Kupke et al., 2012 - Google Patents
Reliability of $\hbox {SrRuO} _ {3}\hbox {/SrTiO} _ {3}\hbox {/SrRuO} _ {3} $ Stacks for DRAM ApplicationsKupke et al., 2012
View PDF- Document ID
- 9068771316442846710
- Author
- Kupke S
- Knebel S
- Schroeder U
- Schmelzer S
- Bottger U
- Mikolajick T
- Publication year
- Publication venue
- IEEE electron device letters
External Links
Snippet
A layer stack of strontium ruthenate/strontium titanate/strontium ruthenate was fabricated by low-rate rf sputtering. A high dielectric permittivity of approximately 200 at a capacitive effective thickness of 0.4 nm in combination with a very low leakage current density JC of 5× …
- 229910002367 SrTiO 0 title description 23
Classifications
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L21/00—Processes or apparatus adapted for the manufacture or treatment of semiconductor or solid state devices or of parts thereof
- H01L21/02—Manufacture or treatment of semiconductor devices or of parts thereof
- H01L21/04—Manufacture or treatment of semiconductor devices or of parts thereof the devices having at least one potential-jump barrier or surface barrier, e.g. PN junction, depletion layer, carrier concentration layer
- H01L21/18—Manufacture or treatment of semiconductor devices or of parts thereof the devices having at least one potential-jump barrier or surface barrier, e.g. PN junction, depletion layer, carrier concentration layer the devices having semiconductor bodies comprising elements of Group IV of the Periodic System or AIIIBV compounds with or without impurities, e.g. doping materials
- H01L21/30—Treatment of semiconductor bodies using processes or apparatus not provided for in groups H01L21/20 - H01L21/26
- H01L21/31—Treatment of semiconductor bodies using processes or apparatus not provided for in groups H01L21/20 - H01L21/26 to form insulating layers thereon, e.g. for masking or by using photolithographic techniques; After treatment of these layers
- H01L21/314—Inorganic layers
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L21/00—Processes or apparatus adapted for the manufacture or treatment of semiconductor or solid state devices or of parts thereof
- H01L21/02—Manufacture or treatment of semiconductor devices or of parts thereof
- H01L21/02104—Forming layers
- H01L21/02107—Forming insulating materials on a substrate
- H01L21/02109—Forming insulating materials on a substrate characterised by the type of layer, e.g. type of material, porous/non-porous, pre-cursors, mixtures or laminates
- H01L21/02112—Forming insulating materials on a substrate characterised by the type of layer, e.g. type of material, porous/non-porous, pre-cursors, mixtures or laminates characterised by the material of the layer
- H01L21/02172—Forming insulating materials on a substrate characterised by the type of layer, e.g. type of material, porous/non-porous, pre-cursors, mixtures or laminates characterised by the material of the layer the material containing at least one metal element, e.g. metal oxides, metal nitrides, metal oxynitrides or metal carbides
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L28/00—Passive two-terminal components without a potential-jump or surface barrier for integrated circuits; Details thereof; Multistep manufacturing processes therefor
- H01L28/40—Capacitors
- H01L28/60—Electrodes
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01G—CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES OR LIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE
- H01G4/00—Fixed capacitors; Processes of their manufacture
- H01G4/002—Details
- H01G4/018—Dielectrics
- H01G4/06—Solid dielectrics
- H01G4/08—Inorganic dielectrics
- H01G4/12—Ceramic dielectrics
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L29/00—Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor
- H01L29/40—Electrodes; Multistep manufacturing processes therefor
- H01L29/43—Electrodes; Multistep manufacturing processes therefor characterised by the materials of which they are formed
- H01L29/49—Metal-insulator-semiconductor electrodes, e.g. gates of MOSFET
- H01L29/51—Insulating materials associated therewith
- H01L29/516—Insulating materials associated therewith with at least one ferroelectric layer
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Kupke et al. | Reliability of $\hbox {SrRuO} _ {3}\hbox {/SrTiO} _ {3}\hbox {/SrRuO} _ {3} $ Stacks for DRAM Applications | |
Mehmood et al. | Bulk depolarization fields as a major contributor to the ferroelectric reliability performance in lanthanum doped Hf0. 5Zr0. 5O2 capacitors | |
Reisinger et al. | A comparative study of dielectric relaxation losses in alternative dielectrics | |
Mittmann et al. | Impact of iridium oxide electrodes on the ferroelectric phase of thin Hf0. 5Zr0. 5O2 films | |
Nguyen | Ultrahigh energy-storage performance in lead-free BZT thin-films by tuning relaxor behavior | |
Liu et al. | Highly stable performance of flexible Hf 0.6 Zr 0.4 O 2 ferroelectric thin films under multi-service conditions | |
JP2002519864A (en) | DC sputtering process for fabricating thin film ferroelectric capacitors with smooth electrodes and improved memory retention | |
KR20010109297A (en) | Scalable lead zirconium titanate(pzt) thin film material and deposition method, and ferroelectric memory device structures comprising such thin film material | |
JP5401199B2 (en) | Dielectric thin film composition exhibiting linear dielectric properties | |
Baniecki et al. | H 2 O vapor-induced leakage degradation of Pb (Zr, Ti) O 3 thin-film capacitors with Pt and IrO 2 electrodes | |
Zhang et al. | Effects of Hf buffer layer at the Y-doped HfO2/Si interface on ferroelectric characteristics of Y-doped HfO2 films formed by reactive sputtering | |
Chen et al. | Barrier heights, polarization switching, and electrical fatigue in Pb (Zr, Ti) O3 ceramics with different electrodes | |
Mizutani et al. | Cerium oxide capping on Y-doped HfO2 films for ferroelectric phase stabilization with endurance improvement | |
Han et al. | An empirical investigation on the effect of oxygen vacancy in ZrO 2 thin film on the frequency-dependent capacitance degradation in the metal–insulator–metal capacitor | |
Oh et al. | Accurate Evaluation of High-k HZO/ZrO 2 Films by Morphotropic Phase Boundary | |
Ding et al. | Atomic-layer-deposited Al2O3-HfO2 laminated and sandwiched dielectrics for metal–insulator–metal capacitors | |
James et al. | Tunability, ferroelectric and leakage studies on pulsed laser ablated (Pb0. 92La0. 08)(Zr0. 60Ti0. 40) O3 thin films | |
JP2002353422A (en) | MFMOS capacitor having high dielectric constant material and method of manufacturing the same | |
Bhanu et al. | Influence of Mg ion concentration in ZrO2 gate dielectric layered silicon based MOS capacitors for memory applications: Thorough understanding of conduction processes | |
Zhu et al. | Atomic Layer Deposited High‐κ Films and Their Role in Metal‐Insulator‐Metal Capacitors for Si RF/Analog Integrated Circuit Applications | |
US20130244447A1 (en) | Oxidation of metallic films | |
Victor et al. | Impact of microstructure on electrical characteristics of laser ablation grown ZrTiO4 thin films on Si substrate | |
Kundu et al. | Thickness‐Dependent Electrical Properties of Pb (Zr, Ti) O 3 Thin Film Capacitors for Memory Device Applications | |
Kang et al. | Reliability characteristics of MIM capacitor studied with ΔC-F characteristics | |
Walters | Scaling and design of thin film ferroelectric hafnium oxide for memory and logic devices |