JPS54152639A - Repair welding method for steel pipe - Google Patents
Repair welding method for steel pipeInfo
- Publication number
- JPS54152639A JPS54152639A JP6096578A JP6096578A JPS54152639A JP S54152639 A JPS54152639 A JP S54152639A JP 6096578 A JP6096578 A JP 6096578A JP 6096578 A JP6096578 A JP 6096578A JP S54152639 A JPS54152639 A JP S54152639A
- Authority
- JP
- Japan
- Prior art keywords
- groove
- steel pipe
- longer
- pipe
- value
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To perfectly make the residual stress of the weld zone to be the compression stress in case of the local repair for the weld defects by means of the welding under water cooling for the inner surface of the pipe, by making the length of weld to be longer than the value to be obtained from the specified formula.
CONSTITUTION: The inner surface of the pipe is welded under water cooling, forming the groove at the part to be repaired of the butt welded steel pipe, so as to make the circumferential length l of this groove to be longer than the value obtained from the following formula. That is, the groove length l is made longer than the value to be obtained from l=45 logD×S1/S2 mm, in which S1 mm2 is the sectional area showing the groove shape of the original weld zone, S2mm2 is the sectional area showing the rewelded groove shape, and Dmm is the diameter of the steel pipe. Moreover, above groove is desired to be formed either along the original weld zone or leaving the first layer. Additionally, this method is desirable to be applied to the steel pipe made of the austenitic stainless steel.
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6096578A JPS54152639A (en) | 1978-05-24 | 1978-05-24 | Repair welding method for steel pipe |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6096578A JPS54152639A (en) | 1978-05-24 | 1978-05-24 | Repair welding method for steel pipe |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS54152639A true JPS54152639A (en) | 1979-12-01 |
Family
ID=13157629
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6096578A Pending JPS54152639A (en) | 1978-05-24 | 1978-05-24 | Repair welding method for steel pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS54152639A (en) |
-
1978
- 1978-05-24 JP JP6096578A patent/JPS54152639A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5592285A (en) | Welding method of hard metal | |
JPS55147495A (en) | Butt welding method | |
JPS5499747A (en) | Reinforcing method for welded joint or stainless steel pipe and construction of welded join of stainless steel pipe | |
ATE30683T1 (en) | WELDED DOUBLE-WALLED PIPE AND PROCESS FOR ITS MANUFACTURE. | |
JPS54152639A (en) | Repair welding method for steel pipe | |
JPS54130451A (en) | Reducing method for residual stress at welded joint of steel | |
JPS56102394A (en) | Welding method of pipings | |
JPS53130242A (en) | Welding method for manufacture of thick-walled large diameter welded steel pipe | |
JPS56131083A (en) | Welded joint method for stainless steel tube | |
JPS53130241A (en) | Welding method for manufacture of thick walled steel pipe | |
JPS55112196A (en) | Repair welding method of pipe structure | |
JPS5573468A (en) | Butt-welded structure of thin-wall tubular body and welding method thereof | |
JPS5573494A (en) | Welding method of steel pipe | |
JPS5650797A (en) | Increasing method for weld-part fatigue strength of high-tension steel | |
JPS55141313A (en) | Manufacture of laminated metallic rod | |
JPS5536092A (en) | Seaming method of billet and pipe sleeve | |
JPS5495952A (en) | Repairing method for vertical plane of large cast steel structure by building up | |
JPS5728680A (en) | Method for welding parts | |
JPS5413433A (en) | Welding method for stainless steel | |
Groß | High-Frequency HFI-Welded Steel Pipe | |
JPS56160882A (en) | Butt welding for different material joint of piping | |
JPS54107462A (en) | Welding method of austenitic stainless steel pipe | |
JPS5770097A (en) | Structure of butt welded joint of pipe | |
JPS5617199A (en) | Method of improving stress corrosion cracking resistance of weld zone of austenite stainless steel pipe | |
JPS55133896A (en) | Welding method of pipe joint |