Feist et al., 1980 - Google Patents
Performance of mildewcides in a semitransparent stain wood finishFeist et al., 1980
View PDF- Document ID
- 779429794501808220
- Author
- Feist W
- Mraz E
- Publication year
- Publication venue
- Forest Products Journal
External Links
Snippet
The mildewcidal properties of six commercially available chemicals were evaluated as additives at three concentrations in a semitransparent oil-base wood stain. Outdoor exposure data on test specimens at three locations with distinctly different climates …
- 239000002023 wood 0 title abstract description 24
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B27—WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL; NAILING OR STAPLING MACHINES IN GENERAL
- B27K—PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR; CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- B27K3/00—Impregnating wood, e.g. impregnation pretreatment, for example puncturing; Wood impregnation aids not directly involved in the impregnation process
- B27K3/34—Organic impregnating agents
- B27K3/50—Mixtures of different organic impregnating agents
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B27—WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL; NAILING OR STAPLING MACHINES IN GENERAL
- B27K—PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR; CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- B27K3/00—Impregnating wood, e.g. impregnation pretreatment, for example puncturing; Wood impregnation aids not directly involved in the impregnation process
- B27K3/16—Inorganic impregnating agents
- B27K3/32—Mixtures of different inorganic impregnating agents
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B27—WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL; NAILING OR STAPLING MACHINES IN GENERAL
- B27K—PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR; CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- B27K3/00—Impregnating wood, e.g. impregnation pretreatment, for example puncturing; Wood impregnation aids not directly involved in the impregnation process
- B27K3/02—Processes; Apparatus
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Hoadley | Understanding wood | |
AU688525B2 (en) | Method of waterproofing wood and associated composition | |
Feist | Weathering of wood in structural uses | |
Williams | Water repellents and water-repellent preservatives for wood | |
Prieto et al. | Wood coatings | |
Feist et al. | Weathering durability of chromium-treated southern pine | |
Baysal | Surface characteristics of CCA treated Scots pine after accelerated weathering | |
Feist | Role of pigment concentration in the weathering of semitransparent stains | |
Roux et al. | Natural weathering of various surface coatings on five species at four European sites | |
Feist et al. | Performance of mildewcides in a semitransparent stain wood finish | |
Feist et al. | Performance and durability of finishes on previously coated CCA-treated wood | |
EP0682091A2 (en) | Surface treatment composition and a method for protecting the surfaces of building materials against undesirable reactions caused by microorganisms | |
Arnold et al. | Effect of weathering of new wood on the subsequent performance of semitransparent stains | |
Miller et al. | The effectiveness of end-grain sealers in improving paint performance in softwood joinery: L-joint results after 4 years natural weathering | |
US20150125712A1 (en) | Compositions and methods for resisting discoloration of wood and treated wood | |
Feist et al. | Wood finishing: Water repellents and water-repellent preservatives | |
Moody et al. | Effect of loading rate on the edgewise compressive strength of corrugated fiberboard | |
Cassens | Finishing wood exteriors: selection, application, and maintenance | |
Feist et al. | Durability of exterior natural wood finishes in the Pacific Northwest | |
Hunt | Finishing wood | |
Upreti et al. | Role of pretreatments in the protection of wood surface and finishes in the weathering of Pterocarpus marsupium wood | |
Groves et al. | Field performance of transparent coatings | |
Baysal et al. | IImpact of uv irradiance on selected parameters of scots pine impregnated with some commonly used fire-retardants | |
Morrell et al. | Protecting wood decks from biodegradation and weathering: Evaluation of deck finish systems | |
Williams et al. | Effect of surface preparation on service life of top-coats applied to weathered primer paint |