SU522131A1 - The method of obtaining strontium sulfide solution - Google Patents
The method of obtaining strontium sulfide solutionInfo
- Publication number
- SU522131A1 SU522131A1 SU2037939A SU2037939A SU522131A1 SU 522131 A1 SU522131 A1 SU 522131A1 SU 2037939 A SU2037939 A SU 2037939A SU 2037939 A SU2037939 A SU 2037939A SU 522131 A1 SU522131 A1 SU 522131A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- water
- stage
- strontium sulfide
- sulfide solution
- solution
- Prior art date
Description
(54) СПОСОБ ПОЛУЧЕНИЯ РАСТВОРА СУЛЬФИДА СТРОНЦИЯ(54) METHOD FOR OBTAINING STRONTIUM SULFIDE SOLUTION
После i 5 мии 1о6работки при 85°С суспензию суль4шдд стронци отвод т из мельншхы и раздел ют на барабанном вакуум-фильтре, откуда отвод т в качестве продукционного 33,86 кг/мин раствора суль фида строгани концентрацией 11,39%. В раствор пе- : реходит 97% водорастворимых солей стронци , содержащихс в плаве. Шлам в количестве 1,94 кг направЛЯ|От в реактор с мешалкой, куда одновременно подают 30 кг воды, что соответствует соотношению/ Т 1К, равному 1:15. Водную обработку на второй стадии ведут в течение 40 мин при , после чего суспензию раздел ют на барабанном вакуумфильтре , отфильтрованный раствор с когщентрацией 1,32% в количестве 30,4 кт подают в иировую мельницу на первую стадию, а шлам в количестве 1,24 кг направл ют на обезвреживание.After i5 mii 1-6 processing at 85 ° C, the suspension of sul4shdd strontium is removed from the mill and separated on a drum suction filter, from which 33.86 kg / min of a planing sulfide solution with a concentration of 11.39% is removed as a production one. 97% of water-soluble strontium salts contained in the melt are transferred to the solution. Sludge in the amount of 1.94 kg directing | From into the reactor with a stirrer, which simultaneously serves 30 kg of water, which corresponds to the ratio / T 1K, equal to 1:15. Water treatment in the second stage is carried out for 40 minutes, after which the suspension is separated on a drum-type vacuum filter, the filtered solution with a co-concentration of 1.32% in an amount of 30.4 kt is fed to an iridescent mill in the first stage, and the slurry in an amount of 1.24 kg sent for disposal.
В предлагаемом способе расход воды на обработку уменьшаетс в 1,3 - 1,9 раза, а степень перехода /In the proposed method, the water consumption for treatment is reduced 1.3-1.9 times, and the degree of transition /
водорастворимых солей стронци в раствор повы1шетс до 97% против 90% по известному способу.water-soluble strontium salts in solution will rise to 97% versus 90% by a known method.
Claims (2)