CN102039768A - Process for making tree sparks with molten iron - Google Patents
Process for making tree sparks with molten iron Download PDFInfo
- Publication number
- CN102039768A CN102039768A CN2010105073250A CN201010507325A CN102039768A CN 102039768 A CN102039768 A CN 102039768A CN 2010105073250 A CN2010105073250 A CN 2010105073250A CN 201010507325 A CN201010507325 A CN 201010507325A CN 102039768 A CN102039768 A CN 102039768A
- Authority
- CN
- China
- Prior art keywords
- molten iron
- iron
- coke
- sparks
- tree
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention provides a process for making tree sparks with molten iron, which comprises: placing 600 kilograms of coke in a furnace and igniting the coke to heat the furnace for 5 to 8 hours; after the furnace is heated, adding cock and iron blocks by a coke and iron layer alternating process method to smelt iron to obtain molten iron, and getting molten iron with a willow scoop immersed in water for 10 days; pouring molten iron in the willow scoop onto a wall to make crown-link sparks. When the process for making tree sparks with molten iron is used, tree sparks can be generated by pouring molten iron onto a wall, and a high entertaining effect is achieved.
Description
Technical field
The present invention relates to the metal smelt technical field, particularly a kind of technology of beating the tree flower with molten iron.
Background technology
Molten iron is used for making various ironwares, and purposes is limited, is not used in and views and admires.
Summary of the invention
The invention provides a kind of technology of beating the tree flower with molten iron of can generation tree crown spark.
To achieve these goals, the invention provides following technical scheme:
A kind of technology of beating the tree flower with molten iron is characterized in that, comprising:
Earlier 600 jin of coke being put into stove lights and carries out hot stove, hot stove 5-8 hour;
Hot stove finishes and adds coke and iron block according to the step that adds one deck iron block on one deck coke and smelt iron and obtain molten iron, and the willow spoon that was soaked in water 10 days has been ladled out described molten iron;
Molten iron in the described willow spoon is sprinkled to the crown spark of wall generation tree.
Further among the embodiment, also in described hot stove, add copper billet or aluminium block, obtain copper water or aluminium water, to reach the appreciation effect of different color metal sparks.
By implementing above technical scheme, have following technique effect: the technology of beating tree flower with molten iron that the utility model provides is by splashing molten iron on wall, can the crown spark of generation tree, have very big sight.
The specific embodiment
Technical scheme is for a better understanding of the present invention described embodiment provided by the invention in detail below in conjunction with accompanying drawing.
The embodiment of the invention provides a kind of technology of beating the tree flower with molten iron, comprises step:
A, earlier 600 jin of coke are put into stove and lighted and carry out hot stove, hot stove 5-8 hour;
B, hot stove finish and add coke and iron block according to the step that adds one deck iron block on one deck coke and smelt iron and obtain molten iron;
C, the willow spoon that was soaked in water 10 days have been ladled out described molten iron;
D, the molten iron in the described willow spoon is bold and vigorous to the crown spark of wall generation tree.
Further among the embodiment, in the above-mentioned steps, also in described hot stove, add copper billet or aluminium block, obtain copper water or aluminium water, to reach the appreciation effect of different color metal sparks.
Describe the Application Example of an above-mentioned technology below in detail:
Above-mentioned technology is widely used in warm spring town, and beating tree flower needs in advance a few hours to prepare, and essential apparatus has handle surplus iron-smelting furnace, hair-dryer, hand-held type and the double willow spoon ten of lifting the fire-resistant pot of formula, soaking, the some buckets of cold water.Willow must be obtained from the big willow that grows on the water's edge, and is long throughout the year in the waterside because of it, have very high fire resistance, and the willow spoon must shift to an earlier date immersion in 10 days.Iron-smelting furnace is to be made with special material: the inside one deck is the refractory material of high temperature of tolerance more than 1600 degree, by waste mud and greatly a urn watt slag be mixed and made into refractory material other refractory materials such as (also) available refractory cements, outside one deck wraps up with iron sheet.The eye (also can be many stoves) of one circle is arranged on the iron-smelting furnace, be commonly called as one-eyed stove, molten iron is exactly to flow out from here.Fire-resistant pot also is to grope for many years to make by artists: one deck of its inside is to make (also available other refractory materials) by waste mud and coke blacking, and one deck iron sheet is also wrapped in the outside.For iron and carbon are separated cleverly, according to the technology of one deck carbon one deck iron with reference to carbon: the ratio of iron=1: 3.75 is separated it.Also aluminium and carbon can be heated into aluminium water according to above-mentioned method, perhaps copper and carbon be heated into copper water according to above-mentioned method, wherein: " flower " of molten iron is red, and " flower " of copper water is green, and " flower " of aluminium water is white.Intersecting and beating, giving the different visual impression of people.
Carry out hot stove then: earlier 600 jin of coke are put into stove and lighted and carry out hot stove, need about 8 hours of hot stove in the time of summer, need hot stove 5 in the time of winter---6 hours.Hot stove finishes and smelts iron, and whenever adds 40 jin of coke and can smelt iron 150 jin in water.Come out of the stove and generally need 50 minutes from the blow-on molten iron of lighting a fire.After molten iron was burned, the molten iron that two stout mans will have been melted was poured in fire-resistant pot, and it is preceding to lift to wall (Ru Baomen) rapidly, was responsible for spilling the three fully armed in advance to four-player of molten iron, wore straw hat, wore old sheepskin jacket (hair side outwardly), and pin is wrapped up in and hidden the fiery door curtain made of cloth.The people who is responsible for spilling molten iron takes turns to take out a wet willow spoon in bucket, having ladled out the exert oneself fort bar top of Chao Gaogao of one spoonful of molten iron rapidly sprinkles and goes, one spoonful connects one spoonful molten iron and runs into and burst sputter immediately behind the brick wall of hard ice-cold fort bar and come, form the spark of tree crown shape, in different poses and with different expressions, ten thousand flower Pentiums.Whenever, need water is dried before spoon is used clean, and whenever can splash 30 to the willow spoon---40 times.Spilling of each spoonful molten iron just as the fireworks display in red-letter day of dishing out by hand together, blown in the air, forms the shock scene of " fiery trees and silver flowers all night with lights turned on ".
The spark that splashes forms one by one the semi-circular pattern around the top, hole of fort door, with sky, the earth shine as daytime general, and splash and peculiarly shaped, grand especially.
More than a kind of technology of beating the tree flower with molten iron was described in detail to the embodiment of the invention provides, for one of ordinary skill in the art, thought according to the embodiment of the invention, part in specific embodiments and applications all can change, in sum, this description should not be construed as limitation of the present invention.
Claims (2)
1. a technology of beating the tree flower with molten iron is characterized in that, comprising:
Earlier 600 jin of coke being put into stove lights and carries out hot stove, hot stove 5-8 hour;
Hot stove finishes and adds coke and iron block according to the step that adds one deck iron block on one deck coke and smelt iron and obtain molten iron, and the willow spoon that was soaked in water 10 days has been ladled out described molten iron;
Molten iron in the described willow spoon is sprinkled to the crown spark of wall generation tree.
2. beat the technology of tree flower according to claim 1 with molten iron, it is characterized in that, also in described hot stove, add copper billet or aluminium block, obtain copper water or aluminium water, to reach the appreciation effect of different color metal sparks.