SU59036A1 - The method of obtaining solid elastic polymers of ethylene - Google Patents

The method of obtaining solid elastic polymers of ethylene

Info

Publication number
SU59036A1
SU59036A1 SU22132A SU22132A SU59036A1 SU 59036 A1 SU59036 A1 SU 59036A1 SU 22132 A SU22132 A SU 22132A SU 22132 A SU22132 A SU 22132A SU 59036 A1 SU59036 A1 SU 59036A1
Authority
SU
USSR - Soviet Union
Prior art keywords
ethylene
solid elastic
elastic polymers
obtaining solid
atm
Prior art date
Application number
SU22132A
Other languages
Russian (ru)
Inventor
А.И. Динцес
Н.И. Постнов
Original Assignee
А.И. Динцес
Н.И. Постнов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.И. Динцес, Н.И. Постнов filed Critical А.И. Динцес
Priority to SU22132A priority Critical patent/SU59036A1/en
Application granted granted Critical
Publication of SU59036A1 publication Critical patent/SU59036A1/en

Description

Известно (золучение твердых эластичных полимеров этилена путем полимеризации последнего при давлении свыше 1000 атм. в присутствии индиферентных газов и при температурах от 100 до 400.It is known (zolishing of solid elastic polymers of ethylene by polymerization of the latter at pressures above 1000 atm. In the presence of indifferent gases and at temperatures from 100 to 400.

Авторы насто щего изобретени  предлагают способ получени  твердых эластичных полимеров этилена также при давлении свыше 1000 атм. и температуре выше 100°, состо щий в том, что в реакционный аппарат сначала ввод т воду, а затем при повышении давлени  и температуры в аппарат загружают этилен.The authors of the present invention propose a method for producing solid elastic polymers of ethylene, also at pressures above 1000 atm. and a temperature above 100 ° C, consisting in that water is first introduced into the reaction apparatus, and then ethylene is charged into the apparatus with increasing pressure and temperature.

Введение в реакционный аппарат воды , как установлено авторами изобретени , не преп тствует получению чистых стандартных твердых полимеров этилена с температурой плавлени  около ИО и молекул рным весом - 8 000. В то же врем  вследствие большой теплоемкости и большой скрытой теплоты вода способствует уничтожению местных перегревов, возможных вследствие большой экзотерд ичности реакции, благодар  чему устран етс  опасность взрывов; вместе с тем вода заметно ускор ет, пр,9 цесс полимеризации., . The introduction of water into the reaction apparatus, as established by the inventors, does not prevent the preparation of pure standard solid polymers of ethylene with a melting point of about IO and a molecular weight of 8,000. At the same time, due to the large heat capacity and large latent heat, possible due to the large exotherm of the reaction, which eliminates the danger of explosions; At the same time, water noticeably accelerates, pr, 9, the polymerization process.,.

Технологический процесс при осуществлении предлагаемого способа проводитс  по приводимому ниже примеРУПример . В реактор емкостью 80 мл загружаетс  28 вес. ч. свеже прокип ченой воды. Реактор промываетс  трижды этиленом под давлением 20 атм. и заполн етс  жидким этиленом при давлении 1300 атм. Температура реактора доводитс  до 280°, давление при этом возрастает до 2900 атм., а затем: начинает падать и через 4 часа доходит до 1500 атм. При этом образуетс  50% от этилена полимера, обладающего стандартными качествами, т. е. имеющего температуру плавлени  около 140 и молекул рный вес - 8000.The technological process in the implementation of the proposed method is carried out according to the following example. Example. In the reactor with a capacity of 80 ml is loaded 28 weight. h. freshly prokip chenoy water. The reactor is washed three times with ethylene at a pressure of 20 atm. and is filled with liquid ethylene at a pressure of 1300 atm. The temperature of the reactor is brought to 280 °, the pressure at the same time increases to 2900 atm., And then: it begins to fall and after 4 hours it reaches 1500 atm. This forms 50% of ethylene polymer with standard qualities, i.e. having a melting point of about 140 and a molecular weight of 8,000.

Преимущества предлагаемого способа , по сравнению с существующими методами получени  твердых эластичных полимеров этилена, видны из описанного выше и заключаютс , главным образом, в устранении возможности взрывов, ускорении процесса и чистоте получаемого продукта.The advantages of the proposed method, compared with the existing methods for producing solid elastic polymers of ethylene, can be seen from the above and consist mainly in eliminating the possibility of explosions, speeding up the process and purity of the resulting product.

Предмет изобретени .The subject matter of the invention.

Способ получени  твердых эластич , пблимёров,, этилена при., The method of obtaining solid elastic, heat, ethylene, at.,

свыше 1000 атм. и температуре выше 100°, отличающийс  тем, что в реакционный аппарат сначала загружают воду, затем при повышенных давлении и температуре ввод т этилен.over 1000 atm. and a temperature above 100 ° C, characterized in that water is first charged into the reaction apparatus, then ethylene is introduced at elevated pressure and temperature.

SU22132A 1939-02-27 1939-02-27 The method of obtaining solid elastic polymers of ethylene SU59036A1 (en)