CN101670511A - 旧铸轧辊轴承座的修复方法 - Google Patents
旧铸轧辊轴承座的修复方法 Download PDFInfo
- Publication number
- CN101670511A CN101670511A CN200910196164A CN200910196164A CN101670511A CN 101670511 A CN101670511 A CN 101670511A CN 200910196164 A CN200910196164 A CN 200910196164A CN 200910196164 A CN200910196164 A CN 200910196164A CN 101670511 A CN101670511 A CN 101670511A
- Authority
- CN
- China
- Prior art keywords
- bringing
- section
- bearing
- axis hole
- cast roll
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种旧铸轧辊轴承座的修复方法。属轴承座修复技术。它是用气割火焰分别对轴承内孔的上方和下方加热内弧,使其温度达到500-600℃,然后用水急剧冷却加热区,使内孔上方向外凸起,短轴线变长;再在轴承座左右侧分别加热轴承座外方加热段,加热至500-600℃时,用水急剧冷却加热区,使内孔左右方向向内凸起使长轴线变短。本发明的有益效果是:该方法操作简单,能使旧轴承座恢复至基本尺寸,可以正常使用。
Description
技术领域
本发明涉及一种铸轧辊轴承座,具体是一种旧铸轧辊轴承座的修复方法。
背景技术
铸轧辊轴承座由于长期处于高温高压状态下运行,上下受力过重,容易产生疲劳变形,使轴孔变为如图1所示横放的椭圆形。即形成上下方向有些压偏,孔径上下尺寸变小,左右尺寸变大,久而久之不圆度误差越来越大,致使铸轧辊轴承座无法正常使用。
发明内容
为解决上述问题,本发明提供一种旧铸轧辊轴承座的修复方法,使用本方法修复变形的旧铸轧辊轴承座,能使其基本恢复原始尺寸,重新投入使用。
本发明是以如下技术方案实现的:一种旧铸轧辊轴承座的修复方法,利用热变形技术使铸轧辊轴承座恢复至正常状态,具体步骤如下:
1)首先用火焰加热轴承座轴孔上方内弧,即上加热段,使其温度达到500--600℃,然后用水急剧冷却加热区域,使内孔上方向外凸起,短轴线变长;上加热段的加热区域为轴孔周长的1/15左右;
2)用火焰加热轴承轴孔下方内弧,即下加热段,使其温度达到500--600℃,然后用水急剧冷却加热区域,使内孔下方向外凸起,短轴线变长;下加热段为轴孔周长的1/15左右;
3)在轴承座左右侧分别加热轴承座外方加热段,加热至500--600℃时,用水急剧冷却加热区,使内孔左右方向向内凸起使长轴线变短;加热段的长度为轴孔周长的1/15左右。
本发明的有益效果是:该方法利用热变形技术修复轴承座,操作方法简单,使用此方法使轴承座恢复了基本尺寸,可以正常使用。
附图说明
图1是变形后的铸轧辊轴承座示意图;
图2是旧铸轧辊轴承座上下加热段示意图;
图3是修复后的铸轧辊轴承座示意图。
图中:1、铸轧辊轴承座,2、轴孔,3、上加热段,4、下加热段,5、左加热段,6、右加热段。
具体实施方式
实施例1
本实施例修复的是轴孔直径为500mm的变形的旧铸轧辊轴承座。
如图2所示,本实施例首先用气割火焰加热轴承轴孔2上方宽约100mm左右段内弧上加热段3,使其温度达到500--600℃,然后用水急剧冷却加热区,使内孔上方向外凸起,短轴线变长;再用气割火焰加热轴承轴孔下方宽约100mm左右段内弧下加热段4,使其温度达到500--600℃,然后用水急剧冷却加热区,使内孔下方向外凸起,短轴线变长。也可以先加热下部,再加热上部。在轴承座1左右侧分别加热轴承座外方宽约100mm左加热段5和右加热段6,加热至500--600℃时,用水急剧冷却加热区,使内孔左右方向向内凸起使长轴线变短。
如图3所示,铸轧辊轴承座恢复至正常形状。
Claims (1)
1、一种旧铸轧辊轴承座的修复方法,其特征是利用热变形技术使铸轧辊轴承座恢复至正常状态,具体步骤如下:
1)首先用火焰加热轴承座轴孔上方内弧,即上加热段,使其温度达到500--600℃,然后用水急剧冷却加热区域,使内孔上方向外凸起,短轴线变长;上加热段的加热区域为轴孔周长的1/15左右;
2)用火焰加热轴承轴孔下方内弧,即下加热段,使其温度达到500--600℃,然后用水急剧冷却加热区域,使内孔下方向外凸起,短轴线变长;下加热段为轴孔周长的1/15左右;
3)在轴承座左右侧分别加热轴承座外方加热段,加热至500--600℃时,用水急剧冷却加热区,使内孔左右方向向内凸起使长轴线变短;加热段的长度为轴孔周长的1/15左右。