JPS6411009A - Manufacture of seamless steel pipe - Google Patents
Manufacture of seamless steel pipeInfo
- Publication number
- JPS6411009A JPS6411009A JP62167101A JP16710187A JPS6411009A JP S6411009 A JPS6411009 A JP S6411009A JP 62167101 A JP62167101 A JP 62167101A JP 16710187 A JP16710187 A JP 16710187A JP S6411009 A JPS6411009 A JP S6411009A
- Authority
- JP
- Japan
- Prior art keywords
- rolling
- pipe end
- end part
- faulty
- thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To prevent faulty biting and to obtain a seamless steel pipe having a uniform thickness by rolling a thickness of pipe end part in a tapered shape on a rolling stage through a piercing mill or an elongator of Mannessmann type, then subjecting to elongation rolling and rolling the thickness of the pipe end part in a tapered shape. CONSTITUTION:In the stage of rolling the pipe end part in a tapered shape so that the thickness of the pipe end part becomes thinner toward the pipe end the rolling is performed without causing a faulty biting and a faulty shape of the pipe end. Furthermore, the blank pipe is elongation rolled by a succeeding plug mill and at the time of rolling the pipe end part in a tapered shape, a failing to roll caused by the faulty biting, etc., are not caused and the seamless steel pipe having uniform thickness is obtained in the last drawing roll mill.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP62167101A JPS6411009A (en) | 1987-07-06 | 1987-07-06 | Manufacture of seamless steel pipe |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP62167101A JPS6411009A (en) | 1987-07-06 | 1987-07-06 | Manufacture of seamless steel pipe |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS6411009A true JPS6411009A (en) | 1989-01-13 |
Family
ID=15843446
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP62167101A Pending JPS6411009A (en) | 1987-07-06 | 1987-07-06 | Manufacture of seamless steel pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6411009A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2012187625A (en) * | 2011-03-14 | 2012-10-04 | Sumitomo Metal Ind Ltd | Method of cold-rolling seamless tube |
WO2013153794A1 (en) * | 2012-04-12 | 2013-10-17 | 新日鐵住金株式会社 | Cold rolling method for seamless pipe |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5520764A (en) * | 1978-07-27 | 1980-02-14 | Ugine Kuhlmann | Method of obtaining highly pure 1*55dinitroo anthraquinone |
JPS59209414A (en) * | 1983-05-12 | 1984-11-28 | Kawasaki Steel Corp | Pipe end thinning rolling method |
JPS6116528A (en) * | 1985-06-14 | 1986-01-24 | Hitachi Ltd | Wafer cleaning equipment |
-
1987
- 1987-07-06 JP JP62167101A patent/JPS6411009A/en active Pending
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5520764A (en) * | 1978-07-27 | 1980-02-14 | Ugine Kuhlmann | Method of obtaining highly pure 1*55dinitroo anthraquinone |
JPS59209414A (en) * | 1983-05-12 | 1984-11-28 | Kawasaki Steel Corp | Pipe end thinning rolling method |
JPS6116528A (en) * | 1985-06-14 | 1986-01-24 | Hitachi Ltd | Wafer cleaning equipment |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2012187625A (en) * | 2011-03-14 | 2012-10-04 | Sumitomo Metal Ind Ltd | Method of cold-rolling seamless tube |
WO2013153794A1 (en) * | 2012-04-12 | 2013-10-17 | 新日鐵住金株式会社 | Cold rolling method for seamless pipe |
JP5408388B1 (en) * | 2012-04-12 | 2014-02-05 | 新日鐵住金株式会社 | Seamless pipe cold rolling method |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES2014170A6 (en) | Method and arrangement for reducing the outer diameter and wall thickness of an essentially cylindrical hollow rough-pierced tube blank by rolling. | |
JPS6415216A (en) | Grooving method for inner surface of metallic pipe | |
SU724078A3 (en) | Sleeve for making seamless tubes | |
FR2469962B1 (en) | ||
JPS6411009A (en) | Manufacture of seamless steel pipe | |
JPS6431505A (en) | Piercing method for seamless pipe | |
JPS57187114A (en) | Manufacture of square steel pipe | |
JPS6411008A (en) | Manufacture of seamless pipe | |
JPS5557301A (en) | Production of thick steel plate | |
JPS57103714A (en) | Manufacture of seamless steel pipe | |
GB1309132A (en) | Method and apparatus for forming thin metal belts | |
GB789155A (en) | Improvements in or relating to the stretching seamless metallic hollow bodies | |
JPS55114408A (en) | Mandrel circulating device of seamless metal pipe producing equipment | |
JPS5781908A (en) | Rolling method with inclined roll | |
JPS54110955A (en) | Edger rolling mill for shape steel rolling | |
IT1058140B (en) | Hot rolling ingots into tube with uniform wall thickness | |
ES2001141A6 (en) | Manufacture of tubes | |
SU498047A1 (en) | Method of rolling metal in planetary rollers | |
GB1291744A (en) | Method of manufacturing seamless steel pipes | |
SU592469A1 (en) | Cold pilgrim-step tube-rolling method | |
JPS6418510A (en) | Rolling method for tube by diagonal roll mill | |
Kummerling | Comparison of Various Cross-Rolling Processes for Elongation Stages in the Production of Seamless Tubes | |
JPS6466006A (en) | Method for rolling seamless steel pipe by cross helical rolling mill | |
JPS55112107A (en) | Rolling method for press roll piercing | |
JPS6427707A (en) | Manufacture of steamless steel tube for rim of wheel |