TW200943402A - Method for forming adhesive dies singulated from a wafer - Google Patents
Method for forming adhesive dies singulated from a waferInfo
- Publication number
- TW200943402A TW200943402A TW97112546A TW97112546A TW200943402A TW 200943402 A TW200943402 A TW 200943402A TW 97112546 A TW97112546 A TW 97112546A TW 97112546 A TW97112546 A TW 97112546A TW 200943402 A TW200943402 A TW 200943402A
- Authority
- TW
- Taiwan
- Prior art keywords
- adhesive layer
- wafer
- cut
- dies
- gap
- Prior art date
Abstract
Disclosed is a method for forming adhesive dies singulated from a wafer. A cut gap is formed between dies of the wafer. An adhesive layer formed on an extendable film is transfer-printed to the wafer. Aligned with the cut gap, a guiding groove for tearing is formed in the adhesive layer but not penetrate through. The extendable film is extended until the adhesive layer is torn into pieces along the guiding groove. Dies attached with the adhesive layer are picked up from the extendable film. Accordingly, the adhesive layer is free from cut burrs protruding from die-attaching plane at its edges, it can solve conventional problem of die-attached skew and remained gap caused by the cut burrs. Additionally, the adhesive layer is diced under low temperature to avoid improper curing at its edges.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW97112546A TWI377614B (en) | 2008-04-07 | 2008-04-07 | Method for forming adhesive dies singulated from a wafer |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW97112546A TWI377614B (en) | 2008-04-07 | 2008-04-07 | Method for forming adhesive dies singulated from a wafer |
Publications (2)
Publication Number | Publication Date |
---|---|
TW200943402A true TW200943402A (en) | 2009-10-16 |
TWI377614B TWI377614B (en) | 2012-11-21 |
Family
ID=44869007
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW97112546A TWI377614B (en) | 2008-04-07 | 2008-04-07 | Method for forming adhesive dies singulated from a wafer |
Country Status (1)
Country | Link |
---|---|
TW (1) | TWI377614B (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN102896702A (en) * | 2011-07-27 | 2013-01-30 | 隆达电子股份有限公司 | Crystal grain separation process and device thereof |
TWI614798B (en) * | 2013-02-25 | 2018-02-11 | Disco Corp | Processing method of laminated wafer |
TWI806982B (en) * | 2018-03-09 | 2023-07-01 | 日商迪思科股份有限公司 | Processing method of package substrate |
TWI810429B (en) * | 2019-01-30 | 2023-08-01 | 日商迪思科股份有限公司 | How to register the origin position of the cutting device |
-
2008
- 2008-04-07 TW TW97112546A patent/TWI377614B/en not_active IP Right Cessation
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN102896702A (en) * | 2011-07-27 | 2013-01-30 | 隆达电子股份有限公司 | Crystal grain separation process and device thereof |
TWI614798B (en) * | 2013-02-25 | 2018-02-11 | Disco Corp | Processing method of laminated wafer |
TWI806982B (en) * | 2018-03-09 | 2023-07-01 | 日商迪思科股份有限公司 | Processing method of package substrate |
TWI810429B (en) * | 2019-01-30 | 2023-08-01 | 日商迪思科股份有限公司 | How to register the origin position of the cutting device |
Also Published As
Publication number | Publication date |
---|---|
TWI377614B (en) | 2012-11-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
WO2010074906A3 (en) | Group iii-v devices with delta-doped layer under channel region | |
WO2012116207A3 (en) | Charge storage apparatus, systems and methods | |
TW200741847A (en) | Method for separating protective tape, and apparatus using the same | |
IN2013DN02549A (en) | ||
MX2019003609A (en) | Methods and devices for skin closure. | |
EP2393134A3 (en) | Encapsulating sheet for optical semiconductor | |
WO2014070534A3 (en) | Integrated bondline spacers | |
EP2575177A3 (en) | Manufacturing method of compound semiconductor device | |
MY175783A (en) | Production method for laminate film, laminate film, and production method for semiconductor device employing same | |
MY181191A (en) | Metal-foil-assisted fabrication of thin-silicon solar cell | |
WO2012109050A3 (en) | Junction termination structures including guard ring extensions and methods of fabricating electronic devices incorporating same | |
WO2016089340A3 (en) | Pre-formed thermoplastic filler for thermoset structure | |
TW200943402A (en) | Method for forming adhesive dies singulated from a wafer | |
MY162202A (en) | Methods of treating a semiconductor layer | |
PH12016500005B1 (en) | Dicing sheet | |
EP2530723A3 (en) | Photovoltaic device comprising silicon microparticles | |
SG10201907601SA (en) | Film-like adhesive composite sheet and method for manufacturing semiconductor device | |
EP2843706A3 (en) | Semiconductor device and method of fabricating the same | |
IN2012DN05153A (en) | ||
WO2012067444A3 (en) | Conductive film with an oxide film and method for producing same | |
EP4435152A3 (en) | Structures and methods for low temperature bonding | |
WO2012001600A3 (en) | Method of forming compound semiconductor nanowire | |
WO2012106223A3 (en) | Pre-cut wafer applied underfill film on dicing tape | |
WO2015034366A3 (en) | A method for manufacturing a ceramic roof tile provided with a solar panel | |
GB2525821A (en) | Lens-foil based security device |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |