[go: up one dir, main page]

RU2445392C1 - Cast iron - Google Patents

Cast iron Download PDF

Info

Publication number
RU2445392C1
RU2445392C1 RU2011115307/02A RU2011115307A RU2445392C1 RU 2445392 C1 RU2445392 C1 RU 2445392C1 RU 2011115307/02 A RU2011115307/02 A RU 2011115307/02A RU 2011115307 A RU2011115307 A RU 2011115307A RU 2445392 C1 RU2445392 C1 RU 2445392C1
Authority
RU
Russia
Prior art keywords
cast iron
iron
barium
molybdenum
calcium
Prior art date
Application number
RU2011115307/02A
Other languages
Russian (ru)
Inventor
Юлия Алексеевна Щепочкина (RU)
Юлия Алексеевна Щепочкина
Original Assignee
Юлия Алексеевна Щепочкина
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Юлия Алексеевна Щепочкина filed Critical Юлия Алексеевна Щепочкина
Priority to RU2011115307/02A priority Critical patent/RU2445392C1/en
Application granted granted Critical
Publication of RU2445392C1 publication Critical patent/RU2445392C1/en

Abstract

FIELD: metallurgy.
SUBSTANCE: cast iron contains the following components, wt %: carbon 2.0-2.8; silicon 0.8-1.2; manganese 0.8-1.2; chrome 0.1-0.2; barium 0.001- 0.002; molybdenum 1.5-1.9; nickel 4.0-4.5; calcium 0.001-0.002; copper 0.3-0.7; boron 0.1-0.15; hafnium 0.2-0.3; and iron is the rest.
EFFECT: increasing cast iron thermal resistance.
1 tbl

Description

Изобретение относится к области черной металлургии, в частности к составам чугуна, который может быть использован в машиностроении.The invention relates to the field of ferrous metallurgy, in particular to compositions of cast iron, which can be used in mechanical engineering.

Известен чугун, содержащий, мас.%; углерод 2,0-2,8; кремний 0,7-2,5; марганец 0,3-1,2; хром 0,1-1,0; барий 0-0,2; молибден 0-0,7; никель 0-3,0, кальций 0-0,2; железо - остальное [1].Known cast iron, containing, wt.%; carbon 2.0-2.8; silicon 0.7-2.5; manganese 0.3-1.2; chrome 0.1-1.0; barium 0-0.2; molybdenum 0-0.7; nickel 0-3.0; calcium 0-0.2; iron - the rest [1].

Задачей изобретения является повышение термостойкости чугуна.The objective of the invention is to increase the heat resistance of cast iron.

Технический результат достигается тем, что чугун, содержащий углерод, кремний, марганец, хром, барий, молибден, никель, кальций, железо, дополнительно включает медь, бор, гафний при следующем соотношении компонентов, мас.%: углерод 2,0-2,8; кремний 0,8-1,2, марганец 0,8-1,2, хром 0,1-0,2; барий 0,001-0,002; молибден 1,5-1,9; никель 4,0-4,5; кальций 0,001-0,002; медь 0,3-0,7; бор 0,1-0,15; гафний 0,2-0,3; железо - остальное.The technical result is achieved by the fact that cast iron containing carbon, silicon, manganese, chromium, barium, molybdenum, nickel, calcium, iron, additionally includes copper, boron, hafnium in the following ratio of components, wt.%: Carbon 2.0-2, 8; silicon 0.8-1.2, manganese 0.8-1.2, chromium 0.1-0.2; barium 0.001-0.002; molybdenum 1.5-1.9; nickel 4.0-4.5; calcium 0.001-0.002; copper 0.3-0.7; boron 0.1-0.15; hafnium 0.2-0.3; iron is the rest.

В таблице приведены составы чугуна.The table shows the composition of cast iron.

ТаблицаTable КомпонентыComponents Содержание, мас.% в составахContent, wt.% In the compositions 1one 22 33 УглеродCarbon 2,02.0 2,42,4 2,82,8 КремнияSilicon 1,21,2 1,01,0 0,80.8 МарганецManganese 1,21,2 1,01,0 0,80.8 ХромChromium 0,20.2 0,250.25 0,10.1 БарийBarium 0,0010.001 0,00150.0015 0,0020.002 МолибденMolybdenum 1,91.9 1,71.7 1,51,5 НикельNickel 4,04.0 4,34.3 4,54,5 КальцийCalcium 0,0020.002 0,00150.0015 0,0010.001 МедьCopper 0,30.3 0,50.5 0,70.7 БорBoron 0,150.15 0,130.13 0,10.1 ГафнийHafnium 0,20.2 0,250.25 0,30.3 ЖелезоIron остальноеrest остальноеrest остальноеrest Термостойкость (нагрев до 450°C - охлаждение до 20°C в воде), циклыHeat resistance (heating to 450 ° C - cooling to 20 ° C in water), cycles не менее 150not less than 150 не менее 150not less than 150 не менее 150not less than 150

В составе чугуна компоненты проявляют себя следующим образом. Хром стабилизирует карбиды, способствует повышению твердости чугуна, препятствует росту окалины. Гафний, молибден и никель улучшают металлическую основу сплава, препятствуют возникновению и развитию трещин при перепадах температур. Кальций и барий выполняют функцию раскислителей. Медь и бор способствуют равномерному прогреву чугунных изделий, что также предупреждает возникновение трещин.In the composition of cast iron, the components manifest themselves as follows. Chromium stabilizes carbides, increases the hardness of cast iron, and prevents the growth of scale. Hafnium, molybdenum and nickel improve the metal base of the alloy, prevent the occurrence and development of cracks at temperature extremes. Calcium and barium act as deoxidizers. Copper and boron contribute to uniform heating of cast iron products, which also prevents the occurrence of cracks.

Чугун выплавляют в вагранках и отливают в песчаные формы. Температура расплава при заливке литейных форм должна быть не ниже 1330°C. Отливки подвергают отжигу при температуре 720-740°C с последующим охлаждением на воздухе.Cast iron is smelted in cupola furnaces and cast in sand forms. The melt temperature when casting molds should not be lower than 1330 ° C. The castings are annealed at a temperature of 720-740 ° C, followed by cooling in air.

Источник информацииThe source of information

1. Заявка №60-121254 Японии, 1985.1. Application No. 60-121254 of Japan, 1985.

Claims (1)

Чугун, содержащий углерод, кремний, марганец, хром, барий, молибден, никель, кальций, железо, отличающийся тем, что он дополнительно содержит медь, бор, гафний при следующем соотношении компонентов, мас.%:
углерод 2,0-2,8 кремний 0,8-1,2 марганец 0,8-1,2 хром 0,1-0,2 барий 0,001-0,002 молибден 1,5-1,9 никель 4,0-4,5 кальций 0,001-0,002 медь 0,3-0,7 бор 0,1-0,15 гафний 0,2-0,3 железо остальное
Cast iron containing carbon, silicon, manganese, chromium, barium, molybdenum, nickel, calcium, iron, characterized in that it additionally contains copper, boron, hafnium in the following ratio, wt.%:
carbon 2.0-2.8 silicon 0.8-1.2 manganese 0.8-1.2 chromium 0.1-0.2 barium 0.001-0.002 molybdenum 1.5-1.9 nickel 4.0-4.5 calcium 0.001-0.002 copper 0.3-0.7 boron 0.1-0.15 hafnium 0.2-0.3 iron rest
RU2011115307/02A 2011-04-18 2011-04-18 Cast iron RU2445392C1 (en)