Rojas et al., 2023 - Google Patents
Fracture behaviour of plasma electrolytic oxide coatings on an aluminium substrate using acoustic emissionRojas et al., 2023
- Document ID
- 5639449628804693459
- Author
- Rojas C
- Simchen F
- Winter L
- Rymer L
- Lampke T
- Publication year
- Publication venue
- Surface and Coatings Technology
External Links
Snippet
Due to their low density and high specific strength, aluminium alloys provide a great range of application, but they are limited regarding corrosion and wear resistance. Plasma electrolytic oxidation (PEO) is an innovative process to produce oxide ceramic surfaces on aluminium to …
Classifications
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N2203/00—Investigating strength properties of solid materials by application of mechanical stress
- G01N2203/0058—Kind of property studied
- G01N2203/006—Crack, flaws, fracture or rupture
- G01N2203/0062—Crack or flaws
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N2203/00—Investigating strength properties of solid materials by application of mechanical stress
- G01N2203/02—Details not specific for a particular testing method
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Rubio-González et al. | Effect of laser shock processing on fatigue crack growth of duplex stainless steel | |
Kakiuchi et al. | Prediction of fatigue limit in additively manufactured Ti-6Al-4V alloy at elevated temperature | |
Wang et al. | Mechanical properties and microstructural response of 2A14 aluminum alloy subjected to multiple laser shock peening impacts | |
Venkatesh et al. | Microstructural response of various chromium carbide based coatings to erosion and nano impact testing | |
Kohn et al. | Acoustic emission during fatigue of Ti-6Al-4V: Incipient fatigue crack detection limits and generalized data analysis methodology | |
Zhong et al. | Fatigue crack initiation and early propagation behavior of 2A97 Al–Li alloy | |
Dai et al. | Fatigue life of micro-arc oxidation coated AA2024-T3 and AA7075-T6 alloys | |
Madhavi et al. | Influence of micro arc oxidation coating thickness and prior shot peening on the fatigue behavior of 6061-T6 Al alloy | |
Masaki et al. | Effects of laser peening treatment on high cycle fatigue properties of degassing-processed cast aluminum alloy | |
Laborda et al. | Fatigue assessment of multilayer coatings using lock-in thermography | |
Student et al. | Evaluation of the mechanical properties of combined metal-oxide-ceramic layers on aluminum alloys | |
Kabir et al. | Correlations between microstructure and room temperature tensile behavior of a duplex TNB alloy for systematically heat treated samples | |
Rojas et al. | Fracture behaviour of plasma electrolytic oxide coatings on an aluminium substrate using acoustic emission | |
Iwai et al. | Evaluation of erosive wear resistance of TiN coatings by a slurry jet impact test | |
Patel et al. | Effect of friction stir processing on plain fatigue and fretting fatigue behaviour of the AA6063 alloys | |
Heuler et al. | Fatigue behaviour of steel castings containing near‐surface defects | |
Jalali et al. | Creep micromechanics in meso-length scale samples | |
Danyuk et al. | The effect of stacking fault energy on acoustic emission in pure metals with face-centered crystal lattice | |
Simsir et al. | A comparative study of hardness/scratch/wear properties of TiCN and TiAlN coatings on DIN 1.2842 steel by CA-PVD method | |
CN117092006A (en) | Method for measuring porosity of irregular columnar structure of thermal barrier coating | |
Zhang et al. | Effects of thin cladding layer and annealing treatments on mechanical properties of AISI4340 steel | |
Dudareva et al. | The Cnfluence of Chemical Composition of Aluminum Alloys on the Quality of Oxide Layers Formed by Microarc Oxidation | |
Mikado et al. | Fatigue lifetime and crack growth behavior of WC-Co cemented carbide | |
Bidlingmaier et al. | Acoustic Emission during Room Temperature Deformation of a y-TiAl Based Alloy | |
Łępicka | Coating failure detection in scratch testing: A cross-sectional SEM/FIB microscopic study coupled with nonlinear analysis methods in a model titanium nitride/stainless steel system |