CN1046747A - A kind of brightening protective agent and manufacture method - Google Patents
A kind of brightening protective agent and manufacture method Download PDFInfo
- Publication number
- CN1046747A CN1046747A CN 89102550 CN89102550A CN1046747A CN 1046747 A CN1046747 A CN 1046747A CN 89102550 CN89102550 CN 89102550 CN 89102550 A CN89102550 A CN 89102550A CN 1046747 A CN1046747 A CN 1046747A
- Authority
- CN
- China
- Prior art keywords
- grams
- product
- lubricating oil
- dish detergent
- talcum powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
A kind of brightening protective agent and manufacture method are made up of light lubricating oil, paraffin, white vaseline, dish detergent, talcum powder, plant pollen and are dewatered with sorbent material.The manufacture method of this product, technology, simple to operate, easy, raw material sources are extensive, require low to processing condition.Nontoxic, the no burn into of this product is pollution-free, free from extraneous odour, light enhancing effect significantly can be used for each vehicle spray painting layer, and the plated item of various household product, the coat of painting of wood-based product, plastics skin, and efficient provide protection is arranged.
Description
The like product such as the glazing that use on market at present are cured, and purpose is to use on various vehicles, makes it shinny.It is made up of compositions such as Vaseline, paraffin waxes.The weak point of this product is, in use will through wipe repeatedly could rise light and soluble in water, water and promptly fall, the time limit of use lacks, the longest maintenance 2~3 days, the product cost height has peculiar smell.
The objective of the invention is to avoid weak point of the prior art and a kind of new brightening protective agent and manufacture method are provided.
Purpose of the present invention can reach by following measure:
Proportioning of the present invention is: (with the gram number that is contained in per 500 grams)
Light lubricating oil 145~155 grams
Paraffin wax 110~125 grams
White vaseline 55~65 grams
Talcum powder 40~60 grams
Dish detergent 100~110 grams
Plant pollen 15~30 grams
In addition, per 500 the gram products in the process of making, need add 10~20 the gram sorbent materials dewater.
Its production method is as follows:
The first step:
Talcum powder 40~60 grams, white vaseline 55~65 grams, light lubricating oil 145~155 are restrained to add together and stir, the back adding dish detergent 100~110 of waiting to stir restrains, carry out secondary stirring then, (dish detergent plays katalysis), stir postprecipitation about 2 hours, add sorbent material 10~20 grams and dewater.
Second step:
After paraffin wax 110~125 gram is heated to cured dissolving, add plant pollen 15~30 grams.
The 3rd step:
The first step is heated to the boiling back mixed with second step.
Form following arrangement this moment: talcum powder is in the bottom, the lubricating oil supernatant liquid thereon, white vaseline is paraffin wax and pollen topmost in the top of lubricating oil emulsion.Form that this kind arrangement is required for the present invention just to be wanted.Because talcum powder and lubricating oil under the katalysis of washing composition, have formed a kind of emulsion, talcum powder directly contacts object surfaces, at body surface energy absorb oil, makes it to form a kind of protective membrane; White vaseline forms barrier film in the middle layer of lubricating oil emulsion and paraffin wax; Therefore the proportion weight of paraffin wax adds plant pollen (what add in the present embodiment is jasmine pollen) and makes them form protective membrane in the superiors.This kind arrangement formation back (with sight as can be seen) is cooled off and is stirred, and after stirring stops, promptly forming this product.In addition, this product is aborning because the ratio difference can produce different effects, and is many as paraffin wax, makes the product hardening, and lubricating oil makes product too soft, or the like.The dish detergent that uses in this product is the family expenses goldfish liquid detergent of selling on the market, also can use other dish detergent.What sorbent material was used is the non-blushing thinner that sell in market.
The best proportioning of this product is: (500 grams are as the criterion)
Light lubricating oil 150 grams
Paraffin wax 120 grams
White vaseline 60 grams
Talcum powder 50 grams
Dish detergent 100 grams
Plant pollen 20 grams
Sorbent material 20 grams
This product contrast prior art has following advantage:
1. this end-use extensively can have efficient protection enhanced shine for plated item, the coat of painting of wood-based product, the plastics profile of each vehicle spray painting layer and various household product.
2. pollution-free, the free from extraneous odour, easy to operate of nontoxic, the no burn into of this product.
3. this product light enhancing effect is remarkable, and than the cured light enhancing effect 50% that improves of glazing, the phase of adding lustre to can reach more than 10 days.
4. this product is not subjected to weather, climatic influences, is suitable for all temps and humidity, and is constant subzero 10 ℃~40 ℃ of effects above freezing.
This product can preserve more than 2 years never degenerate, nonflammable.
6. the raw material that uses of this product extensively, operation and processing method be simple, and general family just can do.And it is of many uses.
Claims (2)
1, a kind of brightening protective agent is made up of compositions such as lubricating oil, paraffin wax, Vaseline, and it is characterized in that: this product contains the composition of dish detergent, talcum powder, plant pollen, and dewaters with sorbent material.The proportioning components of this product is (being as the criterion with 500 gram weight):
Light lubricating oil 145~155 grams
Paraffin wax 110~125 grams
White vaseline 55~65 grams
Dish detergent 100~110 grams
Talcum powder 40~60 grams
Plant pollen 15~30 grams
2, a kind of brightening protective agent and manufacture method is characterized in that: the production method of this product is as follows:
The first step
Talcum powder 40~60 grams, white vaseline 55~65 grams, light lubricating oil 145~155 grams are mixed, and stir, the back of waiting to stir adds dish detergent 100~110 grams, carries out secondary stirring then.(dish detergent plays katalysis).Stir postprecipitation about 2 hours, add sorbent material 10~20 grams and dewater;
Second step
After paraffin wax 110~125 gram is heated to cured dissolving, add pollen 15~30 grams;
The 3rd step
The first step is heated to the boiling back mixes, in naturally cooling, stir, after stirring stops, promptly forming this product with second step.