Crack bridging by inclined fibers has been studied in a brittle fiber–brittle matrix model ceramic composite. Results of the fiber bridging force vs the crack opening displacement have been obtained for different fiber inclination angles using a fracture mechanics …
- 239000000835 fiber 0 title abstract description 128
Classifications
-
- C—CHEMISTRY; METALLURGY
- C04—CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
- C04B—LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
- C04B35/00—Shaped ceramic products characterised by their composition; Ceramics compositions; Processing powders of inorganic compounds preparatory to the manufacturing of ceramic products
- C04B35/71—Ceramic products containing macroscopic reinforcing agents
- C04B35/78—Ceramic products containing macroscopic reinforcing agents containing non-metallic materials
- C04B35/80—Fibres, filaments, whiskers, platelets, or the like
- C04B35/803—The matrix of the ceramic products consisting of oxides only
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N2203/00—Investigating strength properties of solid materials by application of mechanical stress
- G01N2203/0058—Kind of property studied
- G01N2203/006—Crack, flaws, fracture or rupture
- G01N2203/0062—Crack or flaws
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N2203/00—Investigating strength properties of solid materials by application of mechanical stress
- G01N2203/02—Details not specific for a particular testing method
- G01N2203/0202—Control of the test
- G01N2203/0212—Theories, calculations
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Mandell et al. | A microdebonding test for in situ assessment of fibre/matrix bond strength in composite materials | |
Jero et al. | Effect of interfacial roughness on the frictional stress measured using pushout tests | |
Petrovic et al. | Mixed‐Mode Fracture from Controlled Surface Flaws in Hot‐Pressed Si3N4 | |
Eckel et al. | Strength distribution of reinforcing fibers in a Nicalon fiber/chemically vapor infiltrated silicon carbide matrix composite | |
Chou et al. | Silicon carbide platelet/alumina composites: II, mechanical properties | |
Daniel et al. | The behavior of ceramic matrix fiber composites under longitudinal loading | |
Martı́nez-Fernández et al. | Room and elevated temperature tensile properties of single tow Hi-Nicalon, carbon interphase, CVI SiC matrix minicomposites | |
Cai et al. | Crack bridging by inclined fibers/whiskers in ceramic composites | |
Griffin et al. | Evaluation of interfacial properties in borosilicate‐sic composites using pullout tests | |
Majumdar et al. | Evaluation of the Tensile Interface Strength in Brittle‐Matrix Composite Systems | |
Shetty et al. | SiC Monofilament‐Reinforced Si3N4 Matrix Composites | |
Honda et al. | Debonding criterion in the pushout process of fiber-reinforced ceramics | |
Homeny et al. | R‐Curve Behavior in a Silicon Carbide Whisker/Alumina Matrix Composite | |
Xu et al. | Effects of fiber volume fraction on mechanical properties of SiC‐fiber/Si3N4‐matrix composites | |
Xu et al. | Short‐crack mechanical properties and failure mechanisms of Si3N4‐matrix/SiC‐fiber composites | |
Becher et al. | Elevated‐Temperature‐Delayed Failure of Alumina Reinforced with 20 vol% Silicon Carbide Whiskers | |
Abbé et al. | Fiber‐Matrix Bond‐Strength Characterization of Silicon Carbide‐Silicon Carbide Materials | |
Suzuki et al. | Fiber pullout processes and mechanisms of a carbon fiber reinforced silicon nitride ceramic composite | |
Wang et al. | Mechanical Behavior of Nicalon™ Fiber‐Reinforced Calcium Aluminosilicate Matrix Composites | |
Hsueh et al. | Analyses of fiber push-out tests performed on Nicalon/SiC composites with tailored interfaces | |
Buchanan et al. | Notched Fracture Behavior of Oxide/Oxide Nextel (tm) 720/AS Composite | |
Huang et al. | Interfacial properties of SiC monofilament reinforced β′-SiAlON composites | |
Singh et al. | Effect‐of Processing Varcables on Interfacial Properties of an SiG‐Fiber‐Reinforced Reaction‐Bonded Si3N4 Matrix Composite | |
Galbraith et al. | The interfacial failure sequence during fiber pushout in metal matrix composites | |
Wetherhold et al. | Heat Treatments as a Method of Protection for a Ceramic Fiber—Glass Matrix Composite |