CN102864369A - Anti-fatigue cast iron alloy - Google Patents

Anti-fatigue cast iron alloy Download PDF

Info

Publication number
CN102864369A
CN102864369A CN2012103273586A CN201210327358A CN102864369A CN 102864369 A CN102864369 A CN 102864369A CN 2012103273586 A CN2012103273586 A CN 2012103273586A CN 201210327358 A CN201210327358 A CN 201210327358A CN 102864369 A CN102864369 A CN 102864369A
Authority
CN
China
Prior art keywords
cast iron
iron alloy
chromium
fatigue
titanium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012103273586A
Other languages
Chinese (zh)
Inventor
陈敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012103273586A priority Critical patent/CN102864369A/en
Publication of CN102864369A publication Critical patent/CN102864369A/en
Pending legal-status Critical Current

Abstract

The invention relates to an anti-fatigue cast iron alloy. The anti-fatigue cast iron alloy comprises the following components by weight percent: 3.35-3.38% of carbon, 1.8-2.0% of silicon, 0.45-0.57% of manganese, 0.05-0.1% of chromium, 0.2-0.3% of molybdenum, 0.05-0.2 of vanadium, 0.5-0.8% of copper, 0.001-0.1% of niobium, 0.03-0.05% of titanium, 0.005-0.012% of nitrogen, less than 0.15% of phosphorus and sulfur, less than 0.01% of aluminum and the balance being ferrum and inevitable impurities.

Description

A kind of antifatigue cast iron alloy
Technical field
The present invention relates to the cast iron alloy field, refer to specifically a kind of grey cast iron alloy with highly anti-fatigue intensity.
Background technology
Grey cast iron is because cost is relatively low, functional, so the wide range of using.But the compositing range of existing known grey cast iron is quite wide, yet as replenishing of existing performance, what need raising is fatigue strength, and the purposes of the existing grey cast iron of expansion.
Summary of the invention
The purpose of this invention is to provide a kind of grey cast iron, it has good processing characteristics and internal structure is arranged, and this cast iron alloy is compared the fatigue resistance with advantage with existing standard.
The present invention is achieved by the following technical solutions:
A kind of antifatigue cast iron alloy, its composition of percentage composition comprises by weight: the carbon of 3.35-3.38%, the silicon of 1.8-2.0%, the manganese of 0.45-0.57%, the chromium of 0.05-0.1%, the molybdenum of 0.2-0.3%, the vanadium of 0.05-0.2%, the copper of 0.5-0.8%, 0.001-0.1% niobium, the titanium of 0.03-0.05%, the nitrogen of 0.005-0.012%, p and s less than 0.15%, the aluminium less than 0.01%, surplus is iron and inevitable impurity.
Described alloy is when refining, and chromium, titanium, v element will add at first, and then adds iron and carbon, is other element more afterwards.
Described chromium, titanium, v element are to add with ferrochrome, ferrotianium, ferrovanadium mode.
The invention has the beneficial effects as follows,
By technical scheme of the present invention, have good processing characteristics and internal structure when realizing the fatigue resistance of this cast iron alloy.
Embodiment
Below describe technical scheme of the present invention in detail by embodiment.
In the following description, all per-cents of each element in the concrete grey cast iron alloy are weight percentage.
Alloy body in technical scheme of the present invention mainly is to form the grey cast iron with pearlitic texture, its carbon content is 3.35-3.38%, certain carbon content outside this scope also can realize the grey pearlitic texture, but when carbon content during in the scope of the technical program, pearlitic density is very low, the fracture of cast iron is white in color, when carbon content is higher than the scope of the technical program, pearlitic content can increase, but it is inhomogeneous that pearlitic texture can become, although can be by increasing other element such as chromium, copper, niobium, titanium, molybdenum etc., but the amount that needs adding is greater than the amount of the technical program, although can realize pearlitic even structure, can change the performance of cast iron and increase production cost.
The chromium that adds 0.05-0.1%, its effect is to form the stability structure with perlite/carbide, can realize the refined pearl-like body structure, although can be by adding better refined pearl-like body structure of more chromium, the chromium of 0.05-0.1% cooperates the formation optimum structure with other element.
The molybdenum that adds 0.2-0.3%, the vanadium of 0.05-0.2%, the titanium of 0.03-0.05%, the niobium of 0.001-0.1%, it has the nuclear core of refined pearl-like body structure and flake graphite structure, and molybdenum also has the effect of high temperatures pearlitic texture simultaneously.
The content of aluminium is lower than 0.01%, adds the manganese of 0.45-0.57% as the stablizer of pearlitic texture; The copper of 0.5-0.8% promotes perlite to form and stable and control pearlitic texture; The content of nitrogen is 0.005-0.012%, has the flake graphite of compression and promotes perlite to form; P and s in the alloy body is less than 0.15%, and surplus is iron and inevitable impurity.
When refining, chromium, titanium, v element will add at first with ferrochrome, ferrotianium, ferrovanadium mode, and then add iron and carbon, are other element more afterwards.

Claims (3)

1. antifatigue cast iron alloy, it is characterized in that: its composition of percentage composition comprises by weight: the carbon of 3.35-3.38%, the silicon of 1.8-2.0%, the manganese of 0.45-0.57%, the chromium of 0.05-0.1%, the molybdenum of 0.2-0.3%, the vanadium of 0.05-0.%, the copper of 0.5-0.8%, 0.001-0.1% niobium, the titanium of 0.03-0.05%, the nitrogen of 0.005-0.012%, p and s less than 0.15%, the aluminium less than 0.01%, surplus is iron and inevitable impurity.
2. a kind of antifatigue cast iron alloy according to claim 1 is characterized in that: described alloy is when refining, and chromium, titanium, v element will add at first, and then adds iron and carbon, is other element more afterwards.
3. a kind of antifatigue cast iron alloy according to claim 2, it is characterized in that: described chromium, titanium, v element are to add with ferrochrome, ferrotianium, ferrovanadium mode.
CN2012103273586A 2012-09-05 2012-09-05 Anti-fatigue cast iron alloy Pending CN102864369A (en)