SU617105A1 - Shaping sleeve for making thin-wall helical-seam tubes - Google Patents
Shaping sleeve for making thin-wall helical-seam tubesInfo
- Publication number
- SU617105A1 SU617105A1 SU772458109A SU2458109A SU617105A1 SU 617105 A1 SU617105 A1 SU 617105A1 SU 772458109 A SU772458109 A SU 772458109A SU 2458109 A SU2458109 A SU 2458109A SU 617105 A1 SU617105 A1 SU 617105A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- sleeve
- making thin
- shaping sleeve
- wall helical
- seam tubes
- Prior art date
Description
(54) ФОРМОВОЧНАЯ ВТУЛКА ДЛЯ ИЗГОТОВЛЕНИЯ ТОНКОСТЕННЫХ СПИРАЛЬНОШОВНЫХ ТРУБ(54) FORMING SLEEVE FOR THE MANUFACTURE OF THIN-WALLED HEELING PIPES
между (ПОЛОСОЙ и внулремней шоверхностью втулки.between (the strip and the inner surface of the sleeve).
Это достигаетс тем, что формавочна втулка снабжена штуцером дл .подвод смазки IB спиральные 1ка навки, укрепленным на наружной ;по:верхности Бтул1ки ;со ст.О рО:НЫ, противоположной трарези дл задачи полосы, а спиральные «ащавки щьипошнены с переменным сечением , уменьшающимс -по длине втулки в сторону .выхода из иее трубы.This is achieved by the fact that the mold bushing is equipped with a fitting for lubricant IB supplying helical housings fixed on the outer; along: the surface of Btul1ka; with st.O pO: HY, opposite to the trarez for the task of the strip, and spiral wound with variable cross-section decreasing along the length of the sleeve to the side of the exit from its pipe.
Та.кое 1зы;пол1нение |фо.р.мово1чной втулки абвапечивает уменьшение удельных давлений при фюрмовке за счет снижени сил трени на ко«та1ктной повархно-сти, так как в предлагаемом устройстве формуема полоса движетс по тсакому слою омазки.This procedure is complete; reduction of the specific pressures during the fattening process due to the reduction of the frictional forces on the tactical surface, as in the proposed device, the strip is moving along a layer of amazka.
На фит. 1 изображена формо1вочна1Я втулжа, общий вид; на фит. 2 - раз.рез Л-Л на фиг. 1.On the fit. 1 shows a mold sleeve, a general view; on fit. 2 is a cut. LL in FIG. one.
Фор|мовочна втулка щыполпеаа со спиральными KaHaiBKaiMH i/ переменного сечени1Я на ее ра-бочей внутренней поверхности И дро.рез ми 2 дл задачи IB нее полосы. На наружной inoверхиости втулки со стороны, противоположной ирорези дл задачи .полосы, укреплен штуцер 3 дл подвода смазки в спиральные канавки и фланец 4 дл .креплени втулки IK станине тру;бофо)р.мовочнОГО 1стана.Forming sleeve sleeve with spiral KaHaiBKaiMH i / variable cross-section on its working inner surface and half-cut 2 for task IB of its strip. On the outer in-hub of the sleeve on the side opposite to the rifle for the task. Bands, a fitting 3 is fixed for supplying lubricant to the spiral grooves and the flange 4 for fastening the sleeve IK to the frame;
Полоса задаетс IB формующую втулку и движетс .00 внутренней цилиндрической поверхности , одновременно смазыва; сь |пастообразной Омаз,кой, на.ход щейс. в спиральных каназках лод рвгул«руемы(м давлением. Давление в смазочной системе создаетс питателем 5, который поддерживает его Цостолины.м в пределах -ЮО-200 кг/см в зависимости от контактных условий формовки и обесиечивает равно,мерность расхода .смазочной пасты в течение всего процесса формовки и наличие ее тонкого СЛ01Я н.а контактной .пдверхности полосы .и втулки. Консистентностью смазки и размерами 1Пр01фил канавок достигаетс стабильна -мала толщина смазочного сло , снижающего .коэффищиент трени 1п,ри движении за1готовки. При полоса движетс каК бы на смазочной подушке, 1котора .посто нно .подпитываетс ннтателем омазки. В результате заталкиваю .щее усилие трубы диаметром 186 м (ТУ-;14-|3-351-7|5) в формующей втуЛ|Ке из чупуна СЧ ,32-52 (ГОСТ 1412-70) при скорости задачи .полосы 0,3.3 мм/сек составл ет 310 кг. При формОВке |без смазки заталкивающее усилие составл ет 1100 кг. Снижение заталкивающиХ усилий и удельных давле ний при формовке дает ВОЗМОЖНОСТЬ увеличить скор.ости формовки И, тем самым, увеличить производитель;юсть ста а. При выходе из формующей втулки уменьщенивм сечени 1К.анаво.к достигаетс частичное удаление смазочного сло с поверхности трубы. Толщина смазочной пленки, уно .С1им.ай с трубы, находитс в пределах 0,01 - 0,02 мм и, таким образо.м, расход сма.зки составл ет 0,.2 л на 100 1ПО.Г. .метров трубы. Далее осуществл етс контактна. радиочастотна ава.рка трубы.The strip is set by an IB forming sleeve and moves .00 the inner cylindrical surface, simultaneously lubricating; Plasma Omese, Coy, on the way. in spiral Kanazkas of a boat rvgul "ruyema (m pressure. The pressure in the lubrication system is created by a feeder 5, which maintains its Capostolins m within-South-200 kg / cm, depending on the contact conditions of the molding, and equals equally during the whole process of forming and the presence of its thin SL01Ya on the contact strip at the top of the strip and bushings. The blade moves as if on a lubricant cushion, which is permanently. Supported by a reamer. As a result, I push the force of a pipe with a diameter of 186 m (TU-; 14- | 3-351-7 | 5) in the forming wedge | , 32-52 (GOST 1412-70) with a task speed of 0.3.3 mm / s is 310 kg. Forming without lubrication, the pushing force is 1100 kg. Reducing the pressing forces and specific pressures during molding provides an opportunity to increase forming speed And, thereby, to increase the manufacturer; When leaving the forming sleeve, a 1K. Manhole section is reduced in size. Partial removal of the lubricating layer from the pipe surface is achieved. The thickness of the lubricant film, Uno.Si.im.ay from the pipe, is in the range of 0.01-0.02 mm and, thus, the consumption of the lubricant is 0 .2 l per 100PO.G. . meters of pipe. Next is the contact. radio frequency ava.rka pipe.
Формующа втулка мо.жет быть ирименена в трубопрокатной промышленности на всех станах спиральношовной сварки труб диаметфОМThe forming bushing can be used in the tube-rolling industry at all mills for spiral welding of pipes with a diameter of
100-350 мм, выпускаемых .промы1щ.ленностью СОСР.100-350 mm, manufactured by industry.
Фор мующа втулка данной конструкции позвол . ет уменьшить заталкив,ающие усили и удельные давлени при .формовке за счет снижени коэффициентов трени .фор.муемой лолосы с ра-бочей поверхностью формующей втулки .при наличиИ смазки на их контактных поверхност х, IB результате чего .по вл етс возможность увеличить у1по.л формовки, толщииу полосы, применить данную формующую втулку ДЛЯ формаВ|КИ т.ру.б с большим диаметром , значительно уменьшить износ рабочей поверхности втулки, повысить производительность стана за счет увеличени скорости форМОЗКИ .The shaping sleeve of this design allows. It is possible to reduce pushing, pressing forces and specific pressures during shaping by reducing friction coefficients of the formulated loop with the working surface of the forming sleeve, if there is grease on their contact surfaces, IB resulting in the possibility of increasing y1po. l molding, thick strip, apply this forming sleeve FOR forms | KI t.rub with a large diameter, significantly reduce the wear of the working surface of the sleeve, improve the productivity of the mill by increasing the speed of molding.
На Ворошиловградско.м заводе вм. Якубовакого разра|ботан paiб.oчий проект чертежей и изготовлен опытный образец. Внедрение П редлагаемо1го уст1ройства намечено .планом Министерства черной мета.ллургии на IV квартал 1977 года.At Voroshilovgrad. Plant vm. Yakubovky developed a pai bai design of the drawings and a prototype was made. The introduction of the Preferred Device is scheduled for the IV quarter of 1977 by the Ministry of Black Meteorology.
Claims (3)