[go: up one dir, main page]

CN105088395A - Mildew-proof spinnable down feather composite fabric - Google Patents

Mildew-proof spinnable down feather composite fabric Download PDF

Info

Publication number
CN105088395A
CN105088395A CN201510459773.0A CN201510459773A CN105088395A CN 105088395 A CN105088395 A CN 105088395A CN 201510459773 A CN201510459773 A CN 201510459773A CN 105088395 A CN105088395 A CN 105088395A
Authority
CN
China
Prior art keywords
feather
parts
mildew
performance
subsequent use
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510459773.0A
Other languages
Chinese (zh)
Inventor
储荣生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Limited Co Is Spun By Anhui Swan Man
Original Assignee
Limited Co Is Spun By Anhui Swan Man
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Limited Co Is Spun By Anhui Swan Man filed Critical Limited Co Is Spun By Anhui Swan Man
Priority to CN201510459773.0A priority Critical patent/CN105088395A/en
Publication of CN105088395A publication Critical patent/CN105088395A/en
Pending legal-status Critical Current

Abstract

The invention discloses mildew-proof spinnable down feather composite fabric. The fabric is characterized by comprising, by weight, 40-60 parts of poultry feathers, 14-17 parts of down feathers, 1-3 parts of silane coupling agent KH550, 1-2 parts of nano-silica, 1-2 parts of nano-silver, 14-20 parts of chitosan, 30-50 parts of polypropylene, 1-3 parts of spun silk fiber, 2-3 parts of folium artemisiae argyi charcoal, 1-2 parts of bamboo leaf powder and an appropriate amount of water. The added folium artemisiae argyi charcoal, spun silk fiber and bamboo leaf powder improve the bactericidal performance, antiseptic performance, healthcare performance, mildew-proof performance and antibacterial performance of the down feather composite fabric greatly. In prepared down feather composite fiber, the feathers, the down feathers, the chitosan and the polypropylene are proportionally mixed and have complementary advantages, and the prepared spinning material has excellent performance in various aspects, meets the demands of people for fashion, healthcare, color and comfort and is worthy of popularization.

Description

A kind of mildew-resistant eider down compound can weaving face fabric
Technical field
The present invention relates to textile material technical field, being specifically related to a kind of mildew-resistant eider down compound can weaving face fabric and preparation method thereof.
Background technology
In textile industry, only have Isotactic polypropylene can be used to produce textile fabric, this is because Isotactic polypropylene fiber has higher degree of crystallinity and the degree of orientation, regularity is better.Therefore Isotactic polypropylene fiber is widely used as sewing thread, bandage, textile bags and bio-medical material.But because Isotactic polypropylene fiber lacks dyeability, limit its application in textile garment field.Eider down is a kind of natural protein fibre material, except a small amount of for making warming packing material in clothes and bedding and in the composite as except reinforcing material, major part just simple processing process is used as feed or adopts the methods such as fermentation to degrade, and causes a large amount of wastes.When fiber made separately by eider down, fragility is large, tensile strength is low, is not suitable for making coat, is only suitable for being filled in inside clothes obtaining very strong warmth retention property, because eider down content in feather is very few, usually only account for 20 ~ 25%, use cost is too high, feather fiber is not utilized very well, very unfortunately.The present invention utilizes discarded feather to be degraded into keratin solution, then with the chitosan solution blend spinning of modification, compatibility is good, recycling Isotactic polypropylene fills feather fiber, reduce the consumption of feather, gain in weight, and improve the performance of the aspects such as the intensity of fiber, modulus, heat resistance, chemical resistance and anti-corrosive properties, develop novel weaving face fabric, facilitate society and expanding economy.
Summary of the invention
The object of this invention is to provide a kind of mildew-resistant eider down compound can weaving face fabric and preparation method thereof, to overcome the deficiencies in the prior art.
The object of the invention is to be realized by following technological means:
A kind of mildew-resistant eider down compound can weaving face fabric, it is characterized in that, be made up of the raw material of following weight portion: poultry feather 40-60, eider down 14-17, Silane coupling agent KH550 1-3, nano silicon 1-2, Nano Silver 1-2, shitosan 14-20, polypropylene 30-50, silk flock 1-3, charred FOLIUM ARTEMISIAE ARGYI 2-3, bamboo leaf powder 1-2, water are appropriate;
A kind of mildew-resistant eider down compound of the present invention can weaving face fabric, is made up of following concrete steps:
(1) poultry feather and feather stem are separated, use clear water rinsed clean respectively, dry, carry out processed, feather extruding is separated, and feather stem carries out torsion extruding, sterilizing and deodorization under 100-200 ° of C in high-pressure sterilizing pot is added to eider down mixing after again feather and feather stem being cut into mean size, after spontaneous combustion cooling, mixing feather material is placed in alcohol and soaks 4-6 hour, then be neutral post-drying with clear water washing surface, be ground into powder for subsequent use;
(2) Silane coupling agent KH550 appropriate isopropyl alcohol dissolving is placed in reaction vessel, add nano silicon, Nano Silver again, stirring and refluxing 1-3h under 70-90 ° of C, cooling, for subsequent use after suction filtration, washing, drying, again shitosan glacial acetic acid solution is dissolved and make the chitosan-acetic acid solution that content is 3%, then with after NaOH alkalization 2-3h, add above-mentioned mixture for subsequent use, 2-3h is reacted under 40-60 ° of C, cooling, filters, washs, for subsequent use after drying;
(3) material prepared by step (1) and step (2) is used equivalent dissolution with solvents respectively, makes keratin content in feather within the scope of 8-13%, then be mixed and made into composite spinning stoste, carry out after spinning short cut for subsequent use;
(4) polypropylene and all the other remaining material mixing are added to main feeding trough in double screw extruder, the short collodion silk of cutting step (3) obtained again adds at natural exhaust outlet, blending extrusion temperature section is 195 ° of C, 190 ° of C, 190 ° of C, 185 ° of C, 180 ° of C, 165 ° of C, 110 ° of C, obtain composite master batch, composite master batch is carried out spinning.
Advantage of the present invention is: the present invention utilizes discarded feather to carry out dehydration taste removal deodorizing degreasing, makes the keratin solution of suitable solubility, and utilize nano silicon and Nano Silver modification of chitosan by dissolution with solvents, shitosan is had excellent antibacterial, sterilization, the performance that antibacterial and uvioresistant etc. are excellent, the fabric that the present invention utilizes chitosan solution and keratin solution co-blended spinning to obtain has good hygroscopicity, antibiotic property, the features such as biodegradability, and the ABRASION RESISTANCE enhancing material again by adding polypropylene, tensile strength, the characteristic of the aspects such as weight, decreases the consumption of feather fiber, adds the novelty teabag of feather, the charred FOLIUM ARTEMISIAE ARGYI of interpolation, silk flock and bamboo leaf powder greatly improve the sterilization of down composite fabric, anticorrosion, health care, mildew-resistant, the performance of the aspect such as antibacterial, eider down composite fibre prepared by the present invention is by feather, eider down, the material such as shitosan and polypropylene mixes according to a certain percentage, makes to have complementary advantages between them, and the textile material each side of preparation has excellent performance, meets people to fashion, health care, color, the demand of the aspect such as comfortable, is worthy to be popularized.
Detailed description of the invention
A kind of mildew-resistant eider down compound can weaving face fabric, it is characterized in that, be made up of the raw material of following weight portion (kilogram): poultry feather 60, eider down 16, Silane coupling agent KH550 3, nano silicon 2, Nano Silver 1, shitosan 14, polypropylene 43, silk flock 2, charred FOLIUM ARTEMISIAE ARGYI 3, bamboo leaf powder 1, water are appropriate;
A kind of mildew-resistant eider down compound of the present invention can weaving face fabric, is made up of following concrete steps:
(1) poultry feather and feather stem are separated, use clear water rinsed clean respectively, dry, carry out processed, feather extruding is separated, and feather stem carries out torsion extruding, sterilizing and deodorization under 150 ° of C in high-pressure sterilizing pot is added to eider down mixing after again feather and feather stem being cut into mean size, after spontaneous combustion cooling, mixing feather material is placed in alcohol to soak 6 hours, then is neutral post-drying with clear water washing surface, be ground into powder for subsequent use;
(2) Silane coupling agent KH550 appropriate isopropyl alcohol dissolving is placed in reaction vessel, add nano silicon, Nano Silver again, stirring and refluxing 3h under 80 ° of C, cooling, for subsequent use after suction filtration, washing, drying, again shitosan glacial acetic acid solution is dissolved and make the chitosan-acetic acid solution that content is 3%, then with after NaOH alkalization 3h, add above-mentioned mixture for subsequent use, 2h is reacted under 50 ° of C, cooling, filters, washs, for subsequent use after drying;
(3) material prepared by step (1) and step (2) is used equivalent dissolution with solvents respectively, makes keratin content in feather in 11% scope, then be mixed and made into composite spinning stoste, carry out after spinning short cut for subsequent use;
(4) polypropylene and all the other remaining material mixing are added to main feeding trough in double screw extruder, the short collodion silk of cutting step (3) obtained again adds at natural exhaust outlet, blending extrusion temperature section is 195 ° of C, 190 ° of C, 190 ° of C, 185 ° of C, 180 ° of C, 165 ° of C, 110 ° of C, obtain composite master batch, composite master batch is carried out spinning.
The eider down composite fibre performance indications parameter using the present invention to prepare is as follows:
Hydroscopicity (%): 12.6;
Regain (%): 5.2;
Extensibility (%): 32.4;
Tensile break strength (N): 6.2.

Claims (2)

1. a mildew-resistant eider down compound can weaving face fabric, it is characterized in that, be made up of the raw material of following weight portion: poultry feather 40-60, eider down 14-17, Silane coupling agent KH550 1-3, nano silicon 1-2, Nano Silver 1-2, shitosan 14-20, polypropylene 30-50, silk flock 1-3, charred FOLIUM ARTEMISIAE ARGYI 2-3, bamboo leaf powder 1-2, water are appropriate.
2. a kind of mildew-resistant eider down compound can weaving face fabric according to claim 1, it is characterized in that, is made up of following concrete steps:
(1) poultry feather and feather stem are separated, use clear water rinsed clean respectively, dry, carry out processed, feather extruding is separated, and feather stem carries out torsion extruding, sterilizing and deodorization under 100-200 ° of C in high-pressure sterilizing pot is added to eider down mixing after again feather and feather stem being cut into mean size, after spontaneous combustion cooling, mixing feather material is placed in alcohol and soaks 4-6 hour, then be neutral post-drying with clear water washing surface, be ground into powder for subsequent use;
(2) Silane coupling agent KH550 appropriate isopropyl alcohol dissolving is placed in reaction vessel, add nano silicon, Nano Silver again, stirring and refluxing 1-3h under 70-90 ° of C, cooling, for subsequent use after suction filtration, washing, drying, again shitosan glacial acetic acid solution is dissolved and make the chitosan-acetic acid solution that content is 3%, then with after NaOH alkalization 2-3h, add above-mentioned mixture for subsequent use, 2-3h is reacted under 40-60 ° of C, cooling, filters, washs, for subsequent use after drying;
(3) material prepared by step (1) and step (2) is used equivalent dissolution with solvents respectively, makes keratin content in feather within the scope of 8-13%, then be mixed and made into composite spinning stoste, carry out after spinning short cut for subsequent use;
(4) polypropylene and all the other remaining material mixing are added to main feeding trough in double screw extruder, the short collodion silk of cutting step (3) obtained again adds at natural exhaust outlet, blending extrusion temperature section is 195 ° of C, 190 ° of C, 190 ° of C, 185 ° of C, 180 ° of C, 165 ° of C, 110 ° of C, obtain composite master batch, composite master batch is carried out spinning.
CN201510459773.0A 2015-07-31 2015-07-31 Mildew-proof spinnable down feather composite fabric Pending CN105088395A (en)