[go: up one dir, main page]

KR940004380B1 - 탄성모르타르 도막방수재의 제조방법 - Google Patents

탄성모르타르 도막방수재의 제조방법 Download PDF

Info

Publication number
KR940004380B1
KR940004380B1 KR1019910018217A KR910018217A KR940004380B1 KR 940004380 B1 KR940004380 B1 KR 940004380B1 KR 1019910018217 A KR1019910018217 A KR 1019910018217A KR 910018217 A KR910018217 A KR 910018217A KR 940004380 B1 KR940004380 B1 KR 940004380B1
Authority
KR
South Korea
Prior art keywords
weight
vinyl acetate
parts
ethylene vinyl
acetate copolymer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
KR1019910018217A
Other languages
English (en)
Other versions
KR930007852A (ko
Inventor
유중근
Original Assignee
김춘자
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김춘자 filed Critical 김춘자
Priority to KR1019910018217A priority Critical patent/KR940004380B1/ko
Publication of KR930007852A publication Critical patent/KR930007852A/ko
Application granted granted Critical
Publication of KR940004380B1 publication Critical patent/KR940004380B1/ko
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

내용 없음.

Description

탄성모르타르 도막방수재의 제조방법
본 발명은 에틸렌 초산비닐수지 공중합체에 계면활성제를 혼합한 후 금속염인 칼슘스테아레이트를 첨가하여 제조한 균일하고 일정한 반응경화성 에멀젼을 주성분으로 하고 경화제로는 포틀랜트 시멘트를 사용하여 얻어지는 신규한 도막방수제의 제조방법에 관한 것이다.
본 발명의 제조방법에 의하여 얻어진 도막방수재는 에틸렌 초산비닐 공중합체가 가지는 우수한 내후성, 내균열성, 강도, 신장율외에 칼슘 스테아레이트가 갖는 특유의 발수성능을 더하여 옥상이나 벽면등 햇빛에 직접 노출이 되어도 보호모르타르 없이 도막방수와 보행용 바닥재의 목적을 동시에 달성할 수 있을 뿐만 아니라 값이 저렴한 일반 시멘트를 사용하여 강제경화시키므로 경화시간의 단축과 실내 및 지하실에서도 사용할 수 있는 도막방수재이다.
이를 보다 상세히 설명하면 다음과 같다.
물 35-55중량부를 40-50℃로 가열하여 여기에 비이온 계면활성제를 5-10중량부를 넣고 30분간 잘 교반하여 완전히 용해시킨다음 칼슘스테아레이트 40-60중량부를 넣고 고루분산시켜 칼슘스테아레이트 분산액을 만든다. 여기에 비닐아세테이트기가 103-129정도인 에틸렌 초산비닐수지 공중합체 180-200중량부를 넣고 20-30℃의 온도를 유지하며 분산시킨다. 이렇게해서 얻어진 에멀젼 67-77중량%에 경화제로서 포틀랜트시멘트를 33-23중량%의 비율로 혼합 교반함으로써 내후성, 내균열성, 강도 및 경도가 높은 도막방수재를 얻을 수 있다. 이때 에멀젼과 경화제의 합계는 100중량%이다. 이와 같이 제조된 도막방수재는 반응경화형이므로 강제 경화시 경화시간이 촉진되어 시공기간이 단축될 수 있다.
본 발명의 제조방법에서 사용되는 에틸렌 초산비닐수지 공중합체는 그 공중합체내 비닐아세테이트기의 수가 103-129의 범위내의 것을 다양하게 사용할 수 있으나 그 이상이면 비닐아세테이트기가 너무 조밀해서 칼슘 스테아레이트의 칼슘이 수지에 결합되기 어려워 고른 유화분산이 어렵고 그 이하가 되면 에틸렌 초산비닐수지 공중합체의 분자구조가 느슨해 강도 및 경도가 떨어지게 된다.
비이온 계면활성제로는 폴리옥시에틸렌 모노라우레이트, 폴리옥시에틸렌 스테아릴에테르, 폴리옥시에틸렌 라우릴에테르, 폴리옥시에틸렌 모노올레이트, 폴리옥시에틸렌 모노스테아레이트 등을 사용할 수 있으나 본 발명에서는 폴리옥시에틸렌 스테아릴에테르가 바람직하다.
지방산 금속염인 칼슘스테아레이트는 알루미늄 스테아레이트와 대체가 가능하지만 시멘트와 분산성이 더 좋은 칼슘스테아레이트가 더욱 유용하다.
본 발명에 사용되는 시멘트는 일반적으로 많이 사용하는 포틀랜트시멘트를 사용한다.
본 발명을 실시예를 들어 더욱 구체적으로 설명하면 다음과 같다.
[실시예]
깨끗한 물 45중량부를 40℃로 가열하여 비이온 계면활성제인 폴리옥시에틸렌 스테아릴에테르 5중량부를 넣고 30분정도 교반시켜 잘 녹인다. 여기에 칼슘 스테아레이트 분말 50중량부를 비교적 빠른 속도로 교반시켜 유화분산액을 만든다. 그후 에틸렌 초산비닐수지 공중합체 200중량부를 넣고 서서히 교반시켜 잘 혼합한다. 이렇게 해서 만들어진 에멀젼을 주성분으로 하고 여기에 포틀랜트 시멘트를 경화제로 하여 주성분과 경화제의 혼합비를 70 : 30의 중량비로 균일하게 배합하여 소기의 탄성모르타르 도막방수재를 얻었다. 이와 같이 제조한 제품을 깨끗한 유리판 위에 도포하고 시편을 제작하였고, 또한 시판중인 도막방수재로서 JGCOAT(상품명, 중앙방수기업주식회사제, 경도30)를 사용하여 동일하게 시편을 제작하고 이에 대한 물성을 측정하여 비교하면 다음의 표 1과 같은 결과를 얻을 수 있었다.
[표 1]

Claims (3)

  1. 물 35-55중량부를 40-50℃로 가열하고 비이온 계면활성제 5-10중량부와 금속염인 칼슘 스테아레이트 40-60중량부를 첨가하여 유화분산시키고 180-200중량부의 에틸렌 초산비닐수지 공중합체와 잘 혼합시켜 에멀젼을 얻고 이 에멀젼 67-77중량%에 경화제로서 포틀랜트 시멘트를 33-23중량%의 비율로 혼합시키는 것을 특징으로 하는 탄성모르타르 도막방수재의 제조방법.
  2. 제1항에 있어서, 비이온 계면활성제가 폴리옥시에틸렌 스테아릴에테르인 것을 특징으로 하는 제조방법.
  3. 제1항에 있어서, 에틸렌 초산비닐수지 공중합체가 그 공중합체내 비닐 아세테이트기의 수가 103-129인 에틸렌 초산비닐수지 공중합체인 것을 특징으로 하는 제조방법.
KR1019910018217A 1991-10-16 1991-10-16 탄성모르타르 도막방수재의 제조방법 Expired - Fee Related KR940004380B1 (ko)