CN102616023A - 一种水洗标碳带及其制备方法 - Google Patents
一种水洗标碳带及其制备方法 Download PDFInfo
- Publication number
- CN102616023A CN102616023A CN2012100856802A CN201210085680A CN102616023A CN 102616023 A CN102616023 A CN 102616023A CN 2012100856802 A CN2012100856802 A CN 2012100856802A CN 201210085680 A CN201210085680 A CN 201210085680A CN 102616023 A CN102616023 A CN 102616023A
- Authority
- CN
- China
- Prior art keywords
- solvent
- carbon ribbon
- coating
- resin
- acrylic resin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种水洗标碳带,包括支持体,该支持体一面涂布背涂层,另一面自内向外依次涂布辅助涂层、油墨层,其中,所述油墨层由丙烯酸树脂、颜料、助剂和溶剂组成,所述丙烯酸树脂由下述重量百分比原料共聚制得:甲基丙烯酸甲酯0―3%、丙烯酸丁酯14―20%、丙烯酸羟乙酯1%、丙烯酰胺0―1%和溶剂75―85%。该标碳带打印能级较低,介质适应性强,在聚酯标签、尼龙及缎带上有很好的打印清晰度,且打印标签的耐水洗、耐干洗及耐热性能良好,优于目前市场上销售的同类产品。
Description
技术领域
本发明涉及一种水洗标碳带,其具有耐水洗、干洗、耐热等特点,特别适用于服装、鞋帽、皮具等行业水洗标识标签的打印。
背景技术
热转印碳带(Thermal Transfer Ribbon,TTR)自70年代发明至今的几十年中,随着打印机技术和打印介质的发展,已从开始的简单多用途发展到多种类和极强的针对性,以适应打印机技术越来越快、打印分辨率越来越高、打印介质新材料不断出现、应用场合越来越复杂苛刻的发展趋势。
TTR主要由以下几部分构成:a)薄而强的涤纶或其他高密度材料带基;b)带基正面的底涂层以保证墨色均匀及打印时墨色的完整转移;c)蜡或树脂基的墨色层;d)带基的背涂层起防静电、均热及减少磨擦的作用,可以保护打印头,延长其使用寿命。
TTR可简单的分为下述三类产品。
蜡基(Wax)碳带:通常含有高百分比的蜡基原料(蜡含量大于65%)。由于蜡的熔点远低于树脂,用蜡基碳带打印需要的能级远低于使用混合基和树脂基打印;又由于多数蜡比树脂软,蜡基碳带打印图形的耐久性不如混合基和树脂基。蜡基碳带通常具有高密度、高敏度的特点,应用于纸质标签,打印效果优良,成本经济。
蜡/树脂混合基(Wax/Resin)碳带:一般含有高百分比的树脂成分原料(树脂含量在30一50%之间),这就使得该类色带的熔点较高。与蜡基色带相比,用此种碳带打印所需要的能级更高。由于多数的树脂比蜡硬,打印出的图形的防刮性和防化学腐蚀性也比蜡基碳带好。混合基色带兼具优质打印效果与耐久性能,应用广泛,价效皆佳。
树脂基(Resin)碳带:含有最高比例的树脂成分,在打印时需要的能级也比蜡基和混合基高,由于多数的树脂比蜡硬,这种碳带的耐久性,耐磨擦、耐热、耐腐蚀等性能最佳。有些配方能防蒸汽压力,有些则能经水洗或干洗等,但打印成本与前二类相比最高,介质适应性也最差。
发明内容
本发明目的在于提供一种水洗标碳带,该标碳带具有耐水洗、干洗、耐热等特点,特别适用于服装、鞋帽、皮具等行业水洗标识标签的打印。
本发明还提供了所述水洗标碳带的制备方法。
为实现上述目的,本发明采用如下技术方案:
一种水洗标碳带,包括支持体,该支持体一面涂布背涂层,另一面自内向外依次涂布辅助涂层、油墨层,其中,所述油墨层由丙烯酸树脂、颜料、助剂和溶剂组成,所述丙烯酸树脂由下述重量百分比原料共聚制得:甲基丙烯酸甲酯0―3%、丙烯酸丁酯14―20%、丙烯酸羟乙酯1%、丙烯酰胺0―1%和溶剂75―85%。
所述油墨层的各组分重量百分比如下:丙烯酸树脂12―20%、颜料2―5%、助剂1―5%和溶剂70―85%。
所述背涂层以重量百分比计,由5―10%改性硅树脂和90―95%溶剂组成。
所述辅助涂层的各组分重量百分比如下:PU树脂3―10%、EVA树脂2―5%、棕榈蜡10―15%和溶剂70―85%。其中,所选用的PU树脂粘度以在2000-6000cps之间为宜,选用的EVA树脂软化点以在20―30℃之间为宜。
所述溶剂优选为甲苯、丁酮或两者的混合液,其中两者混合时以甲苯与丁酮体积比1:1时效果最佳。所述支持体优选采用厚度为4.0―6.0μm 的PET薄膜。颜料选用碳黑,助剂选用硬化剂即可。
所述水洗标碳带的制备方法,包括以下步骤:
①在支持体的一面涂布背涂层,涂层厚度≤0.1μm,于100±5℃烘干,进入下一工序;
②在支持体的另一面涂布辅助涂层,涂层厚度0.5-1.0μm,于100±5℃烘干,进入下一工序;
③将甲基丙烯酸甲酯、丙烯酸丁酯、丙烯酸羟乙酯、丙烯酰胺和溶剂按比例混匀后回流6-8h,冷却至室温得丙烯酸树脂(所得丙烯酸树脂的比浓对数粘度为0.03-0.2dL/g);然后按比例加入溶剂、颜料和助剂混匀、研磨后,涂布于辅助涂层的表面,涂层厚度1.0-1.5μm,于100±5℃烘干形成油墨层,即得厚度在6.0―8.0μm的水洗标碳带。
本发明通过在油墨层中使用由甲基丙烯酸甲酯、丙烯酸丁酯、丙烯酸羟乙酯和丙烯酰胺共聚而得的丙烯酸树脂,使最后制得的标碳带具有耐水洗、干洗、耐热等优点。该种水洗标碳带在类别上属于树脂基碳带,可在尼龙、缎带等介质上打印,且耐水洗、干洗,可广泛用于服装、鞋帽、皮具等行业水洗标识标签的打印。此外,本发明克服了以往树脂基产品介质适应性差的缺点,且所用原料制备方法简单、环保、成本低廉。
具体实施方式
以下通过优选实施例对本发明作进一步详细说明,但本发明的保护范围并不局限于此。下述实施例如无特殊说明,所用溶剂均为由甲苯与丁酮体积1:1组成的混合液;选用的PU树脂粘度在2000-6000cps之间,选用的EVA树脂软化点在20―30℃之间。
实施例1
一种水洗标碳带,包括支持体,所述支持体为厚度4.5μm的PET薄膜,该支持体一面涂布耐热的背涂层,另一面自内向外依次涂布辅助涂层、油墨层,其中,所述耐热的背涂层由6g改性硅树脂和94g溶剂组成,所用改性硅树脂购自韩国科林株式会社生产的KR-605改性硅树脂。
所述辅助涂层由5g PU树脂、4g EVA树脂、13g棕榈蜡和78g溶剂组成。所用PU树脂选自韩国KORIM公司,EVA树脂选自Du Pont-Mitsui公司,棕榈蜡选自Foncepi公司。
所述油墨层由14g丙烯酸树脂、3g颜料、1g助剂和82g溶剂组成。所用颜料选用Degussa公司生产的碳黑,所用助剂为日本Mitsui公司生产的D-110硬化剂。所述丙烯酸树脂由2g甲基丙烯酸甲酯、16.5g丙烯酸丁酯、1g丙烯酸羟乙酯、0.5g丙烯酰胺和80g溶剂共聚制得。
所述水洗标碳带的制备方法,包括以下步骤:
①将改性硅树脂和溶剂按比例混匀后,直接在支持体PET薄膜的一面常温涂布,涂层厚度0.1μm,于105℃烘干形成背涂层,进入下一工序;
②用溶剂将PU树脂和EVA树脂溶解,然后加入棕榈蜡混匀、砂磨后直接在PET薄膜的另一面常温涂布,涂层厚度0.5μm,于105℃烘干形成辅助涂层,进入下一工序;
③将甲基丙烯酸甲酯、丙烯酸丁酯、丙烯酸羟乙酯、丙烯酰胺和溶剂按比例混匀后回流7h,冷却至室温得丙烯酸树脂;然后按比例加入溶剂、颜料和助剂混匀、砂磨(用以使体系分散均匀)后,用涂布机涂于辅助涂层的表面,涂层厚度1.4μm,于105℃烘干形成油墨层,即得厚度在6.5μm的水洗标碳带,热转印温度122℃。
实施例2
将丙烯酸树脂的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚6.7μm,热转印温度122℃。
实施例3
将丙烯酸树脂的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚6.7μm,热转印温度122℃。
实施例4
将油墨层的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚7.0μm,热转印温度124℃。
实施例5
将辅助涂层的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚6.5μm,热转印温度122℃。
实施例6
将油墨层的各组分比例更改如下:
同时,丙烯酸树脂的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚6.8μm,热转印温度124℃。
实施例7
将油墨层的各组分比例更改如下:
同时,丙烯酸树脂的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚6.8μm,热转印温度124℃。
实施例8
将油墨层比例更改如下:
同时,合成树脂比例改如下,其它条件同实施例1,所制得的水洗标碳带厚6.5μm,热转印温度122℃。
实施例9
将丙烯酸树脂的各组分比例更改如下,其它条件同实施例1,所制得的水洗标碳带厚7.0μm,热转印温度124℃。
本发明所涉及的水洗标碳带,打印能级较低,介质适应性强,在聚酯标签、尼龙及缎带上有很好的打印清晰度,且打印标签的耐水洗、耐干洗及耐热(测试方法参见国标GB/T 3921-2008、GB/T 8629-2001)性能良好,优于目前市场上销售的同类产品。该水洗标碳带的基本性能见下表:
Claims (6)
1.一种水洗标碳带,包括支持体,该支持体一面涂布背涂层,另一面自内向外依次涂布辅助涂层、油墨层,其特征在于,所述油墨层由丙烯酸树脂、颜料、助剂和溶剂组成,所述丙烯酸树脂由下述重量百分比原料共聚制得:甲基丙烯酸甲酯0―3%、丙烯酸丁酯14―20%、丙烯酸羟乙酯1%、丙烯酰胺0―1%和溶剂75―85%。
2.如权利要求1所述的水洗标碳带,其特征在于,所述油墨层的各组分重量百分比如下:丙烯酸树脂12―20%、颜料2―5%、助剂1―5%和溶剂70―85%。
3.如权利要求1所述的水洗标碳带,其特征在于,以重量百分比计,所述背涂层由5―10%改性硅树脂和90―95%溶剂组成。
4.如权利要求1所述的水洗标碳带,其特征在于,所述辅助涂层的各组分重量百分比如下:PU树脂3―10%、EVA树脂2―5%、棕榈蜡10―15%和溶剂70―85%。
5.如权利要求1至4任一所述的水洗标碳带,其特征在于,所述溶剂为甲苯和/或丁酮;所述支持体为厚度4.0―6.0μm 的PET薄膜。
6.权利要求1至4任一所述水洗标碳带的制备方法,其特征在于,包括以下步骤:
①在支持体的一面涂布背涂层,烘干,进入下一工序;
②在支持体的另一面涂布辅助涂层,烘干,进入下一工序;
③将甲基丙烯酸甲酯、丙烯酸丁酯、丙烯酸羟乙酯、丙烯酰胺和溶剂按比例混匀后回流6-8h,冷却至室温得丙烯酸树脂;然后按比例加入溶剂、颜料和助剂混匀、研磨后,涂布于辅助涂层的表面,烘干形成油墨层,即得厚度在6.0―8.0μm的水洗标碳带。