JPS55100896A - Flux for soldering - Google Patents
Flux for solderingInfo
- Publication number
- JPS55100896A JPS55100896A JP755279A JP755279A JPS55100896A JP S55100896 A JPS55100896 A JP S55100896A JP 755279 A JP755279 A JP 755279A JP 755279 A JP755279 A JP 755279A JP S55100896 A JPS55100896 A JP S55100896A
- Authority
- JP
- Japan
- Prior art keywords
- flux
- soldering
- plates
- urea
- granules
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To eliminate corrosion and permit safe handling by using urea in the form of powder or granules or as an aqueous solution to soldering flux for iron plates, copper plates, zinc plates, etc. CONSTITUTION:Urea is used alone in the form of powder or granules or as an aqueous solution of concentration 10% or more for flux for soldering of thin iron plates to themselves or thin copper plates to themselves. Since this flux is inexpensive and urea has no corrosiveness, there is no need for washing away the excess flux with water or warm water after soldering. Further the lack of any violet poison matter provides safety of handling.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP755279A JPS55100896A (en) | 1979-01-24 | 1979-01-24 | Flux for soldering |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP755279A JPS55100896A (en) | 1979-01-24 | 1979-01-24 | Flux for soldering |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS55100896A true JPS55100896A (en) | 1980-08-01 |
Family
ID=11668949
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP755279A Pending JPS55100896A (en) | 1979-01-24 | 1979-01-24 | Flux for soldering |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS55100896A (en) |
-
1979
- 1979-01-24 JP JP755279A patent/JPS55100896A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES504609A0 (en) | PROCEDURE FOR FORMING PHOSPHATE COATINGS | |
JPS5596455A (en) | Preserving agent for urine sample | |
JPS55100896A (en) | Flux for soldering | |
JPS5739177A (en) | Water soluble rust-resisting agent | |
JPS5461249A (en) | Preparation of low-viscosity aqueous polymer solution | |
JPS53136358A (en) | Draft device with shutters for preventing interference between treating liquid | |
JPS5289577A (en) | Electrodialysis of aqueous salt solution containing dissolved gypsum | |
GB970366A (en) | Improvements relating to the coating of metals | |
DE3377869D1 (en) | Corrosion inhibitors for aqueous solutions for the treatment of metals, and process for their preparation | |
JPS5567388A (en) | Manufacture of mineral water | |
JPS57185991A (en) | Corrosion inhibitor for stainless steel | |
JPS547197A (en) | Time limit element | |
JPS5723071A (en) | Anticorrosive for metal | |
JPS5561933A (en) | Deoxygenating composition | |
JPS53126760A (en) | Wastewater disposal method and device | |
JPS53141137A (en) | Method of inhibiting corrosion of metal coming into contact with aqueous calcium chloride solution | |
JPS53137886A (en) | Method of blocking metallic ion | |
JPS5224188A (en) | Treatment of aluminum-sludge including phosphorus | |
JPS56144744A (en) | Water absorbing agent | |
JPS57200221A (en) | Method for preventing hydrolysis of tin salt in acidic solution of tin salt | |
JPS5637089A (en) | Treating method for water | |
Sanyal | Corrosion of Mild Steel by Aqueous Sulphate Solution Inhibited by Nitrite.(Abstract Only) | |
Rudresh et al. | EFFECT OF ALIPHATIC AMINES ON THE CORROSION OF ZINC | |
JPS5244786A (en) | Treatment to increase oxidation resistance of carbonaceous materials | |
JPS5286974A (en) | Treatment of waste matter containing heavy metal |