Canel et al., 2012 - Google Patents
Parameter optimization of nanosecond laser for microdrilling on PVC by Taguchi methodCanel et al., 2012
View PDF- Document ID
- 15780835178840008482
- Author
- Canel T
- Kaya A
- Celik B
- Publication year
- Publication venue
- Optics & Laser Technology
External Links
Snippet
Formation of cavities having maximum aspect ratio (depth-to-width (D/W) ratio) on PVC during laser drilling has several undesirable outcomes with regard to cavity quality. Hence it is essential to select optimum drilling process parameters to maximize aspect ratio and …
- 229920000915 polyvinyl chloride 0 title abstract description 16
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/02—Positioning or observing the workpiece, e.g. with respect to the point of impact; Aligning, aiming or focusing the laser beam
- B23K26/06—Shaping the laser beam, e.g. by masks or multi-focusing
- B23K26/062—Shaping the laser beam, e.g. by masks or multi-focusing by direct control of the laser beam
- B23K26/0626—Energy control of the laser beam
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/02—Positioning or observing the workpiece, e.g. with respect to the point of impact; Aligning, aiming or focusing the laser beam
- B23K26/06—Shaping the laser beam, e.g. by masks or multi-focusing
- B23K26/073—Shaping the laser spot
- B23K26/0736—Shaping the laser spot into an oval shape, e.g. elliptic shape
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/36—Removing material
- B23K26/38—Removing material by boring or cutting
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/36—Removing material
- B23K26/40—Removing material taking account of the properties of the material involved
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K26/00—Working by laser beam, e.g. welding, cutting or boring
- B23K26/02—Positioning or observing the workpiece, e.g. with respect to the point of impact; Aligning, aiming or focusing the laser beam
- B23K26/06—Shaping the laser beam, e.g. by masks or multi-focusing
- B23K26/0604—Shaping the laser beam, e.g. by masks or multi-focusing by a combination of beams
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Canel et al. | Parameter optimization of nanosecond laser for microdrilling on PVC by Taguchi method | |
| Jia et al. | Study of the dynamics of material removal processes in combined pulse laser drilling of alumina ceramic | |
| Raciukaitis et al. | Use of high repetition rate and high power lasers in microfabrication: How to keep the efficiency high? | |
| Bharatish et al. | Characterization of hole circularity and heat affected zone in pulsed CO2 laser drilling of alumina ceramics | |
| Choo et al. | Micromachining of silicon by short-pulse laser ablation in air and under water | |
| Cheng et al. | Femtosecond laser ablation of copper at high laser fluence: Modeling and experimental comparison | |
| Salleo et al. | Machining of transparent materials using an IR and UV nanosecond pulsed laser | |
| Cheng et al. | Effects of laser operating parameters on metals micromachining with ultrafast lasers | |
| Huang et al. | Femtosecond laser machining characteristics of Nitinol | |
| Yung et al. | 355 nm Nd: YAG laser ablation of polyimide and its thermal effect | |
| Li et al. | High efficiency femtosecond laser ablation of alumina ceramics under the filament induced plasma shock wave | |
| Feng et al. | Deep channel fabrication on copper by multi-scan underwater laser machining | |
| Temmler et al. | Experimental investigation on a new hybrid laser process for surface structuring by vapor pressure on Ti6Al4V | |
| Zhu et al. | A computational study of heat transfer and material removal in picosecond laser micro-grooving of copper | |
| EP3752317A1 (en) | Laser drilling and machining enhancement using gated cw and short pulsed lasers | |
| Saxena et al. | High throughput microfabrication using laser induced plasma in saline aqueous medium | |
| Mahdieh et al. | Crater geometry characterization of Al targets irradiated by single pulse and pulse trains of Nd: YAG laser in ambient air and water | |
| Li et al. | Numerical analysis of the effect of temporal and/or spatial shaping on the ms/ns combined pulse laser drilling performance of alumina ceramic | |
| Tangwarodomnukun | Overflow-assisted laser machining of titanium alloy: surface characteristics and temperature field modeling | |
| Stafe et al. | Experimental investigation of the nanosecond laser ablation rate of aluminum | |
| Bustamante et al. | Novel approach to nanosecond laser drilling of a crack-free through hole on SiC wafer | |
| Dietrich et al. | Investigation of increased drilling speed by online high-speed photography | |
| Li et al. | Laser Three-Dimensional incremental Multi-Routine interval scanning for quantitative removal of CFRP: Defect Analysis, ablation mechanism and strategy optimization | |
| Tokarev et al. | Modelling of high-aspect ratio microdrilling of polymers with UV laser ablation | |
| Mendiratta et al. | Improved quality micro-hole fabrication using backside water assisted laser micro-drilling in titanium |