Sanyal, 2017 - Google Patents
Axial crack resistance of cladding tubes for fast reactorsSanyal, 2017
- Document ID
- 1152723668970000520
- Author
- Sanyal G
- Publication year
- Publication venue
- Annals of Nuclear Energy
External Links
Snippet
Structural integrity of the core components of the nuclear reactors is vital for steady economical operation and avoidance of unwanted disasters. Two new test methods have been developed for quantifying the resistance to axial cracking of thin-walled tubular …
- 238000005253 cladding 0 title abstract description 122
Classifications
-
- G—PHYSICS
- G21—NUCLEAR PHYSICS; NUCLEAR ENGINEERING
- G21C—NUCLEAR REACTORS
- G21C3/00—Reactor fuel elements and their assemblies; Selection of substances for use as reactor fuel elements
- G21C3/02—Fuel elements
- G21C3/04—Constructional details
- G21C3/06—Casings; Jackets
- G21C3/07—Casings; Jackets characterised by their material, e.g. alloys
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GASES [GHG] EMISSION, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
- Y02E30/30—Nuclear fission reactors
- Y02E30/40—Other aspects relating to nuclear fission
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Samal et al. | Investigation of failure behavior of two different types of Zircaloy clad tubes used as nuclear reactor fuel pins | |
Jernkvist | Multi-field modelling of hydride forming metals Part II: Application to fracture | |
Du et al. | IASCC of neutron irradiated 316 stainless steel to 125 dpa | |
Holston et al. | On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding | |
Bergant et al. | Failure assessment diagram in structural integrity analysis of steam generator tubes | |
Coleman et al. | The effect of microstructure on delayed hydride cracking behavior of Zircaloy-4 fuel cladding—an International Atomic Energy Agency Coordinated Research Program | |
Plyasov et al. | A review of hydride reorientation in zirconium alloys for water-cooled reactors | |
Desquines et al. | Mechanical properties of Zircaloy-4 PWR fuel cladding with burnup 54-64MWd/kgU and implications for RIA behavior | |
Coleman et al. | Delayed hydride cracking in zircaloy fuel cladding-an IAEA coordinated research programme | |
Sanyal | Axial crack resistance of cladding tubes for fast reactors | |
Cazalis et al. | The plane strain tests in the PROMETRA program | |
Chopra et al. | A review of the effects of coolant environments on the fatigue life of LWR structural materials | |
Seok et al. | High temperature deformation characteristics of Zirlo™ tubing via ring-creep and burst tests | |
Samal et al. | Experimental evaluation of orientation and temperature dependent material stress-strain curves of Zr2. 5% Nb Indian pressure tube material and development of a suitable anisotropic material model | |
Hojna et al. | Effect of the surface grinding on the environmentally assisted crack initiation of 316 L steel in simulated pressurized water reactor water | |
Hong et al. | Mechanical Property Degradation of Unirradiated Zircaloy-4 Cladding After Creep Deformation | |
Yvon et al. | Development of new techniques to assess the mechanical behaviour of Zircaloy-4 during an RIA | |
Fullwood et al. | PRAISDPD: An aging pipe reliability analysis PC code | |
Keim et al. | Review of assessment methods used in nuclear plant life management | |
Gong et al. | Effect of Oxidation Chemistry of Supercritical Water on Stress Corrosion Cracking of Austenitic Steels | |
Yagnik et al. | Effect of hydride distribution on the mechanical properties of zirconium-alloy fuel cladding and guide tubes | |
Nagy et al. | Dynamic finite element analysis of segmented mandrel tests of hydrogenated E110 fuel cladding tubes | |
Hanlon | The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5 Nb Plate | |
Samal et al. | Compendium of Indian NPP material properties generated by RSD, BARC. Volume I, Version 1: Preamble | |
Xu et al. | Validation of weight function based process-zone model for evaluation of delayed hydride cracking initiation in Zr-2.5 Nb pressure tubes |