KR930016062A - How to fuse (alloyed) gold sheets to silver cutlery - Google Patents
How to fuse (alloyed) gold sheets to silver cutlery Download PDFInfo
- Publication number
- KR930016062A KR930016062A KR1019920014838A KR920014838A KR930016062A KR 930016062 A KR930016062 A KR 930016062A KR 1019920014838 A KR1019920014838 A KR 1019920014838A KR 920014838 A KR920014838 A KR 920014838A KR 930016062 A KR930016062 A KR 930016062A
- Authority
- KR
- South Korea
- Prior art keywords
- silver
- gold
- cutlery
- alloyed
- sheet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
본 발명은 금장을 이용한 세공 기술에 관한 것으로서 좁게는 은수저에 금장을 융착시키는 방법이다.The present invention relates to a pore technique using gold, which is a method of fusing gold to a silver cutlery.
사용되는 금장의 두께가 0.05cm 0.001cm이므로 금장을 은수저 표면에 붕사와 땜은을 사용하여 융착시키는 것이 완벽하지 못하고, 따라서 융점이 높은 칠보(700℃-800℃)를 은수저 표면에 부착된 금장 표면에 입히는 것이 불가능 하며 작업의 능률이 저하된다.Since the thickness of the gold sheet used is 0.05cm 0.001cm, it is not perfect to fuse the gold sheet with borax and solder silver on the surface of the silver cutlery. Therefore, the high melting point cloisonne (700 ℃ -800 ℃) is attached to the surface of the silver cutlery. It is not possible to apply it, and the work efficiency is reduced.
본 발명은 이같은 결점을 해결하기 위하여 경도·강도가 높은 합금된 금장 이면에 은판을 가열 융착시키고 반복압연하여 금은장을 제작한 후 이것을 은수저에 붕사와 땜은을 사용하여 가열 융착시킨다. 이 상태에서 프레스금형으로 가압하여 입체무늬와 형상을 만든 후에 칠보를 입히는 방법이다.In order to solve the drawbacks of the present invention, a silver plate is heated and welded on a back surface of alloyed gold sheet having high hardness and strength, and repeatedly rolled to produce a gold silver sheet, which is then heat-bonded by using borax and solder silver on a silver cutlery. In this state, the pressing die is pressed to form a three-dimensional pattern and shape, and then cloisonne.
본 발명은 은수저의 장식에 사용될 뿐만 아니라 마모성이 현저히 증가된 합금된 금은장을 사용하여 각종 장식품과 악세사리 제품에 활용할 수 있다.The present invention can be used not only for decoration of silver cutlery, but also for various ornaments and accessories using alloyed gold and silver sheets with markedly increased wear.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음As this is a public information case, the full text was not included.
제1도의 (가)는 여러개의 합금된 금판의 이면에 은판을 융착한 상태의 사시도이고 (나)는 이것을 연신한 합금된 금은장의 예시도, 제2도의 (가)와 (나)는 합금된 금은장이 융착된 은수저 본체를 금형에 넣고 입체 무늬와 형상을 형성하는 과정과 완성된 은수저의 확대 단면도.(A) of FIG. 1 is a perspective view of a state where the silver plate is welded to the back surface of several alloyed gold plates, and (b) is an illustration of an alloyed gold and silver sheet drawn from this, and (a) and (b) of FIG. An enlarged cross-sectional view of the finished silver cutlery by placing a silver cutlery body fused with gold and silver sheets into a mold and forming a three-dimensional pattern and shape.
Claims (2)