KR101729428B1 - 협개선 가스 실드 아크 용접 방법 - Google Patents
협개선 가스 실드 아크 용접 방법 Download PDFInfo
- Publication number
- KR101729428B1 KR101729428B1 KR1020157016817A KR20157016817A KR101729428B1 KR 101729428 B1 KR101729428 B1 KR 101729428B1 KR 1020157016817 A KR1020157016817 A KR 1020157016817A KR 20157016817 A KR20157016817 A KR 20157016817A KR 101729428 B1 KR101729428 B1 KR 101729428B1
- Authority
- KR
- South Korea
- Prior art keywords
- welding
- improvement
- less
- gas
- angle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
도 2는 V형의 개선 형상에 있어서, 본 발명의 용접을 시공할 때의 시공 요령을 나타내는 도면이다.
도 3은 V형의 개선 형상에 있어서, 본 발명의 용접 방법에 의해 초층 용접을 실시한 후의 개선을 나타내는 도면이다.
도 4는 개선면의 최대 오목부 깊이를 설명하는 도면이다.
도 5는 본 발명의 발명예(No. 7)에 있어서, 본 발명의 용접 방법에 의해 초층 용접을 실시한 후의 개선 단면 사진을 나타내는 도면이다.
2:두꺼운 강재의 개선면
3:저부 개선
4:용접 토치의 급전 칩
5:용접 와이어
6:받침재
7:용접 비드
θ:저부 개선 각도
G:저부 개선 갭
h:저부 개선 높이
t:판 두께
φ:용접 토치 선단의 급전 칩으로부터 공급하는 용접 와이어의 공급 각도
d:저부 개선에 있어서의 용접 와이어의 선단의 측단부와 두꺼운 강재의 개선면의 거리
P:두꺼운 강재의 저부에 있어서의 용융 깊이
H:평균 용접물 높이
Claims (9)
- 저부 개선 각도를 10°이하, 저부 개선 갭을 7㎜이상 15㎜이하로 하고, 판 두께가 22㎜이상인 두꺼운 강재를 협개선의 다층 용접에 의해 접합하는 가스 실드 아크 용접 방법에 있어서,
초층 용접을 2패스 이상으로 해서 각 패스를 저부 개선 갭의 양측에 배분하고, 또한 용접 토치 선단의 급전 칩으로부터 공급하는 용접 와이어의 공급 각도를 상기 급전 칩 선단의 기울기에 의해서, 수선에 대해 5°이상 15°이하의 범위로 제어하는 동시에, 상기 용접 와이어로서, 곡률 반경이 150mm이상 300mm이하로 되는 범위에서 만곡시킨 와이어를 이용하는 것에 의해, 상기 두꺼운 강재의 저부에 있어서의 용융 깊이를 1.5㎜이상으로 하는 것을 특징으로 하는 협개선 가스 실드 아크 용접 방법. - 제 1 항에 있어서,
상기 초층 용접에 있어서, 저부 개선에 있어서의 용접 와이어의 선단의 측단부와 상기 두꺼운 강재의 개선면의 거리를 0.5㎜이상 2.0㎜이하로 하는 것을 특징으로 하는 협개선 가스 실드 아크 용접 방법. - 제 1 항 또는 제 2항에 있어서,
상기 초층 용접에 있어서, 용접물 높이를 상기 저부 개선 갭의 0.4배 이상 1.0배 이하로 하는 것을 특징으로 하는 협개선 가스 실드 아크 용접 방법. - 제 1 항 또는 제 2 항에 있어서,
상기 협개선 가스 실드 아크 용접에 있어서의 실드 가스로서 60체적%이상의 CO2 가스를 함유한 혼합 가스를 이용하는 것을 특징으로 하는 협개선 가스 실드 아크 용접 방법. - 제 3 항에 있어서,
상기 협개선 가스 실드 아크 용접에 있어서의 실드 가스로서 60체적%이상의 CO2 가스를 함유한 혼합 가스를 이용하는 것을 특징으로 하는 협개선 가스 실드 아크 용접 방법. - 삭제
- 삭제
- 삭제
- 삭제