materials Science And Technology (shanghai) Ltd By Share Ltd
Priority to CN201710281699.7A priority Critical patent/CN108912902A/en
Publication of CN108912902A publication Critical patent/CN108912902A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of real color bottom paint and preparation method thereof, the following component including parts by weight:20-25 parts of water, 0.5-0.6 parts of dispersing agent, 0.1-0.2 parts of wetting agent, 0.2-0.3 parts of hydroxyethyl cellulose, 0.3-0.4 parts of defoaming agent, 45-48 parts of pigments and fillers, 16-20 parts of high TG modified acrylic acid emulsion, 2-3 parts of decylene glycol ester, 1.5-2.5 parts of ethylene glycol, 0.2-0.4 parts of preservative, 0.05-0.1 parts of adhesion promoter, 0.5-1 parts of thickener, 3-5 parts of quartz sand, 0.1-0.15 parts of pH adjusting agent;Real color bottom paint good penetrability of the invention, adhesive force is strong, and it is strong that anti-U.S. line paper tears ability.

Description

A kind of reality color bottom paint and preparation method thereof
Technical field
The present invention relates to decorative materials technologies more particularly to a kind of real color bottom paint and preparation method thereof.
Background technique
At present, it is common to use real color bottom paint be made of the raw material of following mass fraction:20-25 parts of water, dispersing agent 0.5- 0.6 part, 0.2-0.3 parts of hydroxyethyl cellulose, 0.1-0.2 parts of wetting agent, 0.1-0.2 parts of pH adjusting agent, defoaming agent 0.3-0.4 Part, 30-35 parts of pigments and fillers, dedicated acrylic emulsion 30-40 parts of priming paint, 2-3 parts of decylene glycol ester, 1.5-2.5 parts of ethylene glycol, anti-corrosion 0.2-0.4 parts of agent, 0.5-1 parts of thickener.
There are the following problems for above-mentioned reality color bottom paint:
1)Lotion additive amount is big, and the additive amount of pigments and fillers cannot be too many, otherwise higher cost;If traditional reality color bottom paint lotion adds Dosage is low, will lead to the raising of coating pigment if pigments and fillers additive amount is excessive, and the adding proportion of coating film forming matter is reduced, led The adhesive force of priming paint and substrate is caused to reduce, the anti-accumulation of salt in the surface soil resistance to salting-out miopragia of priming paint;
2)It is limited by itself film forming matter, penetration is poor, and alkali resistance is weak;
3)Low with substrate adhesion strength, poor adhesive force, it is poor that anti-U.S. line paper tears ability, and priming paint box putty is easy to tear.
Summary of the invention
For poor, the poor adhesive force that solves priming paint penetration in the prior art, anti-U.S. line paper tears the problem of ability difference, The purpose of invention is to provide a kind of real color bottom paint, has high osmosis, excellent with substrate binding force, and it is anti-to be highly resistant to jointing paint U.S. line paper is torn;For this purpose, the present invention will also provide the preparation method of the reality color bottom paint.
To achieve the goals above, the present invention adopts the following technical scheme that:
The first aspect of the present invention provides a kind of real color bottom paint, the following component including parts by weight:
20-25 parts of water
0.5-0.6 parts of dispersing agent
0.1-0.2 parts of wetting agent
0.2-0.3 parts of hydroxyethyl cellulose
0.3-0.4 parts of defoaming agent
45-48 parts of pigments and fillers
16-20 parts of high TG modified acrylic acid emulsion
2-3 parts of decylene glycol ester
1.5-2.5 parts of ethylene glycol
0.2-0.4 parts of preservative
0.05-0.1 parts of adhesion promoter
0.5-1 parts of thickener
3-5 parts of quartz sand
0.1-0.15 parts of pH adjusting agent.
High TG modified acrylic acid emulsion is that emulsion particle diameter is small, and the high acrylic emulsion of glass transition temperature is multiple with other auxiliary agents With coating is improved to the permeability of substrate, the adhesion strength with substrate is increased, adhesive force is good.
Wherein, adhesion promoter is organic silicon auxiliary agent, with high TG modified acrylic acid emulsion collective effect, enhances coating The adhesive force of coating.
Wherein, the pigments and fillers are titanium dioxide and powdered whiting or are titanium dioxide, powdered whiting, talcum powder three Mixture.
Wherein, the quartz sand is the quartz sand of 80-120 mesh.
Using the fine quartz sand of 80-120 mesh, the roughness on film surface layer is increased, reduces connecing for U.S. line paper and film Contacting surface product, weakens mastication forces.
The second aspect of the present invention provides the preparation method of above-mentioned real color bottom paint, includes the following steps:
Water is added in S1 in the reactor, stirring, and mixing speed is 500 revs/min, and mixing time is 3-5 minutes;
S2 sequentially adds dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent, pH adjusting agent, stirring, stirring into reactor Speed is 500-800 revs/min, and mixing time is 10-15 minutes;
S3 sequentially adds pigments and fillers into reactor, stirring, and mixing speed is 1000-1200 revs/min, mixing time 25-30 Minute;
S4 sequentially adds high TG modified acrylic acid emulsion under 300-500 revs/min of mixing speed, decylene glycol ester, ethylene glycol, Adhesion promoter, preservative, thickener stir 10-15 minutes;
S5 is added quartz sand, is uniformly dispersed.
Sequentially add dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent and pH adjusting agent in S2 step, it is pre-dispersed at Slurry, provides wetting and dispersing system for S3 step high speed dispersion pigments and fillers;Pigments and fillers are added in S3 step, and fineness is made in high speed dispersion Qualified white slurry;Using the original for being added separately to pigments and fillers and high TG modified acrylic acid emulsion, coalescing agent, ethylene glycol etc. Because being, pigments and fillers need high speed dispersion, and high speed dispersion can improve the risk of emulsion breaking, in addition, high speed dispersion can also be led It causes system temperature to increase, aggravates the volatilization of coalescing agent and ethylene glycol, also will affect the performance of preservative.
S2 step uses 500-800 revs/min of revolving speed, this step belongs to middling speed dispersion, convenient for hydroxyethyl ether cellulose Sufficiently dissolution;If revolving speed is too low, cause jitter time too long;If revolving speed is too high, highly viscous hydroxyethyl ether cellulose can be generated A large amount of bubbles are not easy to abolish.
S3 step uses 1000-1200 revs/min of revolving speed, this step belongs to high speed dispersion, since the step joined face Filler, it is necessary to which high speed dispersion is so that pigments and fillers by high speed shear, reach fineness range as defined in coating.
S4 step uses 300-500 revs/min of revolving speed, this step belongs to low speed dispersion, since the step joined high TG Modified acrylic acid emulsion and auxiliary agent, rate of dispersion are unsuitable excessively high;If rate of dispersion is too fast, constant temperature is increased, and auxiliary agent can be quick Volatilization, is unfavorable for stable system;Disperse according to high speed, more bubbles can be generated in dispersion process, be unfavorable for system and disappear Bubble, high speed dispersion can also bring emulsion breaking problem.
Wherein, further include the steps that the system after stirring S4 is transferred to texture paint Special dispersing cylinder before the S5.
S1-S4 step is in coating special cylinder, and the dispersion impeller of the equipment is gear-like high speed shear dispersion impeller, motor Power is small, and the rate of dispersion of sand is slow, influences reaction efficiency;Texture paint Special dispersing cylinder is helical form dispersion impeller, rate of dispersion It is moderate, will not bring high speed shear that quartz sand particle size is brought to become smaller, system temperature increase the problems such as;In addition, the addition of quartz sand System viscosity is brought to increase, dispersion resistance increases, and using texture paint Special dispersing cylinder, disperses more uniform.
Compared with prior art, the beneficial effect that the present invention realizes:The anti-accumulation of salt in the surface soil resistance to salting-out of real color bottom paint of the invention, infiltration Property it is good, adhesive force is strong, and to tear ability strong for anti-U.S. line paper;Real color bottom paint of the invention is in the increase of pigments and fillers usage amount, lotion dosage In the case where reduction, it may have strong adhesive force overcomes the technology prejudice that pigments and fillers usage amount increase causes adhesive force to reduce;This Used acrylic emulsion is few during the preparation process for the real color bottom paint of invention, using conventional formulation 1 ton of priming paint of every production, needs Cost be 4200 yuan, using formula of the invention, 1 ton of priming paint of every production, need cost be 3000 yuan, 1200 yuan of save the cost, In Shanghai, the dosage of annual priming paint is 100,000 t, and using formula of the invention, save the cost is 1.2 hundred million yuan altogether.
Specific embodiment
Embodiment 1
The preparation method of real color bottom paint, includes the following steps:
S1 weighs 2000g water, 50g dispersing agent(The 5040 of Nuo Pu section), 15g wetting agent(The PE100 of Corning), 25g ethoxy fibre Dimension element, 35g defoaming agent, 4500g pigments and fillers(Climb the R-258 titanium dioxide and powdered whiting of steel), 1600g high TG modified acroleic acid Lotion(The hundred of the Dow Chemical Company's production, which go through, to rub), 250g decylene glycol ester, 200g ethylene glycol, 20g preservative(The MBS of Sol company), 5g adhesion promoter(The MP200 adhesion promoter of Mai Tu company of the U.S.), 50g thickener(The TT935 of Tao Shi), 400g stone Sand, 10g pH adjusting agent(The AMP95 of Tao Shi);
Water is added in S2 in the reactor, stirring, and mixing speed is 500 revs/min, and mixing time is 3 minutes;
S3 sequentially adds dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent, pH adjusting agent, stirring, stirring into reactor Speed is 600 revs/min, and mixing time is 10 minutes;
S4 sequentially adds pigments and fillers into reactor, stirring, and mixing speed is 1000 revs/min, and mixing time is 25 minutes;
S5 sequentially adds high TG modified acrylic acid emulsion, decylene glycol ester, ethylene glycol, attachment under 300 revs/min of mixing speed Power promotor, preservative, thickener stir 10 minutes.
Embodiment 2
The preparation method of real color bottom paint, includes the following steps:
S1 weighs 2500g water, 55g dispersing agent(The 5040 of Nuo Pu section), 10g wetting agent(The PE100 of Corning), 20g ethoxy fibre Dimension element, 30g defoaming agent, 4600g pigments and fillers(Climb the R-258 titanium dioxide and powdered whiting of steel), 2000g high TG modified acroleic acid Lotion(It goes through and rubs for the hundred of the Dow Chemical Company's production), 200g decylene glycol ester, 150g ethylene glycol, 25g preservative(Sol company MBS), 8g adhesion promoter(The MP200 adhesion promoter of Mai Tu company of the U.S.), 80g thickener(The TT935 of Tao Shi), 300g quartz sand, 12g pH adjusting agent(The AMP95 of Tao Shi);
Water is added in S2 in the reactor, stirring, and mixing speed is 500 revs/min, and mixing time is 4 minutes;
S3 sequentially adds dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent, pH adjusting agent, stirring, stirring into reactor Speed is 500 revs/min, and mixing time is 15 minutes;
S4 sequentially adds pigments and fillers into reactor, stirring, and mixing speed is 1200 revs/min, and mixing time is 30 minutes;
S5 sequentially adds high TG modified acrylic acid emulsion, decylene glycol ester, ethylene glycol, attachment under 500 revs/min of mixing speed Power promotor, preservative, thickener stir 15 minutes.
Embodiment 3
The preparation method of real color bottom paint, includes the following steps:
S1 weighs 2200g water, 60g dispersing agent(The 5040 of Nuo Pu section), 20g wetting agent(The PE100 of Corning), 30g ethoxy fibre Dimension element, 40g defoaming agent, 4800g pigments and fillers(Climb the R-258 titanium dioxide and powdered whiting of steel), 1800g high TG modified acroleic acid Lotion(It goes through and rubs for the hundred of the Dow Chemical Company's production), 300g decylene glycol ester, 250g ethylene glycol, 40g preservative(Sol company MBS), 10g adhesion promoter(The MP200 adhesion promoter of Mai Tu company of the U.S.), 100g thickener(Tao Shi's TT935), 500g quartz sand, 15g pH adjusting agent(The AMP95 of Tao Shi);
Water is added in S2 in the reactor, stirring, and mixing speed is 500 revs/min, and mixing time is 5 minutes;
S3 sequentially adds dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent, pH adjusting agent, stirring, stirring into reactor Speed is 800 revs/min, and mixing time is 12 minutes;
S4 sequentially adds pigments and fillers into reactor, stirring, and mixing speed is 1100 revs/min, and mixing time is 25 minutes;
S5 sequentially adds high TG modified acrylic acid emulsion, decylene glycol ester, ethylene glycol, attachment under 400 revs/min of mixing speed Power promotor, preservative, thickener stir 12 minutes.
Real color bottom paint prepared by embodiment 1-3, which carries out anti-U.S. line paper mastication forces test and anti-accumulation of salt in the surface soil salting-out resistance, to be surveyed Examination.
The anti-U.S. line paper mastication forces test of the real color bottom paint of the present invention and traditional primer base, test are carried out according to GB210-85 The results are shown in Table 1.
Table 1
Traditional primer base Embodiment 1 Embodiment 2 Embodiment 3
Priming paint large area falls off Nothing falls off Sporadicly fall off Nothing falls off
Such as table 1, reality color bottom paint prepared by the present invention is not in that priming paint falls off or bottom when carrying out anti-U.S. line paper mastication forces test Sporadicly falling off occurs in paint, and shows that priming paint adhesive force is strong, and anti-U.S. line paper is torn.
The anti-accumulation of salt in the surface soil resistance to salting-out performance test of primer base of the present invention, test result such as table are carried out according to JG/T210-2007 Shown in 2.
Table 2
As a result
Anti- accumulation of salt in the surface soil test 72h is without exception
Resistance to salting-out test 72h is without exception
The above specific embodiments are only exemplary, is to preferably make skilled artisans appreciate that this is special Benefit, be not to be construed as include to this patent range limitation;As long as any made by the spirit according to disclosed in this patent Equivalent change or modification, each fall within the range that this patent includes.

Claims (5)

1. a kind of reality color bottom paint, which is characterized in that the following component including parts by weight:
20-25 parts of water
0.5-0.6 parts of dispersing agent
0.1-0.2 parts of wetting agent
0.2-0.3 parts of hydroxyethyl cellulose
0.3-0.4 parts of defoaming agent
45-48 parts of pigments and fillers
16-20 parts of high TG modified acrylic acid emulsion
2-3 parts of decylene glycol ester
1.5-2.5 parts of ethylene glycol
0.2-0.4 parts of preservative
0.05-0.1 parts of adhesion promoter
0.5-1 parts of thickener
3-5 parts of quartz sand
0.1-0.15 parts of pH adjusting agent.
2. reality color bottom paint as described in claim 1, which is characterized in that the pigments and fillers be titanium dioxide and powdered whiting or For titanium dioxide, powdered whiting, talcum powder three mixture.
3. reality color bottom paint as described in claim 1, which is characterized in that the quartz sand is the quartz sand of 80-120 mesh.
4. a kind of preparation method of the described in any item real color bottom paints of claim 1-3, which is characterized in that include the following steps:
Water is added in S1 in the reactor, stirring, and mixing speed is 500 revs/min, and mixing time is 3-5 minutes;
S2 sequentially adds dispersing agent, wetting agent, hydroxyethyl cellulose, defoaming agent, pH adjusting agent, stirring, stirring into reactor Speed is 500-800 revs/min, and mixing time is 10-15 minutes;
S3 sequentially adds pigments and fillers into reactor, stirring, and mixing speed is 1000-1200 revs/min, mixing time 25-30 Minute;
S4 sequentially adds high TG modified acrylic acid emulsion under 300-500 revs/min of mixing speed, decylene glycol ester, ethylene glycol, Adhesion promoter, preservative, thickener stir 10-15 minutes;
S5 is added quartz sand, is uniformly dispersed.
5. preparation method as claimed in claim 4, which is characterized in that further include the system turn after stirring S4 before the S5 The step of entering texture paint Special dispersing cylinder.
CN201710281699.7A 2017-04-26 2017-04-26 A kind of reality color bottom paint and preparation method thereof Pending CN108912902A (en)