Li et al., 2005 - Google Patents
Nonuniformities of electrical resistivity in undoped 6H-SiC wafersLi et al., 2005
- Document ID
- 8141452128102315990
- Author
- Li Q
- Polyakov A
- Skowronski M
- Sanchez E
- Loboda M
- Fanton M
- Bogart T
- Gamble R
- Publication year
- Publication venue
- Journal of applied physics
External Links
Snippet
Chemical elemental analysis, temperature-dependent Hall measurements, deep-level transient spectroscopy, and contactless resistivity mapping were performed on undoped semi-insulating (SI) and lightly nitrogen-doped conducting 6H-SiC crystals grown by …
- 235000012431 wafers 0 title abstract description 62
Classifications
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L29/00—Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor
- H01L29/02—Semiconductor bodies; Multistep manufacturing processes therefor
- H01L29/12—Semiconductor bodies; Multistep manufacturing processes therefor characterised by the materials of which they are formed
- H01L29/16—Semiconductor bodies; Multistep manufacturing processes therefor characterised by the materials of which they are formed including, apart from doping materials or other impurities, only elements of Group IV of the Periodic System
- H01L29/1608—Silicon carbide
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01L—SEMICONDUCTOR DEVICES; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01L29/00—Semiconductor devices adapted for rectifying, amplifying, oscillating or switching, or capacitors or resistors with at least one potential-jump barrier or surface barrier, e.g. PN junction depletion layer or carrier concentration layer; Details of semiconductor bodies or of electrodes thereof; Multistep manufacturing processes therefor
- H01L29/02—Semiconductor bodies; Multistep manufacturing processes therefor
- H01L29/12—Semiconductor bodies; Multistep manufacturing processes therefor characterised by the materials of which they are formed
- H01L29/16—Semiconductor bodies; Multistep manufacturing processes therefor characterised by the materials of which they are formed including, apart from doping materials or other impurities, only elements of Group IV of the Periodic System
- H01L29/1602—Diamond
-
- C—CHEMISTRY; METALLURGY
- C30—CRYSTAL GROWTH
- C30B—SINGLE-CRYSTAL-GROWTH; UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL; PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; APPARATUS THEREFOR
- C30B29/00—Single crystals or homogeneous polycrystalline material with defined structure characterised by the material or by their shape
- C30B29/10—Inorganic compounds or compositions
- C30B29/36—Carbides
-
- C—CHEMISTRY; METALLURGY
- C30—CRYSTAL GROWTH
- C30B—SINGLE-CRYSTAL-GROWTH; UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL; PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; APPARATUS THEREFOR
- C30B23/00—Single-crystal growth by condensing evaporated or sublimed material
- C30B23/02—Epitaxial-layer growth
-
- C—CHEMISTRY; METALLURGY
- C30—CRYSTAL GROWTH
- C30B—SINGLE-CRYSTAL-GROWTH; UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL; PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; APPARATUS THEREFOR
- C30B25/00—Single-crystal growth by chemical reaction of reactive gases, e.g. chemical vapour-deposition growth
- C30B25/02—Epitaxial-layer growth
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Kato et al. | n-type doping of (001)-oriented single-crystalline diamond by phosphorus | |
US9337277B2 (en) | High voltage power semiconductor device on SiC | |
Xu et al. | Different origins of the yellow luminescence in as-grown high-resistance GaN and unintentional-doped GaN films | |
Seki et al. | Remarkable p-type activation of heavily doped diamond accomplished by boron ion implantation at room temperature and subsequent annealing at relatively low temperatures of 1150 and 1300° C | |
Eriksson et al. | Toward an ideal Schottky barrier on 3C-SiC | |
Mitchel et al. | Vanadium donor and acceptor levels in semi-insulating 4H-and 6H-SiC | |
Jenny et al. | High-purity semi-insulating 4H-SiC for microwave device applications | |
Negoro et al. | Stability of deep centers in 4H-SiC epitaxial layers during thermal annealing | |
Li et al. | Nonuniformities of electrical resistivity in undoped 6H-SiC wafers | |
Karhu et al. | CVD growth and properties of on-axis vanadium doped semi-insulating 4H-SiC epilayers | |
Sardar et al. | High conductivity β-Ga2O3 formed by hot Si ion implantation | |
Zvanut et al. | Defect levels and types of point defects in high-purity and vanadium-doped semi-insulating 4H–SiC | |
Teraji et al. | High-quality boron-doped homoepitaxial diamond grown by high-power microwave-plasma chemical-vapor deposition | |
Henry et al. | Ga-bound excitons in 3C-, 4H-, and 6H-SiC | |
Lo et al. | Magnetic and structural properties of Gd-implanted zinc-blende GaN | |
Kimoto et al. | Homoepitaxial growth of 4H–SiC (033̄8) and nitrogen doping by chemical vapor deposition | |
Jenny et al. | Effects of annealing on carrier lifetime in 4H-SiC | |
Mitchel et al. | Compensation mechanism in high purity semi-insulating 4H-SiC | |
Litton et al. | Effect of C∕ Si ratio on deep levels in epitaxial 4H–SiC | |
Izzo et al. | Electrical properties of high energy ion irradiated 4H-SiC Schottky diodes | |
Powell et al. | Growth of SiC substrates | |
Colston et al. | Electrical properties of n-type 3C-SiC epilayers in situ doped with extremely high levels of phosphorus | |
Calcagno et al. | Optical and electrical properties of 4H-SiC epitaxial layer grown with HCl addition | |
Huh et al. | Residual impurities and native defects in 6H‐SiC bulk crystals grown by halide chemical-vapor deposition | |
Kojima et al. | Growth of vanadium doped semi-insulating 4H-SiC epilayer with ultrahigh-resistivity |