[go: up one dir, main page]

SU355876A1 - Method of obtaining indium by electrolytic refining - Google Patents

Method of obtaining indium by electrolytic refining

Info

Publication number
SU355876A1
SU355876A1 SU7001456437A SU1456437A SU355876A1 SU 355876 A1 SU355876 A1 SU 355876A1 SU 7001456437 A SU7001456437 A SU 7001456437A SU 1456437 A SU1456437 A SU 1456437A SU 355876 A1 SU355876 A1 SU 355876A1
Authority
SU
USSR - Soviet Union
Prior art keywords
resin
electrolyte
metal
brand
capacity
Prior art date
Application number
SU7001456437A
Other languages
Russian (ru)
Inventor
Л.И. Юрченко
С.А. Алексеев
В.Е. Дьяков
А.Е. Семенов
М.А. Яковлев
Original Assignee
Новосибирский оловянный комбинат
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Новосибирский оловянный комбинат filed Critical Новосибирский оловянный комбинат
Priority to SU7001456437A priority Critical patent/SU355876A1/en
Application granted granted Critical
Publication of SU355876A1 publication Critical patent/SU355876A1/en

Links

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P10/00Technologies related to metal processing
    • Y02P10/20Recycling

Landscapes

  • Electrolytic Production Of Metals (AREA)

Claims (1)

(54) СПОСОБ ПОЛУЧЕНИЯ ИНДИЯ ЭЛЕКТРОЛИТИЧЕСКИМ Изобретение относитс  к области гидрометаллургии рассе нных метаплов. Известен способ получени  инди  высок чистоты электролитическим рафинированием в хлоридном электролите с очисткой электролита на ионообменной смоле. Однако этот способ не обеспечивает полной очист металла от примесей олова и ртути и емкость смолы быстро падает. По предложенному способу электролит после операции анодного растворени  пере очисткой на смоле пропускают через слой активированного угл  и возвращают на катодное осаждение. Способ повышает чисто ту металла и емкость -смолы. Дл  рафинировани  .используют аноды и инди  марки состава,вес%: о Германий l-lOt Германий Олово Свиней 6 Кадмий Никель 4 Мышь к Цинк Ргутъ РАФИНИРСЖАНИЕМ хлор-ионов, рН 1-1,5. Сила на ванне 2Оа, напр жение 2 В, анодна  плотность тока 2,2 А/дм . Электролит на очистку выводитс  со скоростью 3-5 л/ч из анодного пространства . Колонна с углем имеет высоту 1 М и диаметр 6О мм. В нее загружают 1,5 кг угл  марки СКТ. Катодный металл получают в виде губки, следующего состава, вес%: Железо Мышь к Галлий Германий 1 1О 210 Таллий Цинк 1-10 По содержанию примесей этот металл соответствует марке ИН-ОО. Пр мой выход инди  75,4%. Формула изобретени (54) METHOD FOR OBTAINING INDIA ELECTROLYTIC The invention relates to the field of hydrometallurgy of scattered metafields. A known method of obtaining high purity indie by electrolytic refining in a chloride electrolyte with the purification of the electrolyte on an ion exchange resin. However, this method does not ensure complete purification of the metal from impurities of tin and mercury and the capacity of the resin decreases rapidly. According to the proposed method, the electrolyte after the anodic dissolution operation is re-cleaned on the resin is passed through a layer of activated carbon and returned to cathodic deposition. The method increases the pure metal and the capacity of the resin. For refining. Anodes and indies of the composition brand, weight%: o Germanium l-lOt Germanium Tin Pigs 6 Cadmium Nickel 4 Mouse to Zinc Chlorine ions pH 1-1.5. Bath strength 2Oa, voltage 2 V, anode current density 2.2 A / dm. The electrolyte for cleaning is removed at a rate of 3-5 l / h from the anode space. The column with coal has a height of 1 M and a diameter of 6 mm. 1.5 kg of SKT brand coal is loaded into it. The cathode metal is obtained in the form of a sponge, of the following composition, weight%: Iron Mouse to Gallium Germanium 1 1 210 210 Thallium Zinc 1-10 According to the content of impurities, this metal corresponds to the IN-OO brand. Pr my output indi 75.4%. Invention Formula .4 355876.4 355876 3434 с целью повышени  чистоты металла исмоле пропускают через слой активированноемкости смолы, электролит после операции. . го пгл и возвращают на катодное осажанодного растворени  перед очисткой надение.In order to increase the purity of the metal, the resin is passed through an activated resin capacity, the electrolyte after the operation. . go pgl and return to cathodic precipitated dissolution before cleaning put on. ..- ...-.
SU7001456437A 1970-06-24 1970-06-24 Method of obtaining indium by electrolytic refining SU355876A1 (en)