Walker, 2012 - Google Patents
Beating Crusher Wear ChallengesWalker, 2012
- Document ID
- 1898320203032143991
- Author
- Walker S
- Publication year
- Publication venue
- Engineering and Mining Journal
External Links
Snippet
Abstract"" Part lifetimes have improved in recent years. Since higher carbon grades were developed, wear resistance has improved and, subsequently in most applications, the parts last longer. According to Hanny, one top priority within the mining industry is to reduce …
- 238000010009 beating 0 title description 2
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/18—Ferrous alloys, e.g. steel alloys containing chromium
- C22C38/40—Ferrous alloys, e.g. steel alloys containing chromium with nickel
- C22C38/46—Ferrous alloys, e.g. steel alloys containing chromium with nickel with vanadium
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/18—Ferrous alloys, e.g. steel alloys containing chromium
- C22C38/24—Ferrous alloys, e.g. steel alloys containing chromium with vanadium
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C37/00—Cast-iron alloys
- C22C37/06—Cast-iron alloys containing chromium
- C22C37/08—Cast-iron alloys containing chromium with nickel
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/18—Ferrous alloys, e.g. steel alloys containing chromium
- C22C38/36—Ferrous alloys, e.g. steel alloys containing chromium with more than 1.7% by weight of carbon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C37/00—Cast-iron alloys
- C22C37/10—Cast-iron alloys containing aluminium or silicon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/04—Ferrous alloys, e.g. steel alloys containing manganese
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/12—Ferrous alloys, e.g. steel alloys containing tungsten, tantalum, molybdenum, vanadium, or niobium
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Chen et al. | Molybdenum alloying in cast iron and steel | |
Ngqase et al. | An overview on types of white cast irons and high chromium white cast irons | |
Subramanyam et al. | Austenitic manganese steels | |
CA2913601C (en) | Method for the production of high-wear-resistance martensitic cast steel and steel with said characteristics | |
RU2413576C2 (en) | Mill composite lifting element | |
CN105088055A (en) | Wear-resisting hammer head for hammer type breaking machine and production method of wear-resisting hammer head | |
CN102560272A (en) | Ultrahigh-strength abrasion-resistant steel plate and manufacturing method thereof | |
Moghaddam et al. | Impact–abrasion wear characteristics of in-situ VC-reinforced austenitic steel matrix composite | |
CN105803312A (en) | Air-cooled austenite-bainite abrasion-resistant alloy and manufacturing method thereof | |
Okechukwu et al. | Prominence of Hadfield steel in mining and minerals industries: A review | |
CN105002430A (en) | HB360 level complex-phase structure wear-resisting steel plate and production method thereof | |
CN110257728A (en) | A kind of corrosion-resistant grinder hammerhead and preparation method thereof | |
Walker | Beating Crusher Wear Challenges | |
CN1865481A (en) | Process for preparing bainite antiwear steel plate | |
CN105177436A (en) | High-strength, high-tenacity and high-wear-resistance alloy liner plate | |
Jiang et al. | Important factors affecting the gouging abrasion resistance of materials | |
US3410682A (en) | Abrasion resistant chromiummolybdenum cast irons | |
CN111440997A (en) | Ultrahigh manganese cast steel | |
Bhero et al. | Common failures of Hadfield steel in application | |
CN109055857A (en) | A kind of edge of shovel HB500 grades of martensite wear resistant steels and its processing method | |
Aubakirov et al. | Increasing the hardness of low-chromium cast irons by modifying | |
CN108914021A (en) | A kind of anti-abrasive wear alloy of Fe-Cr-B-C and preparation method thereof | |
Agunsoye et al. | Effect of heat treatment on microstructure and mechanical properties of NF6357A cast alloy for wear resistance application | |
Hurricks | Overcoming industrial wear | |
Mahlami et al. | Challenges and developments of hadfield manganese steel castings based on service life |