[go: up one dir, main page]

SU417520A1 - - Google Patents

Info

Publication number
SU417520A1
SU417520A1 SU1765099A SU1765099A SU417520A1 SU 417520 A1 SU417520 A1 SU 417520A1 SU 1765099 A SU1765099 A SU 1765099A SU 1765099 A SU1765099 A SU 1765099A SU 417520 A1 SU417520 A1 SU 417520A1
Authority
SU
USSR - Soviet Union
Prior art keywords
iron
cast iron
silicon
carbon
vanadium20
Prior art date
Application number
SU1765099A
Other languages
Russian (ru)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1765099A priority Critical patent/SU417520A1/ru
Application granted granted Critical
Publication of SU417520A1 publication Critical patent/SU417520A1/ru

Description

1one

Изобретение относитс  к области черной металлургии и литейного производства, в частности , к производству лигатур дл  получени  износостойких отливок из железоуглеродистых сплавов.The invention relates to the field of ferrous metallurgy and foundry, in particular, to the manufacture of master alloys for the production of wear-resistant castings from iron-carbon alloys.

Известна лигатура дл  чугуна, содержаща  углерод, кремний, хром, ванадий, никель и железо.Known ligature for cast iron containing carbon, silicon, chromium, vanadium, nickel and iron.

С целью повышени  физико-механических свойств чугуна она дополнительно содержит медь при следующем соотношении компонентов , %:In order to improve the physical and mechanical properties of cast iron, it additionally contains copper in the following ratio of components,%:

Углерод0,1-2,5Carbon 0.1-2.5

Кремний10-20Silicon 10-20

Хром15-25Chrome 15-25

Ванадий20-45Vanadium20-45

Никель15-35Nickel15-35

Медь0,1 - 10Copper0,1 - 10

ЖелезоОстальноеIronErest

Лигатура легкоплавка  и поэтому хорошо усваиваетс  при вводе на желобе вагранки и позвол ет получать износостойкий чугун непосредственно из ваграночного чугуна.The ligature is fusible and therefore well assimilated when the cupola is placed on the chute and allows to obtain durable cast iron directly from cupola iron.

предмет изобретени subject matter

Лигатура дл  чугуна, содержаща  углерод, кремний, хром, ванадий, никель и железо, отличающа с  тем, что, с целью повышени  физико-механических свойств чугуна, она дополнительно содержит медь при следующем соотношении компонентов, %:The master alloy for cast iron, containing carbon, silicon, chromium, vanadium, nickel and iron, characterized in that, in order to improve the physical and mechanical properties of cast iron, it additionally contains copper in the following ratio of components,%:

Углерод0,1-2,5Carbon 0.1-2.5

Кремний10-20Silicon 10-20

Хром15-25Chrome 15-25

Ванадий20-45Vanadium20-45

Никель15-35Nickel15-35

Медь0,1-10Copper0,1-10

ЖелезоОстальноеIronErest

SU1765099A 1972-03-28 1972-03-28 SU417520A1 (en)