[go: up one dir, main page]

KR101497228B1 - Sealant preferred filling waterproofing method of prefabricated structure joint - Google Patents

Sealant preferred filling waterproofing method of prefabricated structure joint Download PDF

Info

Publication number
KR101497228B1
KR101497228B1 KR20130095911A KR20130095911A KR101497228B1 KR 101497228 B1 KR101497228 B1 KR 101497228B1 KR 20130095911 A KR20130095911 A KR 20130095911A KR 20130095911 A KR20130095911 A KR 20130095911A KR 101497228 B1 KR101497228 B1 KR 101497228B1
Authority
KR
South Korea
Prior art keywords
sealant
primer
prefabricated structure
joint
steel wire
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
KR20130095911A
Other languages
Korean (ko)
Other versions
KR20150019270A (en
Inventor
임인혁
Original Assignee
임인혁
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 임인혁 filed Critical 임인혁
Priority to KR20130095911A priority Critical patent/KR101497228B1/en
Publication of KR20150019270A publication Critical patent/KR20150019270A/en
Application granted granted Critical
Publication of KR101497228B1 publication Critical patent/KR101497228B1/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

본 발명은 조립식 구조물의 접합면에 프라이머를 선도포하고, 지수재를 부착시킨 후 실란트를 밀실되게 충진 경화시켜서 접합면 사이에 분리의 힘이 발생되더라도 실란트가 신축적으로 대응하여 방수 조인트가 유지되도록 한 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법을 제공한다.
본 발명의 적절한 실시 형태에 따르면, 조립식 구조물이 접합될 각 접합면의 양면에 각기 프라이머를 도포하는 단계와; 프라이머가 도포된 한 면에 지수재를 2열로 나란하게 부착하는 단계와; 2열 지수재의 사이에 실란트를 우선적으로 충진하는 단계와; 조립식 구조물을 강선의 인장 또는 볼트 조임시켜 실란트가 2열 지수재의 사이에 압밀되도록 하는 단계를 포함하여, 충진 된 실란트가 경화되도록 한 후 구조물의 접합면 사이에 지수재가 1차로 물 유입을 차단하고, 2차로 실란트가 물 유입을 차단하는 것을 특징으로 한다.
In the present invention, the primer is firstly attached to the joint surface of the prefabricated structure, the expansive material is adhered, and the sealant is filled and cured so that the waterproof joint is maintained even if the separation force is generated between the joint surfaces, A method of sealing a sealant line leak in a prefabricated structure connection is provided.
According to a preferred embodiment of the present invention, the prefabricated structure is provided with a primer on each side of each joint surface to be joined; Attaching the index material in two rows side by side on one side to which the primer is applied; A step of preferentially filling the sealant between the two row thermo exponent materials; Comprising the step of tensioning or bolting the prefabricated structure to allow the sealant to consolidate between the second row index material so that the filled sealant is allowed to cure and then the index material firstly blocks water ingress between the joining surfaces of the structure, And the second sealant blocks the inflow of water.

Description

조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법{Sealant preferred filling waterproofing method of prefabricated structure joint}{Sealant preferred filling waterproofing method of prefabricated structure joint}

본 발명은 조립식 구조물 접합부의 누수 차단 방법에 관한 것으로, 특히 접합면에 프라이머를 우선적으로 도포하고, 지수재를 부착시킨 후 실란트틀 밀실되게 충진 경화시켜서 방수 조인트를 갖도록 한 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법에 관한 것이다.The present invention relates to a leakage-blocking method for a joint of a prefabricated structure. More particularly, the present invention relates to a method of sealing a joint of a prefabricated structure, in which a primer is first applied to a joint surface, an exponent is applied, and a sealant is sealed- And to a leakage water blocking method.

일반적으로 조립식 콘크리트 구조물을 조립할 경우 흔히 부재와 부재 사이에 코킹을 하거나, 무수축 몰탈을 주입하거나, 2열의 지수재 사이로 실란트를 고압으로 주입하여 누수를 차단하는 방법 등이 있다.Generally, when a prefabricated concrete structure is assembled, there is a method of caulking between a member and a member, injecting no shrinkage mortar, or injecting a sealant at high pressure between two rows of exposures to block leakage.

코킹은 일반적으로 시공하는 방법이지만 외부에 노출되어 있어, 파손 염려 및 내구성에 지장을 초래할 수 있고, 무수축 몰탈 주입 방법은 신, 구 콘크리트의 접착에 의하여 접착이 완전히 되지 않고, 분리되는 현상이 나타나는 문제가 있다. 또한 지수재를 2열로 붙이고 2열 지수재 내측으로 실란트를 고압으로 주입하여 누수를 차단하는 방법이 있으나, 이 방법은 부재와 부재의 접합면이 평편할 경우 효과가 있으나 전단키 등 부재의 면이 평평하지 않고 굴곡이 있을 경우는 2열 지수재가 각각의 부재에 밀착되지 않아 틈새로 실란트가 누출되어 지수재 사이에 실란트가 밀실하게 채워지지 않는 경우가 발생되어 완벽한 방수 조인트를 구현하기 어렵다.The caulking is generally a method of construction, but it is exposed to the outside, which may cause damage to the damage and durability. In the shrink-proof mortar injection method, the adhesion of the new and old concrete is not completely completed, there is a problem. In addition, there is a method of sealing the leakage by inserting the exponent into two rows and injecting the sealant into the inside of the double row exponential at high pressure. However, this method is effective when the joining surface of the member and the member is flat, If there is a curvature, the two-row exponential material does not come in close contact with the respective members. As a result, the sealant leaks through the gap and the sealant is not filled tightly between the exponents.

본 발명의 배경이 되는 기술로는 한국 등록특허 등록번호 제10-0776242호로서, 콘크리트 패널과 콘크리트 패널용 방수기구 및 콘크리트패널의 조인트 방수방법이 있다. 이는 세그먼트로 이루어진 서로 다른 콘크리트 패널의 접합면을 방수처리하는 콘크리트 패널용 방수기구에 있어서, 상기 서로 다른 콘크리트 패널의 접합면이 서로 맞닿을 때, 접합면으로부터 인접한 외측에 형성된 단턱에 의해 형성되는 고정홈에 삽입되는 수팽창 지수재와; 상기 수팽창 지수재의 내부에 삽입고정되는 제2고정편과; 상기 수팽창 지수재에 형성된 다수개의 제2통공과 제2고정편에 형성된 다수개의 제3통공으로 관통되어 콘크리트 패널이 서로 맞닿는 접합면 사이로 관통체결되는 앵커볼트를 포함하는 것을 특징으로 한다.As a background of the present invention, Korean Patent Registration No. 10-0776242 discloses a waterproofing device for concrete panels and concrete panels, and a joint waterproofing method for concrete panels. The waterproofing device for waterproofing the joint surfaces of different concrete panels made of segments is characterized in that when the joint surfaces of the different concrete panels are brought into contact with each other, A water expansion index material inserted into the groove; A second fixing piece inserted and fixed in the water swell index material; And an anchor bolt penetrating through the plurality of second through holes formed in the water expansition index material and the plurality of third through holes formed in the second fixing piece and passing through the joint surfaces where the concrete panels are in contact with each other.

상기 배경기술에서는 접합면으로 물이 침투하려 할 때, 물이 수팽창 지수재와 반응하게 되어 수팽창 지수재의 용적이 팽창함에 따라 고정홈에 수팽창 지수재가 더욱 밀착됨으로써 누수를 방지한다. 그러나 상기 배경기술에서 부재간의 물리적인 분리의 힘에 의해 접합면의 이격이 발생될 경우 수팽창 지수재만으로는 누수를 차단할 수 없는 문제가 있다.In the background art, when water tends to penetrate into the joint surface, the water reacts with the water expansion index material, and as the volume of the water expansion index material expands, the water expansion index material is further adhered to the fixing groove, thereby preventing water leakage. However, in the background art, there is a problem in that when the separation surface is separated due to the force of physical separation between members, leakage of water can not be blocked by only the water expansion index material.

한국 등록특허 등록번호 제10-0309316호(조립식 박스 암거의 2중 방수 방법)Korean Registered Patent No. 10-0309316 (Dual waterproofing method for prefabricated box culvert) 한국 공개특허 공개번호 제10-2013-0024650호(콘크리트 구조물용 방수장치)Korean Patent Laid-Open Publication No. 10-2013-0024650 (Waterproofing device for concrete structures) 한국 등록실용 등록번호 제20-0292646호(콘크리트 구조물 연결용 지수 구조)Korean Registered Practical Registration No. 20-0292646 (Index Structure for Concrete Structure Connection)

본 발명은 조립식 구조물의 접합면에 프라이머를 선도포하고, 지수재를 부착시킨 후 실란트를 밀실되게 충진 경화시켜서 접합면 사이에 분리의 힘이 발생되더라도 실란트가 신축적으로 대응하여 방수 조인트가 유지되도록 한 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법을 제공함에 그 목적이 있다. In the present invention, the primer is firstly attached to the joint surface of the prefabricated structure, the expansive material is adhered, and the sealant is filled and cured so that the waterproof joint is maintained even if the separation force is generated between the joint surfaces, The present invention provides a sealant line leakproofing method for a joint of a prefabricated structure.

또한, 본 발명은 조립식 구조물의 접합면에 강제적인 압축력이 작용되도록 하여 지수재의 지수력이 향상되도록 한 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법을 제공함에 그 목적이 있다It is another object of the present invention to provide a sealant line leakage preventing method for a joint of a prefabricated structure in which an urging force is applied to a joint surface of a prefabricated structure,

본 발명의 적절한 실시 형태에 따르면,According to a preferred embodiment of the present invention,

조립식 구조물이 접합될 각 접합면의 양면에 각기 프라이머를 도포하는 단계와;Applying a primer to both sides of each joint surface to which the prefabricated structure is to be joined;

프라이머가 도포된 한 면에 지수재를 2열로 나란하게 부착하는 단계와;Attaching the index material in two rows side by side on one side to which the primer is applied;

2열 지수재의 사이에 실란트를 우선적으로 충진하는 단계와;A step of preferentially filling the sealant between the two row thermo exponent materials;

조립식 구조물을 강선의 인장 또는 볼트 조임시켜 실란트가 2열 지수재의 사이에 압밀되도록 하는 단계를 포함하여,Tightening the prefabricated structure by tensioning or bolting the steel wire so that the sealant is consolidated between the two-

충진된 실란트가 경화되도록 한 후 구조물의 접합면 사이에 지수재가 1차로 물 유입을 차단하고, 2차로 실란트가 물 유입을 차단하는 것을 특징으로 한다.After the filled sealant is allowed to cure, the exponent material interrupts the water inflow primarily between the joint surfaces of the structure and the second sealant blocks the inflow of water.

또한, 조립식 구조물의 양쪽 접합면에 테이퍼를 가지고 일정 폭과 깊이로 함몰되어 있는 실란트 충진홈이 각기 형성되고, 각 실란트 충진홈에 상기 프라이머가 도포되는 것을 특징으로 한다.In addition, a sealant filling groove having a taper and a predetermined width and depth is formed on both bonding surfaces of the prefabricated structure, and the primer is applied to each sealant filling groove.

또한, 강선 또는 볼트는 실란트 충진홈에 연통되어 있는 조립용 강선홀을 통해 설치되어 강선의 인장 또는 볼트 조임 시 실란트의 일부가 조립용 강선홀로 침입되는 것을 특징으로 한다.Further, the steel wire or bolt is installed through a steel wire hole for assembly, which is communicated with the sealant fill groove, so that a part of the sealant penetrates into the steel wire hole for assembly when the steel wire is tensioned or bolted.

본 발명에 따른 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법에 의하면, 구조물의 접합면 사이에 물이 침투하게 되면, 지수재가 1차로 물 유입을 차단하고, 2차로 실란트가 물 유입을 효과적으로 차단하게 된다. 이때 조립식 구조물의 접합면과 지수재의 사이에는 프라이머층이 형성되어 있고 강선 또는 볼트의 장력으로 실란트에 압축력이 도입되어 실란트의 접합이 밀착되므로 물의 침입이 효과적으로 차단된다.According to the sealing method of sealing the sealant line filling structure according to the present invention, when the water penetrates between the joint surfaces of the structure, the exponent material firstly blocks water inflow and the second sealant effectively blocks the inflow of water . At this time, a primer layer is formed between the joint surface of the prefabricated structure and the exponent material, and the penetration of water is effectively blocked because the sealing force of the sealant is tightened by the compressive force introduced into the sealant by the tension of the steel wire or bolt.

또한, 조립식 구조물 간에 분리되는 힘이 발현되더라도, 실란트가 프라이머층을 통해 조립식 구조물의 접합면에 견고히 부착된 실란트가 자체의 신축력으로 늘어나며 저항하므로 누수를 효과적으로 방지하게 된다.In addition, even if a force separating the prefabricated structures is developed, the sealant, which is firmly attached to the joint surface of the prefabricated structure through the primer layer, stretches and resists due to its own stretching force, thereby effectively preventing leakage.

따라서 지하구조물(지하주차장, 저류조)의 외벽 시공, 박스(BOX) 시공 등 누수 방지를 필요로 하는 조립식 구조물의 접합부 조인트 방수 시공에 폭 넓게 이용될 수 있다.Therefore, it can be widely used for waterproofing joints of joints of prefabricated structures requiring leakage prevention such as outer wall construction of underground structures (underground parking lot, reservoir) and box construction.

본 명세서에서 첨부되는 다음의 도면들은 본 발명의 바람직한 실시 예를 예시하는 것이며, 발명의 상세한 설명과 함께 본 발명의 기술사상을 더욱 이해시키는 역할을 하는 것이므로, 본 발명은 첨부한 도면에 기재된 사항에만 한정되어서 해석되어서는 아니 된다.
도 1 및 도 2는 본 발명의 실시 예에 따른 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법을 설명하는 시공 순서도.
도 3은 강선 또는 볼트를 이용하여 조립식 구조물의 접합부에 압축력이 도입된 상태를 나타내는 단면도.
도 4는 도 3의 부분을 부분 절단된 사시도로 나타낸 도면.
BRIEF DESCRIPTION OF THE DRAWINGS The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate exemplary embodiments of the invention and, together with the description, serve to explain the principles of the invention, Shall not be construed as limiting.
BRIEF DESCRIPTION OF THE DRAWINGS FIG. 1 and FIG. 2 are installation sequence diagrams illustrating a method for sealing sealant line leakage of a prefabricated structure joint according to an embodiment of the present invention. FIG.
3 is a cross-sectional view showing a state where a compressive force is introduced into a joint portion of the prefabricated structure using a steel wire or a bolt.
Figure 4 is a partially cut away perspective view of the portion of Figure 3;

아래에서 본 발명은 첨부된 도면에 제시된 실시 예를 참조하여 상세하게 설명이 되지만 제시된 실시 예는 본 발명의 명확한 이해를 위한 예시적인 것으로 본 발명은 이에 제한되지 않는다. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will be described in detail below with reference to the embodiments shown in the accompanying drawings, but the present invention is not limited thereto.

먼저, 도 1(가)와 같이 조립식 구조물(10,10)이 접합될 각 접합면(101)의 양면에 프라이머(12)가 각기 도포된다. 프라이머(12)는 이 분야에서 공지된 임의의 재료가 사용될 수 있으며, 예를 들어 에폭시 수지 등 고분자 수지가 사용될 수 있다. 프라이머(12)는 1회 또는 그 이상의 도포로 형성되어 후술할 실란트(16)와의 부착력을 향상시킨다. 프라이머(12)는 조립식 구조물(10,10)의 양쪽 접합면에 테이퍼를 가지고 일정 폭(w)과 깊이(h)로 함몰되어 있는 실란트 충진홈(102)에 도포된다. 프라이머(12)의 도포 두께는 접합면의 표면 조도에 따라 차이를 갖지만 예로 100㎛~0.5mm가 될 수 있다.First, as shown in Fig. 1 (A), primers 12 are applied to both surfaces of each bonding surface 101 to which the prefabricated structures 10 and 10 are to be bonded, respectively. As the primer 12, any material known in this field can be used, and for example, a polymer resin such as an epoxy resin can be used. The primer 12 is formed by one or more coatings to improve adhesion with the sealant 16, which will be described later. The primer 12 is applied to the sealant filling grooves 102 having tapered surfaces at both sides of the prefabricated structures 10 and 10 and recessed at a certain width w and depth h. The coating thickness of the primer 12 varies depending on the surface roughness of the bonding surface, but may be, for example, 100 탆 to 0.5 mm.

다음, 도 1(나)와 같이 프라이머(12)가 도포된 한 면에 지수재(14)를 2열로 나란하게 부착시킨다. 이때 지수재(14)는 프라이머(12)의 접착력에 의해 실란트 충진홈(102)의 상부 모서리에 접착된 상태로 부착 위치를 유지한다. 지수재(14)는 수팽창 고무 지수재 등 이 분야에서 공지된 임의의 재료가 사용될 수 있다. 지수재(14)는 본 실시 예에서 단면이 원형으로 구성되어 있으나 이러한 단면 형상에 한정되는 것은 아니다.Next, as shown in FIG. 1 (B), the exponent material 14 is adhered in two rows side by side on one surface coated with the primer 12. At this time, the exponent 14 maintains the attachment position in a state of being adhered to the upper edge of the sealant filling groove 102 by the adhesive force of the primer 12. The index material 14 may be any material known in the art such as a water-swellable rubber index material. The exponent material 14 is circular in cross section in the present embodiment, but is not limited to this cross-sectional shape.

그 다음, 도 1(다)와 같이 2열 지수재(14와 14)의 사이에 실란트(16)를 충진한다. 실란트(16)는 기밀, 수밀의 기능 외에 부재 상호간의 신축, 진동, 변형을 흡수 완화하기 위한 것으로 고무상의 물질 또는 연질 혹은 액상 고무 조성물로 구성된다, 실란트(16)는 예를 들어 실리콘계, 변성 실리콘계, 폴리 설파이드계, 폴리 우레탄계 등이 될 수 있다. 이때 실란트(16)는 실란트 충진홈(102)을 포함하여 2열 지수재(14와 14)의 사이의 공간에 외부로 새어나가지 않고 밀실하게 충진된다.Then, the sealant 16 is filled between the two-column exponents 14 and 14 as shown in Fig. 1 (C). The sealant 16 is composed of a rubber-like substance or a soft or liquid rubber composition for absorbing relaxation, vibration, and deformation of members relative to each other in addition to functions of airtightness and watertightness. The sealant 16 is, for example, , Polysulfide type, polyurethane type, and the like. At this time, the sealant 16 including the sealant filling grooves 102 is filled tightly without leaking out to the space between the two-row exponential materials 14 and 14.

그 다음, 도 2(라)와 같이 조립식 구조물(10,10)을 접합시켜 일정한 시간을 두고 실란트(16)를 경화시킨다.Then, the prefabricated structures 10 and 10 are bonded together as shown in FIG. 2 (D), and the sealant 16 is cured for a predetermined time.

이후, 실란트(16)가 2열 지수재(14와 14) 사이에 압밀되도록 도 3과 같이 조립식 구조물(10,10)의 접합면을 강선(20)의 인장을 통해 밀착시킬 수 있다. 예로, 강선(20)은 실란트 충진홈(102)에 연통되어 있는 조립용 강선홀(104)을 통해 설치될 수 있다. 이 경우 강선(20)의 인장시 실란트(16)의 일부가 조립용 강선홀(104)로 침입하게 되고, 이로 인해 강선(20)의 부식을 방지할 수 있는 부가적인 이점을 갖게 된다. 강선(20)의 인장은 양단에 주지의 웨지 및 그 정착장치를 통해 이루어질 수 있다. 즉, 강선(20)을 유압잭으로 긴장시킨 후 웨지를 정착장치에 고정시켜서 인장을 발휘할 수 있다.3, the joint surfaces of the prefabricated structures 10 and 10 can be brought into close contact with each other through the tensile force of the steel wire 20 so that the sealant 16 is consolidated between the two-column index materials 14 and 14. For example, the steel wire 20 can be installed through the steel wire hole for assembly 104 communicated with the sealant filling groove 102. In this case, when the steel wire 20 is pulled, a part of the sealant 16 penetrates into the steel wire hole for assembly 104, thereby providing an additional advantage of preventing corrosion of the steel wire 20. The tension of the steel wire 20 can be made at both ends through a known wedge and its fixing device. That is, after the steel wire 20 is tensioned by the hydraulic jack, the wedge can be fixed to the fixing device to exert tension.

여기서, 강선(20)에 대체하여 볼트의 조임을 통해 실란트(16)가 2열 지수재(14와 14) 사이에 압밀되도록 할 수도 있다. 볼트의 조임은 양단 또는 일단에 나사 체결되는 너트를 조여서 발생시킬 수 있다.Here, the sealant 16 may be consolidated between the two-row index members 14 and 14 by fastening the bolts in place of the steel bar 20. Tightening of the bolt can be generated by tightening a nut screwed on both ends or one end.

이와 같이 본 발명에 따른 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법에 의하면, 도 2의 (마)와 같이 구조물(10)(10)의 접합면 사이에 물(W)이 침투하게 되면, 지수재(14)가 1차로 물 유입을 차단하고, 2차로 실란트(16)가 물 유입을 차단하게 된다.According to the sealing method of sealing the prefabricated structures according to the present invention, when the water W penetrates between the joint surfaces of the structures 10 and 10 as shown in FIG. 2 (e) The first sealant 14 blocks the inflow of water and the second sealant 16 blocks the inflow of water.

이때 조립식 구조물(10)의 접합면(101)과 지수재(14)의 사이에는 프라이머(12)층이 형성되어 있어 실란트(16)의 접합이 밀착되므로 실린트층으로 물의 침입이 효과적으로 차단된다.At this time, a layer of primer 12 is formed between the joint surface 101 of the prefabricated structure 10 and the exponent material 14, so that the adhesion of the sealant 16 is intimately contacted, so that the invasion of water into the silt layer is effectively blocked.

또한, 강선(20)의 인장이나 볼트 조임으로 지수재(14) 및 실란트(16)를 강제적으로 압착시켜 누수를 방지한다.Further, the expelling material 14 and the sealant 16 are forcedly pressed by tensile or bolt tightening of the steel wire 20 to prevent water leakage.

또한, 조립식 구조물(10)(10)간에 분리되는 힘이 발현되더라도, 실란트(16)가 프라이머(12)층을 통해 각각의 조립식 구조물(10)(10)의 접합면에 견고히 부착된 상태에서 그 자체의 신축력으로 늘어나며 저항하면서 누수를 효과적으로 방지하게 된다.The sealant 16 is firmly attached to the joint surface of each of the prefabricated structures 10 and 10 via the primer layer 12 even when a force for separating the prefabricated structures 10 and 10 is developed. It is stretched by its own stretching force and effectively prevents leakage by resistance.

따라서 지하주차장, 저류조 등의 지하구조물의 외벽 시공이나, 박스(BOX) 시공 등 누수 방지를 필요로 하는 조립식 구조물의 접합부 조인트 방수 시공에 폭 넓게 이용될 수 있다.Therefore, it can be widely used for splice joint waterproofing construction of a prefabricated structure requiring prevention of leakage such as construction of an outer wall of an underground structure such as an underground parking lot, a storage tank, and construction of a box (BOX).

지금까지 본 발명은 제시된 실시 예를 참조하여 상세하게 설명이 되었지만 이 분야에서 통상의 지식을 가진 자는 제시된 실시 예를 참조하여 본 발명의 기술적 사상을 벗어나지 않는 범위에서 다양한 변형 및 수정 발명을 만들 수 있을 것이다. 본 발명은 이와 같은 변형 및 수정 발명에 의하여 제한되지 않으며 다만 아래에 첨부된 청구범위에 의하여 제한된다. While the present invention has been particularly shown and described with reference to exemplary embodiments thereof, it is evident that many alternatives, modifications and variations will be apparent to those skilled in the art in light of the above teachings. will be. The invention is not limited by these variations and modifications, but is limited only by the claims appended hereto.

10: 조립식 구조물
102: 실란트 충진홈
12: 프라이머
14: 지수재
16: 실란트
20: 강선 또는 볼트
10: Prefabricated structure
102: sealant filled groove
12: Primer
14: Index material
16: sealant
20: Steel wire or bolt

Claims (3)

조립식 구조물(10,10)이 접합될 각 접합면(101)의 양면에 각기 프라이머(12)를 도포하는 단계와;
프라이머(12)가 도포된 한 면에 지수재(14)를 2열로 나란하게 부착하는 단계와;
2열 지수재(14와 14)의 사이에 실란트(16)를 우선적으로 충진하는 단계와;
조립식 구조물(10,10)을 강선(20)의 인장 또는 볼트 조임시켜 실란트(16)가 2열 지수재(14와 14)의 사이에 압밀되도록 하되, 강선(20) 또는 볼트는 실란트 충진홈(102)에 연통되어 있는 조립용 강선홀(104)을 통해 설치되어 강선(20)의 인장 또는 볼트 조임시 실란트(16)의 일부가 조립용 강선홀(104)로 침입되도록 하는 단계를 포함하여,
충진된 실란트(16)가 경화되도록 한 후 구조물의 접합면 사이에 지수재(14)가 1차로 물 유입을 차단하고, 2차로 실란트(16)가 물 유입을 차단하는 것을 특징으로 하는 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법.
Applying primer (12) to both sides of each joint surface (101) to which the prefabricated structures (10, 10) are to be joined;
Attaching the exponent material (14) in two rows side by side on one side to which the primer (12) is applied;
Preferentially filling the sealant (16) between the two row thermo exponents (14 and 14);
The prefabricated structures 10 and 10 are tensioned or bolted to the steel wire 20 so that the sealant 16 is consolidated between the two row index materials 14 and 14 while the steel wire 20 or bolt is sealed in the sealant fill groove 102, and a part of the sealant 16 when the steel wire 20 is tensioned or bolted, into the steel wire hole 104 for assembly,
Characterized in that after the filled sealant (16) is cured, the exponent material (14) interrupts the first flow of water between the joining surfaces of the structure and the second sealant (16) Of sealant line leakage.
제1항에 있어서,
조립식 구조물(10,10)의 양쪽 접합면에 테이퍼를 가지고 일정 폭과 깊이로 함몰되어 있는 실란트 충진홈(102)이 각기 형성되고, 각 실란트 충진홈(102)에 상기 프라이머(12)가 도포되는 것을 특징으로 하는 조립식 구조물 접합부의 실란트 선 충진 누수 차단 방법.
The method according to claim 1,
Sealant filling grooves 102 each having a taper and having a predetermined width and depth are formed on both joint surfaces of the assembled structures 10 and 10 and the primer 12 is applied to each sealant filling groove 102 Wherein the sealant line is sealed with a sealant.
삭제delete
KR20130095911A 2013-08-13 2013-08-13 Sealant preferred filling waterproofing method of prefabricated structure joint Active KR101497228B1 (en)