SU104599A1 - The method of preparation of dyed cotton for sale - Google Patents
The method of preparation of dyed cotton for saleInfo
- Publication number
- SU104599A1 SU104599A1 SU453587A SU453587A SU104599A1 SU 104599 A1 SU104599 A1 SU 104599A1 SU 453587 A SU453587 A SU 453587A SU 453587 A SU453587 A SU 453587A SU 104599 A1 SU104599 A1 SU 104599A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- cotton
- sale
- preparation
- dyed cotton
- solution
- Prior art date
Description
ИзвесП(), что дл того, чтобы в пр дильном производстве nepe|it.ботка окрапюнного хлопка протекала ycneiniio. пеобходимо пар ду с другими требующимис свойствами ирпдать хлопку достаточные упругое-.; и электропроводиость.IzvesP (), so that in spin production nepe | it.working of pericunum cotton proceeded ycneiniio. it is necessary to pair with other required properties to bind sufficient cotton elastic- .; and electrical conductivity.
В еилу того, что эти свойства у окраи1епиого хлопка хуже, чем у сурового , окрашеипый хлопок обрабатывают , например, раствором поваренпой соли дл сообщеип емл электропроводности, тер емой в про цессе крашени и промывки. Прч этом окрашенный хлопок обычно пе эмульсируют, так как обработка эмульсией, содержащей олеииовое мыло, сиижает упругость хлопка, что ухудшает его пр дильные свойства.To the extent that these properties of poker cotton are worse than those of severe cotton, they are treated, for example, with a solution of cooking salt for the common electrical conductivity lost during dyeing and washing. In this case, dyed cotton is usually not emulsified, since the treatment with an emulsion containing oleiic soap causes the elasticity of the cotton to deteriorate, which deteriorates its spin properties.
Предлагаемый способ позвол ет одиовремеиио повысить электропроводность и упругость окрашенного хлопка, что достигаетс обработкой его после промывки раствором попаренной соли, содержащем мыло из высокомо.текул рно прсде. 1чирмо11 кислоты, и высунпи ают. The proposed method allows odoutime to increase the electrical conductivity and elasticity of dyed cotton, which is achieved by treating it after washing with a solution of a steamed salt containing high-quality soap. 1chimo11 acid, and pop out.
Дл осуи1.ествленн способа готов т на МЯГКО воде раствор, содержащий 10 c/J, например, стеаринового мыла и 2 г:.1 поваренной соли.For this method, a solution containing 10 c / J of, for example, stearic soap and 2 g: .1 table salt is prepared on a SOFT water.
Обработку промытого окра1пенного хлопка таким раствором ripii телтературе не ниже 30°, пос.те чего хлопок высушивают.The treatment of washed cotton with such a solution of ripii telemetry is not lower than 30 °, after which the cotton is dried.
Предмет изобретепи Subject invention
Способ подготовки окрашеииого хлопка к пр дению путем обработки его после краикии раствором поваренной соли, отличающийс тем, что, с пелью придани окрапгенному волокну повышенной элект1Уопроводности и упругости, после про-мывки его обрабатывают раствором, со.тержащим поваренную соль и мы .ю из высокомолекул рной предельной жирной кислоты, и высунглнаютA method of preparing colored cotton for spraying by treating it after cracking with a solution of sodium chloride, characterized in that, with a special effect, the electroplating and elasticity of the opaque fiber is treated with a solution containing sodium chloride and we are made from a high molecular weight after washing. prue fatty acid, and get out