[go: up one dir, main page]

SU516490A1 - Solder flux - Google Patents

Solder flux

Info

Publication number
SU516490A1
SU516490A1 SU2054025A SU2054025A SU516490A1 SU 516490 A1 SU516490 A1 SU 516490A1 SU 2054025 A SU2054025 A SU 2054025A SU 2054025 A SU2054025 A SU 2054025A SU 516490 A1 SU516490 A1 SU 516490A1
Authority
SU
USSR - Soviet Union
Prior art keywords
flux
heat
resistant
solder
ammonium bifluoride
Prior art date
Application number
SU2054025A
Other languages
Russian (ru)
Inventor
Анатолий Васильевич Толстоусов
Original Assignee
Предприятие П/Я В-8843
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я В-8843 filed Critical Предприятие П/Я В-8843
Priority to SU2054025A priority Critical patent/SU516490A1/en
Application granted granted Critical
Publication of SU516490A1 publication Critical patent/SU516490A1/en

Description

1one

Изобретение относитс  к области пайки, в частности к составам флюса дл  пайки преимущественно нержавеющих, жаростойких и жаропрочных сталей медно-цинковыми припо ми.The invention relates to the field of soldering, in particular to flux compositions for soldering, mainly stainless, heat-resistant and heat-resistant steels with copper-zinc solder.

Известен флюс дл  пайки нержавеющих и жаропрочных сталей медно-цинковыми припо ми, содержащий 50 % буры 50 % борной кислоты.A known flux for brazing stainless and heat-resistant steels with copper-zinc alloys, containing 50% borax 50% boric acid.

Основным недостатком известного флюса  вл етс  невысока  активность при пайке указанных материалов.The main disadvantage of the known flux is the low activity when soldering these materials.

Цель изобретени  - создание флюса дл  пайки нержавеющих, жаростойких и жаропрочных сталей, обладающего повьппенной активностью и обеспечивающего получение качественного па ного соединени , выполненного медно-цинковыми припо ми .The purpose of the invention is to create a flux for soldering stainless, heat-resistant and heat-resistant steels with high activity and providing high-quality brazing compound made of copper-zinc solders.

Это достигаетс  путем введени  в известный состав флюса бифторида аммони .This is achieved by incorporating ammonium bifluoride into a known flux composition.

Предлагаемьш флюс имеет следующий состав, вес %:Offered flux has the following composition, weight%:

Бура30-40Bura 30-40

Бифторид аммони 10-20Ammonium bifluoride 10-20

Борна  кислотаОстальноеBorna acidErest

Повышенна  активность предлагаемого флюса позвол ет получать качественное па ное соединение The increased activity of the proposed flux allows to obtain high-quality solder compound.

без предварительной загибки поверхности па емого материала.without pre-folding the surface of the material to be fallen.

Предлагаемый флюс не оказьшает коррозионного воздействи  на па емый материал.The proposed flux does not corrode the burned material.

Дл  испьггани  активности флюса был вз т образец из стали Х18П9Т размером 5050 5. На незачищенную поверхность наносилс  равным слоем флюс следующего состава, вес. %: бура 35, бифторид аммони  15, борна  кислота остальное и Юг латунного припо , с внутренней стороны пластина нагревалась газовой горелкой ГЗУ-2-62 до температуры плавлени  флюса и припо . При нагреве флюс равномерно растекс  по поверхности пластины , после чего расплавилс  припой, образу  равномерную площадь растекани  припо . После удалени  флюса пластина имела чистую светлую поверхность с равномерно растекщимс  припоем.To use flux activity, a sample of steel 50505 in size H18P9T was taken. A flux of the following composition, weight, was applied on an uncleaned surface with an equal layer. %: borax 35, ammonium bifluoride 15, boric acid else and the south of brass solder, on the inner side the plate was heated with a gas burner GZU-2-62 to the melting point of the flux and solder. When heated, the flux spread evenly over the surface of the plate, after which the solder was melted, forming a uniform area of solder flow. After removing the flux, the plate had a clean, bright surface with uniformly spreadable solder.

Claims (1)

Формула изобретени Invention Formula Флюс дл  пайки нержавеющих, жаростойких и жаропрочных сталей медно-цинковыми припо ми, содержащий борную кислоту и буру, отличающийс  тем, что, с целью повыщени  активности о516490 cJ флюса и получени  качественного па ного соединеНИЛ , его состав дополнительпо содержит бифторид аммони  при следующем соотношении компонентов ,вес. %: 4 Бура30-40 Бифторид аммони 10-20 Борна  кислотаОстальноеThe flux for brazing stainless, heat-resistant and heat-resistant steels with copper-zinc alloys containing boric acid and borax, characterized in that, in order to increase the activity of o516490 cJ flux and obtain high-quality brazing compound, its composition additionally contains ammonium bifluoride in the following ratio ,weight. %: 4 Bura30-40 Ammonium bifluoride 10-20 Borna acidOstal
SU2054025A 1974-08-16 1974-08-16 Solder flux SU516490A1 (en)